Cytotoxicity of silica-glass fiber reinforced composites

被引:25
作者
Meric, Gokce [1 ,2 ]
Dahl, Jon E. [1 ]
Ruyter, I. Eystein [1 ]
机构
[1] NIOM, Nord Inst Dent Mat, NO-1305 Haslum, Norway
[2] Univ Oslo, Inst Clin Dent, Dept Prosthet Dent, Oslo, Norway
关键词
biocompatibility; polymer; residual monomer; silanization; sizing;
D O I
10.1016/j.dental.2008.01.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. Silica-glass fiber reinforced polymers can be used for many kinds of dental applications. The fiber reinforcement enhances the mechanical properties of the polymers, and they have good esthetic attributes. There is good initial bonding of glass fibers to polymers via an interface made from silane coupling agents. The aim of this in vitro study was to determine the cytotoxicity of two polymers reinforced with two differently sized silica-glass fibers before and after thermal cycling. Cytotoxicity of the polymers without fibers was also evaluated. Methods. Two different resin mixtures (A and B) were prepared from poly(vinyl chloridecovinylacetate) powder and poly(methyl methacrylate) (PMMA) dissolved in methyl methacrylate and mixed with different cross-linking agents. The resin A contained the cross-linking agents ethylene glycol dimethacrylate and 1,4-butanediol dimethacrylate, and for resin B diethylene glycol dimethacrylate was used. Woven silica-glass fibers were used for reinforcement. The fibers were sized with either linear poly(butyl methacrylate)-sizing or cross-linking PMMA-sizing. Cytotoxicity was evaluated by filter diffusion test (ISO 7405:1997) of newly made and thermocycled test specimens. Extracts were prepared according to ISO 10993-12 from newly made and from thermocycled specimens and tested by the MTT assay. The results from the experiments were statistically analyzed by one-way ANOVA and Tukey's test (p < 0.05). Results. The filter diffusion test disclosed no change in staining intensity at the cell-test sample contact area indicating non-cytotoxicity in all experimental groups. Cell viability assessed by MTT assay was more than 90% in all experimental groups. All are non-cytotoxic. Significance. It can be concluded that correctly processed heat polymerized silica-glass fiber reinforced polymers induced no cytotoxicity and that thermocycling did not alter this property. (c) 2008 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:1201 / 1206
页数:6
相关论文
共 38 条
[1]   Resistance to fracture of endodontically treated teeth restored with different post systems [J].
Akkayan, B ;
Gülmez, T .
JOURNAL OF PROSTHETIC DENTISTRY, 2002, 87 (04) :431-437
[2]  
[Anonymous], 1999, 13407 ISO, P1
[3]  
[Anonymous], 2004, 1099321 ISO
[4]   THE LEVEL OF RESIDUAL MONOMER IN ACRYLIC DENTURE BASE MATERIALS - WITH PARTICULAR REFERENCE TO A MODIFIED METHOD OF ANALYSIS [J].
AUSTIN, AT ;
BASKER, RM .
BRITISH DENTAL JOURNAL, 1980, 149 (10) :281-286
[5]   Case report - Hypersensitivity to denture materials [J].
Barclay, SC ;
Forsyth, A ;
Felix, DH ;
Watson, IB .
BRITISH DENTAL JOURNAL, 1999, 187 (07) :350-352
[6]   Effect of glass fibre reinforcement on residual methyl methacrylate content of denture base polymers [J].
Bayraktar, G ;
Duran, O ;
Guvener, B .
JOURNAL OF DENTISTRY, 2003, 31 (04) :297-302
[7]  
Dahl Jon E, 2006, Gerodontology, V23, P17, DOI 10.1111/j.1741-2358.2006.00103.x
[8]  
Edmondson J.M., 1998, METHODS CELL SCI, V11, P15, DOI [10.1007/BF01404408, DOI 10.1007/BF01404408]
[9]   CARBON GRAPHITE FIBER REINFORCED POLY(METHYL METHACRYLATE) - PROPERTIES UNDER DRY AND WET CONDITIONS [J].
EKSTRAND, K ;
RUYTER, IE ;
WELLENDORF, H .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1987, 21 (09) :1065-1080
[10]  
Huang FM, 2001, INT J PROSTHODONT, V14, P439