Carbonation of Stainless Steel Slag as a Process for CO2 Storage and Slag Valorization

被引:102
作者
Baciocchi, Renato [1 ]
Costa, Giulia [1 ]
Di Bartolomeo, Elisabetta [2 ]
Polettini, Alessandra [3 ]
Pomi, Raffaella [3 ]
机构
[1] Univ Roma Tor Vergata, Dept Civil Engn, I-00133 Rome, Italy
[2] Univ Roma Tor Vergata, Dept Chem Sci & Technol, I-00133 Rome, Italy
[3] Univ Roma La Sapienza, Dept Civil & Environm Engn, I-00184 Rome, Italy
关键词
Stainless steel slag; Particle size; Mineral carbonation; CO2; uptake; Mineralogy; Leaching; BASIC OXYGEN FURNACE; ACCELERATED CARBONATION; DICALCIUM SILICATE; SEQUESTRATION; DIOXIDE; WASTE; ASH; PRESSURE; PRODUCTS;
D O I
10.1007/s12649-010-9047-1
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
This paper examines the main results of an accelerated carbonation treatment applied to different types and size fractions of stainless steel slag. The objectives of this work were essentially to assess the CO2 uptake achievable by each type of slag under mild operating conditions and to investigate the effects of carbonation on the mineralogy and leaching behaviour of the residues. The following types of materials were tested: different size fractions of commingled slag, milled electric arc furnace (EAF) slag and argon oxygen decarburization (AOD) slag. Each material was thoroughly characterized in terms of elemental composition, mineralogy and leaching behaviour. Accelerated carbonation batch experiments were performed exposing humidified (with liquid to solid ratios <0.6 l/kg) slag to 100% CO2 for operating times between 0.5 and 24 h, at controlled temperature and pressure. Maximum CO2 uptakes of 130, 180 and 300 g CO2/kg slag were achieved (at 50 degrees C and 3 bar) for the finest fraction of the mixture, the milled EAF slag and the AOD slag, respectively. The mineralogy of each type of residue showed to be affected by the treatment, exhibiting an increase in calcite concentration and a decrease in the content of specific silicate and oxide phases. The leaching behaviour of all types of carbonated slag was also modified, exhibiting a reduction by 1-2 units of the natural pH of the materials, accompanied by a decrease of Ca release and an increase of Si leaching, as a result of modified leaching-controlling phases. In conclusion, at the tested operating conditions, AOD slag was the most reactive material with CO2. Milling, however, proved effective in increasing the carbonation yield of the EAF slag compared to that measured for the different size fractions of the commingled slag mixture.
引用
收藏
页码:467 / 477
页数:11
相关论文
共 48 条
[1]   Accelerated carbonation of different size fractions of bottom ash from RDF incineration [J].
Baciocchi, R. ;
Costa, G. ;
Lategano, E. ;
Marini, C. ;
Polettini, A. ;
Pomi, R. ;
Postorino, P. ;
Rocca, S. .
WASTE MANAGEMENT, 2010, 30 (07) :1310-1317
[2]   Influence of particle size on the carbonation of stainless steel slag for CO2 storage [J].
Baciocchi, Renato ;
Costa, Giulia ;
Polettini, Alessandra ;
Pomi, Raffaella .
GREENHOUSE GAS CONTROL TECHNOLOGIES 9, 2009, 1 (01) :4859-4866
[3]   The effects of accelerated carbonation on CO2 uptake and metal release from incineration APC residues [J].
Baciocchi, Renato ;
Costa, Giulia ;
Di Bartolomeo, Elisabetta ;
Polettini, Alessandra ;
Pomi, Raffaella .
WASTE MANAGEMENT, 2009, 29 (12) :2994-3003
[4]   Reactivity of alkaline lignite fly ashes towards CO2 in water [J].
Back, Martin ;
Kuehn, Michael ;
Stanjek, Helge ;
Peiffer, Stefan .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2008, 42 (12) :4520-4526
[5]   Investigation of accelerated carbonation for the stabilisation of MSW incinerator ashes and the sequestration of CO2 [J].
Bertos, MF ;
Li, X ;
Simons, SJR ;
Hills, CD ;
Carey, PJ .
GREEN CHEMISTRY, 2004, 6 (08) :428-436
[6]   CO2 Sequestration Potential of Steel Slags at Ambient Pressure and Temperature [J].
Bonenfant, Danielle ;
Kharoune, Lynda ;
Sauve, Sebastien ;
Hausler, Robert ;
Niquette, Patrick ;
Mimeault, Murielle ;
Kharoune, Mourad .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2008, 47 (20) :7610-7616
[7]   Accelerated carbonation and leaching behavior of the slag from iron and steel making industry [J].
Chen, Quanyuan ;
Johnson, D. C. ;
Zhu, Lingyun ;
Yuan', Menghong ;
Hills, C. D. .
JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2007, 14 (04) :297-301
[8]   Current status and perspectives of accelerated carbonation processes on municipal waste combustion residues [J].
Costa, Giulia ;
Baciocchi, Renato ;
Polettini, Alessandra ;
Pomi, Raffaella ;
Hills, Colin D. ;
Carey, Paula J. .
ENVIRONMENTAL MONITORING AND ASSESSMENT, 2007, 135 (1-3) :55-75
[9]   Steel converter slag as a raw material for precipitation of pure calcium carbonate [J].
Eloneva, Sanni ;
Teir, Sebastian ;
Salminen, Justin ;
Fogelholm, Carl-Johan ;
Zevenhoven, Ron .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2008, 47 (18) :7104-7111
[10]  
Federacciai (Federation of Italian Steel Companies), IT STEEL IND KEY STA