Does Illinois bituminous coal manifest glass transition: DMA, DSC, and FTIR results

被引:8
作者
Markevicius, Gediminas [1 ]
West, Richard D. [1 ]
Malhotra, Vivak M. [1 ]
Hofer, Stephen [1 ]
机构
[1] So Illinois Univ, Dept Phys, Carbondale, IL 62901 USA
关键词
Bituminous coal; Glass transition; Thermomechanical behavior; Dynamic mechanical analysis; Differential scanning calorimetry; 2ND-ORDER TRANSITIONS; TEMPERATURE; CO2; IR; CHEMISTRY;
D O I
10.1016/j.fuel.2012.07.062
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
It has been argued that coal, especially deep, unmineable seams, holds the potential of sequestering carbon dioxide (CO2) while recovering fuel gases. In the recent past, it has been proposed that various ranked coals display glass transition or second order transition at 100 degrees C <= T <= 200 degrees C under nitrogen environment, and this transition temperature shifts to lower temperatures when coals were pressurized with relatively low pressure (<= 3 MPa) CO2. If glass transition does exist in coal, then on pressurizing the deep, unmineable coal seams, where pressures are expected to be higher than 3 MPa of CO2, the presence of glass transition could potentially pose reservoir stability concerns. We undertook differential scanning calorimetric (DSC) and dynamic mechanical analysis (DMA) measurements on Murphysboro seam coal (Illinois bituminous) at 30 degrees C <= T <= 250 degrees C under N-2 gas environment to ascertain whether this coal even has a glass transition. These experiments were further complemented by conducting in situ diffuse reflectance infrared spectroscopic measurements (DRIFT). It is worth mentioning that the DMA technique is much more sensitive in detecting glass transition than the DSC technique, and previously reported glass transitions were ascertained by the DSC method. Though we did observe thermal events, ascribed to the evaporation of bulk and hydrogen-bonded water at 90 degrees C <= T <= 190 degrees C, we did not observe any glass or second order transition for Murphysboro coal at 30 degrees C <= T <= 250 degrees C. The storage modulus (E') of the coal steadily decreased as the temperature increased from 30 degrees C with E' showing two minima at 158 degrees C and 221 degrees C. These minima could be attributed to the evaporation of CO2 from the coal produced during self oxidation rather than any thermodynamic event. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:220 / 226
页数:7
相关论文
共 26 条
  • [21] HYDROGEN-BONDING IN POLYMERS - INFRARED TEMPERATURE STUDIES OF AN AMORPHOUS POLYAMIDE
    SKROVANEK, DJ
    HOWE, SE
    PAINTER, PC
    COLEMAN, MM
    [J]. MACROMOLECULES, 1985, 18 (09) : 1676 - 1683
  • [22] INFRARED-SPECTROSCOPY OF COAL MACERAL CONCENTRATES AT ELEVATED-TEMPERATURES
    VASSALLO, AM
    LIU, YL
    PANG, LSK
    WILSON, MA
    [J]. FUEL, 1991, 70 (05) : 635 - 639
  • [23] Variations in the mechanical behavior of Illinois bituminous coals
    West, Richard D.
    Markevicius, Gediminas
    Malhotra, Vivak M.
    Hofer, Stephen
    [J]. FUEL, 2012, 98 : 213 - 217
  • [24] Sequestration of carbon dioxide in coal with enhanced coalbed methane recovery - A review
    White, CM
    Smith, DH
    Jones, KL
    Goodman, AL
    Jikich, SA
    LaCount, RB
    DuBose, SB
    Ozdemir, E
    Morsi, BI
    Schroeder, KT
    [J]. ENERGY & FUELS, 2005, 19 (03) : 659 - 724
  • [25] PHYSICAL TRANSITIONS IN PITTSBURGH NO-8 COAL AS OBSERVED BY DIFFERENTIAL SCANNING CALORIMETRY AND SOLVENT SWELLING
    YUN, Y
    SUUBERG, EM
    [J]. ENERGY & FUELS, 1992, 6 (03) : 328 - 330
  • [26] Yun Y, 1993, PREPR PAP AM CHEM SO, V38, P489