Numerical investigation of the stress concentration on 7075-T651 aluminum alloy with one or two hemispherical pits under uniaxial or biaxial loading

被引:14
作者
Zuniga Tello, Ishvari F. [1 ]
Dominguez Almaraz, Gonzalo M. [1 ]
Lopez Garza, Victor [1 ]
Guzman Tapia, Manuel [1 ]
机构
[1] Univ Michoacana, Santiago Tapia 403, Morelia 58000, Michoacan, Mexico
关键词
Numerical simulations; Aluminum alloy 7075-T651; Stress concentration; Hemispherical pits; Uniaxial and biaxial loading; FATIGUE-CRACK GROWTH; PITTING CORROSION; LOCALIZED CORROSION; BEHAVIOR; TRANSITION; EVOLUTION; DAMAGE; PLATE; HOLE;
D O I
10.1016/j.advengsoft.2018.09.013
中图分类号
TP39 [计算机的应用];
学科分类号
081203 ; 0835 ;
摘要
Numerical simulations were carried out in order to obtain the stress concentrations induced by simulated hemispherical pits with 500 mu m of diameter on square plates of 100 mm(2) of the aluminum alloy 7075-T651, for three different plate thickness: 0.7, 1.6 and 3 mm. The pertinence of this study is supported by the fact that modern industries using this aluminum alloy, such as the aeronautical, marine, mold tool manufacturing and arms industries, are affected by the combination of loading and corrosion, which leads to stress concentration and the failure of material. Numerical simulations were performed to investigate the effect of one and two pits on the surface of aluminum plates, for the transverse or longitudinal load orientation and under uni-axial and biaxial loading. In addition, the depth of the pits across the thickness of the plate together with the proximity of two pits under the last described conditions were investigated. It was found that the orientation of two pits in regards the applied load plays a significant role on the stress concentration under uniaxial loading. Finally, graphs for the stress concentration and the corresponding general tendencies were obtained associated with hemispherical pits and the mentioned parameters of the plates, together with the general conclusions concerning these numerical results.
引用
收藏
页码:23 / 35
页数:13
相关论文
共 37 条
  • [31] Atmospheric Pitting Corrosion Studies of AA7075-T6 under Electrolyte Droplets: Part I. Effects of Droplet Size, Concentration, Composition, and Sample Aging
    Thomson, M. S.
    Frankel, G. S.
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2017, 164 (12) : C653 - C663
  • [32] Preparation of bimodal grain size 7075 aviation aluminum alloys and their corrosion properties
    Tian, Wenming
    Li, Songmei
    Liu, Jianhua
    Yu, Mei
    Du, Yujie
    [J]. CHINESE JOURNAL OF AERONAUTICS, 2017, 30 (05) : 1777 - 1788
  • [33] Pitting corrosion of naturally aged AA 7075 aluminum alloys with bimodal grain size
    Tian, Wenming
    Li, Songmei
    Wang, Bo
    Liu, Jianhua
    Yu, Mei
    [J]. CORROSION SCIENCE, 2016, 113 : 1 - 16
  • [34] Improvement of abrasion resistance in artificial seawater and corrosion resistance in NaCl solution of 7075 aluminum alloy processed by laser shock peening
    Wang, Hao
    Ning, Chengyi
    Huang, Yihui
    Cao, Zhenya
    Chen, Xiaoxiao
    Zhang, Wenwu
    [J]. OPTICS AND LASERS IN ENGINEERING, 2017, 90 : 179 - 185
  • [35] Wei RP, 2001, MATER SCI RES INT, V7, P147
  • [36] The concentration of stress and strain in finite thickness elastic plate containing a circular hole
    Yang, Zheng
    Kim, Chang-Boo
    Cho, Chongdu
    Beom, Hyeon Gyu
    [J]. INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2008, 45 (3-4) : 713 - 731
  • [37] Zhang X, 2013, PROC INT CONF ENV SC