Strain-controlled fatigue properties of dissimilar welded joints between Ti-6Al-4V and Ti17 alloys

被引:53
|
作者
Wang, S. Q. [1 ,2 ]
Liu, J. H. [2 ]
Chen, D. L. [1 ]
机构
[1] Ryerson Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
[2] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
加拿大创新基金会; 加拿大自然科学与工程研究理事会;
关键词
Titanium alloy; Electron beam welding; Dissimilar welded joints; Fatigue; Cyclic deformation; Twinning; LOW-CYCLE FATIGUE; GAS TUNGSTEN ARC; BEAM MELTED TI-6AL-4V; ELECTRON-BEAM; MECHANICAL-PROPERTIES; TITANIUM-ALLOY; MAGNESIUM ALLOY; ROOM-TEMPERATURE; DEFORMATION-BEHAVIOR; YOUNGS MODULUS;
D O I
10.1016/j.matdes.2013.02.034
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study was to evaluate the microstructure, hardness and cyclic deformation behavior of electron beam welded dissimilar joints of Ti-6Al-4V and Ti17 (Ti-5Al-4Mo-4Cr-2Sn-2Zr) titanium alloys. The welding resulted in a significant microstructural change across the joint, with hexagonal close-packed (hcp) martensite alpha' and orthorhombic martensite alpha '' in the fusion zone (FZ), alpha' in the heat-affected zone (HAZ) of Ti-6Al-4V side, and coarse beta in the HAZ of Ti17 side. A characteristic asymmetrical hardness profile across the dissimilar joint was observed with the highest hardness in the FZ and a lower hardness on the Ti-6Al-4V side than on the Ti17 side, where a soft zone was observed. The dissimilar joint exhibited a lower Young's modulus and higher cyclic strain hardening exponent than both Ti-6Al-4V and Ti17 base metals (BMs), and had the monotonic and cyclic yield strengths lying inbetween those of two BMs with higher values for Ti17 alloy. Both BMs and joint showed essentially symmetrical hysteresis loops and equivalent fatigue life, and exhibited cyclic stabilization at lower strain amplitude sup to 0.6%, while cyclic softening occurred after initial cyclic stabilization at higher strain amplitudes. The initial cyclic stabilization was shortened with increasing strain amplitude. In the Ti-6Al-4V BM fatigued at a high strain amplitude of 1.2%, a short initial cyclic hardening emerged, corresponding to the presence of twinning and its resistance to the dislocation movement. Fatigue failure of the dissimilar joint occurred in the HAZ of Ti17 side where the soft zone was present, with crack initiation from the specimen surface or near-surface defect and crack propagation characterized by typical fatigue striations. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:716 / 727
页数:12
相关论文
共 50 条
  • [41] The transition from strain rate insensitivity to sensitivity of Ti-6Al-4V alloys deformed at cryogenic temperature
    Guo, Mengqiang
    Zhang, Yu
    Zhou, Chang
    Wu, Hao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 902
  • [42] Fracture Toughness of Ti-6Al-4V and Ti-6Al-4V ELI Alloys Fabricated by Electron Beam Melting With Different Orientation and Positions
    Ninerola, Ruben
    Giner, Eugenio
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2025, 48 (05) : 2339 - 2353
  • [43] Quality characterization of dissimilar laser welded joints of Ti6Al4V with AISI 304 by using copper deposition technique
    Chatterjee, Suman
    Sahoo, Sushanta Kumar
    Swain, B.
    Mahapatra, Siba Sankar
    Roy, Tarapada
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 106 (9-10): : 4577 - 4591
  • [44] Dehydrogenation of Hydrogenated Ti-6Al-4V Alloy
    Yuan Baoguo
    Liu Dahai
    Li Chunfeng
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (09) : 2104 - 2107
  • [45] Fatigue crack propagation properties of Ti-6Al-4V in vacuum environments
    Oguma, H.
    Nakamura, T.
    INTERNATIONAL JOURNAL OF FATIGUE, 2013, 50 : 89 - 93
  • [46] Microstructure and Mechanical Features of Electron Beam Welded Dissimilar Titanium Alloys: Ti-10V-2Fe-3Al and Ti-6Al-4V
    Utama, Muhammad Iman
    Park, Nokeun
    Baek, Eung Ryul
    METALS AND MATERIALS INTERNATIONAL, 2019, 25 (02) : 439 - 448
  • [47] Oxygen effects on the mechanical properties and lattice strain of Ti and Ti-6Al-4V
    J. -M. Oh
    B. -G. Lee
    S. -W. Cho
    S. -W. Lee
    G. -S. Choi
    J. -W. Lim
    Metals and Materials International, 2011, 17 : 733 - 736
  • [48] Oxygen Effects on the Mechanical Properties and Lattice Strain of Ti and Ti-6Al-4V
    Oh, J. -M.
    Lee, B. -G.
    Cho, S. -W.
    Lee, S. -W.
    Choi, G. -S.
    Lim, J. -W.
    METALS AND MATERIALS INTERNATIONAL, 2011, 17 (05) : 733 - 736
  • [49] Microstructural response at the interface and its effect on the fatigue fracture behavior of rotary friction welded dissimilar titanium alloys: Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) and Ti-6Al-2Sn-4Zr-2Mo (Ti6242)
    Wang, Binwen
    Chen, Xianmin
    Yang, Jun
    Jin, Feng
    Wang, Qian
    MATERIALS RESEARCH EXPRESS, 2021, 8 (10)
  • [50] Microstructure evolution and high cycle fatigue failure behavior of friction stir-welded Ti-6Al-4V at varying welding speeds
    Mashinini, Peter Madindwa
    Dinaharan, Isaac
    Hattingh, Danie Gerhardus
    Selvam, Jebaraj David Raja
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 122 (9-10): : 4041 - 4054