Mitigation of hot cracking in Inconel 718 superalloy by ultrasonic vibration during gas tungsten arc welding

被引:59
作者
Thavamani, R. [1 ]
Balusamy, V. [1 ]
Nampoothiri, Jayakrishnan [2 ]
Subramanian, R. [1 ]
Ravi, K. R. [1 ,2 ]
机构
[1] PSG Coll Technol, Dept Met Engn, Coimbatore 641004, Tamil Nadu, India
[2] PSG Inst Adv Studies, Struct Nanomat Lab, Coimbatore 641004, Tamil Nadu, India
关键词
High-temperature alloys; Microstructure; Thermodynamic modeling; Ultrasonic vibration; HEAT-AFFECTED ZONE; GRAIN-REFINEMENT; LIQUATION CRACKING; BASE SUPERALLOYS; COOLING RATE; FUSION ZONE; LAVES PHASE; SOLIDIFICATION; ALLOY; MICROSTRUCTURE;
D O I
10.1016/j.jallcom.2017.12.295
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present study, Gas Tungsten Arc Welding (GTAW) of Inconel 718 alloy has been carried out at different welding currents with and without ultrasonic vibration. In the absence of ultrasonic treatment, samples welded with a current of 80 A have shown a crack length of 15 mm which is found to increase to 35 mm for a welding current of 120 A. The slow solidification rate associated with high welding current causes increase in hot cracking length. Non-equilibrium Scheil solidification simulation of Inconel 718 based on CALPHAD approach suggests that the long freezing range of more than 175 degrees C, small fraction of eutectic, i.e., less than 10% in susceptible freezing range (SFR) and segregation of low melting point Laves and gamma '' (Ni3Nb) phases play critical roles in hot cracking behavior of Inconel 718 alloy. Ultrasonic treatment during solidification of weld metal has decreased the crack sensitivity and dendritic arm length of Inconel 718 alloy from 47.5% to 13.3% for the welding current of 120 A. There was a corresponding reduction in dendritic arm length from 1256 to 89 mu m. Further, it was observed that the welding current has very limited role in the hot cracking behavior of Inconel 718 alloy in the presence of ultrasonic vibration. Dendritic fragmentation, grain refinement and reduction in solute segregation are recognized as the main factors that mitigate hot cracking tendency of Inconel 718 alloy by ultrasonic vibration. (C)2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:870 / 878
页数:9
相关论文
共 37 条
  • [1] Effect of dilution on the behavior of solidification cracking in PTAW overlay deposit on Ni-base superalloys
    Ahn, Y
    Yoon, B
    Kim, H
    Lee, C
    [J]. METALS AND MATERIALS INTERNATIONAL, 2002, 8 (05): : 469 - 477
  • [2] The effect of cooling rate on the solidification of INCONEL 718
    Antonsson, T
    Fredriksson, H
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2005, 36 (01): : 85 - 96
  • [3] Criteria of Grain Refinement Induced by Ultrasonic Melt Treatment of Aluminum Alloys Containing Zr and Ti
    Atamanenko, T. V.
    Eskin, D. G.
    Zhang, L.
    Katgerman, L.
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (08): : 2056 - 2066
  • [4] Brochu M., 2013, 13 INT C FRACT JUN 1
  • [5] STRENGTHENING MECHANISMS IN INCONEL-718 SUPER-ALLOY
    CHATURVEDI, MC
    HAN, YF
    [J]. METAL SCIENCE, 1983, 17 (03): : 145 - 149
  • [6] Effect of boron segregation at grain boundaries on heat-affected zone cracking in wrought INCONEL 718
    Chen, W
    Chaturvedi, MC
    Richards, NL
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2001, 32 (04): : 931 - 939
  • [7] Investigation of dendritic growth and liquation cracking in laser melting deposited Inconel 718 at different laser input angles
    Chen, Yuan
    Lu, Fenggui
    Zhang, Ke
    Nie, Pulin
    Hosseini, Seyed Reza Elmi
    Feng, Kai
    Li, Zhuguo
    Chu, Paul K.
    [J]. MATERIALS & DESIGN, 2016, 105 : 133 - 141
  • [8] Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling
    Chen, Yuan
    Lu, Fenggui
    Zhang, Ke
    Nie, Pulin
    Hosseini, Seyed Reza Elmi
    Feng, Kai
    Li, Zhuguo
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 670 : 312 - 321
  • [9] Dvornak M.J., 1991, WELDING RES S, P271
  • [10] MICROSTRUCTURAL CHARACTERIZATION AND ELEMENTAL PARTITIONING IN A DIRECT-AGED SUPERALLOY (DA-718)
    FAYMAN, YC
    [J]. MATERIALS SCIENCE AND ENGINEERING, 1987, 92 : 159 - 171