Strain-controlled fatigue properties of dissimilar welded joints between Ti-6Al-4V and Ti17 alloys

被引:53
|
作者
Wang, S. Q. [1 ,2 ]
Liu, J. H. [2 ]
Chen, D. L. [1 ]
机构
[1] Ryerson Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
[2] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
加拿大自然科学与工程研究理事会; 加拿大创新基金会;
关键词
Titanium alloy; Electron beam welding; Dissimilar welded joints; Fatigue; Cyclic deformation; Twinning; LOW-CYCLE FATIGUE; GAS TUNGSTEN ARC; BEAM MELTED TI-6AL-4V; ELECTRON-BEAM; MECHANICAL-PROPERTIES; TITANIUM-ALLOY; MAGNESIUM ALLOY; ROOM-TEMPERATURE; DEFORMATION-BEHAVIOR; YOUNGS MODULUS;
D O I
10.1016/j.matdes.2013.02.034
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study was to evaluate the microstructure, hardness and cyclic deformation behavior of electron beam welded dissimilar joints of Ti-6Al-4V and Ti17 (Ti-5Al-4Mo-4Cr-2Sn-2Zr) titanium alloys. The welding resulted in a significant microstructural change across the joint, with hexagonal close-packed (hcp) martensite alpha' and orthorhombic martensite alpha '' in the fusion zone (FZ), alpha' in the heat-affected zone (HAZ) of Ti-6Al-4V side, and coarse beta in the HAZ of Ti17 side. A characteristic asymmetrical hardness profile across the dissimilar joint was observed with the highest hardness in the FZ and a lower hardness on the Ti-6Al-4V side than on the Ti17 side, where a soft zone was observed. The dissimilar joint exhibited a lower Young's modulus and higher cyclic strain hardening exponent than both Ti-6Al-4V and Ti17 base metals (BMs), and had the monotonic and cyclic yield strengths lying inbetween those of two BMs with higher values for Ti17 alloy. Both BMs and joint showed essentially symmetrical hysteresis loops and equivalent fatigue life, and exhibited cyclic stabilization at lower strain amplitude sup to 0.6%, while cyclic softening occurred after initial cyclic stabilization at higher strain amplitudes. The initial cyclic stabilization was shortened with increasing strain amplitude. In the Ti-6Al-4V BM fatigued at a high strain amplitude of 1.2%, a short initial cyclic hardening emerged, corresponding to the presence of twinning and its resistance to the dislocation movement. Fatigue failure of the dissimilar joint occurred in the HAZ of Ti17 side where the soft zone was present, with crack initiation from the specimen surface or near-surface defect and crack propagation characterized by typical fatigue striations. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:716 / 727
页数:12
相关论文
共 50 条
  • [1] Cyclic deformation of dissimilar welded joints between Ti-6Al-4V and Ti17 alloys: Effect of strain ratio
    Wang, S. Q.
    Liu, J. H.
    Lu, Z. X.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 598 : 122 - 134
  • [2] Strain-controlled fatigue properties of linear friction welded dissimilar joints between Ti-6Al-4V and Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloys
    Wen, G. D.
    Ma, T. J.
    Li, W. Y.
    Wang, S. Q.
    Guo, H. Z.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 612 : 80 - 88
  • [3] Effect of strain rate and temperature on strain hardening behavior of a dissimilar joint between Ti-6Al-4V and Ti17 alloys
    Wang, S. Q.
    Liu, J. H.
    Chen, D. L.
    MATERIALS & DESIGN, 2014, 56 : 174 - 184
  • [4] Tensile and fatigue properties of electron beam welded dissimilar joints between Ti-6Al-4V and BT9 titanium alloys
    Wang, S. Q.
    Liu, J. H.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 584 : 47 - 56
  • [5] Tensile and fatigue behavior of electron beam welded dissimilar joints of Ti-6Al-4V and IMI834 titanium alloys
    Wang, S. Q.
    Li, W. Y.
    Zhou, Y.
    Li, X.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 649 : 146 - 152
  • [6] Strain-controlled fatigue in B-modified Ti-6Al-4V alloys
    Singh, Gaurav
    Gaddam, Raghuveer
    Petley, Vijay
    Datta, Ranjan
    Pederson, Robert
    Ramamurty, Upadrasta
    SCRIPTA MATERIALIA, 2013, 69 (09) : 698 - 701
  • [7] Low Cycle Fatigue Behaviors of TI-6AL-4V Alloy Controlled by Strain and Stress
    Wang, Ruifeng
    Li, Youtang
    An, Huping
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS XI, 2013, 525-526 : 441 - +
  • [8] Effect of microstructure on the fatigue properties of Ti-6Al-4V titanium alloys
    Wu, G. Q.
    Shi, C. L.
    Sha, W.
    Sha, A. X.
    Jiang, H. R.
    MATERIALS & DESIGN, 2013, 46 : 668 - 674
  • [9] Flexible control of the microstructure and mechanical properties of friction stir welded Ti-6Al-4V joints
    Kitamura, K.
    Fujii, H.
    Iwata, Y.
    Sun, Y. S.
    Morisada, Y.
    MATERIALS & DESIGN, 2013, 46 : 348 - 354
  • [10] Formation of residual stresses during quenching of Ti17 and Ti-6Al-4V alloys: Influence of phase transformations
    Teixeira, J.
    Marechal, D.
    Wimpory, R. C.
    Denis, S.
    Lefebvre, F.
    Frappier, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 832