Pipe lining abrasion testing for paste backfill operations

被引:47
作者
Hewitt, David [1 ]
Allard, Sebastian [2 ]
Radziszewski, Peter [1 ]
机构
[1] McGill Univ, Dept Mech Engn, Comminut Dynam Lab, Montreal, PQ H3A 2K6, Canada
[2] Canada Kalprotect Inc, Kirkland, PQ H9H 4S4, Canada
关键词
Mineral processing; Waste processing; Tailings; Tailings disposal; WEAR;
D O I
10.1016/j.mineng.2009.03.010
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Pipe wear in paste backfill mining operations represents a great cost to mining companies. The replacement of prematurely worn pipes results in the shut down of the entire paste system. Abrasion testing performed on various pipe lining samples yielded both quantitative and qualitative data. Both standard and non-standard methods were explored during testing. The pipe materials are ranked by their relative wear resistance as well as energy per unit mass loss, The latter may allow for better prediction of pipe wear, this in turn could prove worthwhile when scheduling maintenance downtime for such a system where cost savings would be beneficial. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1088 / 1090
页数:3
相关论文
共 7 条
[1]  
Bikbaev K.A., 1973, Chem. Pet. Eng, V9, P73, DOI [10.1007/BF01139742, DOI 10.1007/BF01139742]
[2]   Review of current high density paste fill and its technology [J].
Jung, SJ ;
Biswas, K .
MINERAL RESOURCES ENGINEERING, 2002, 11 (02) :165-182
[3]   A CLASSIFICATION OF 3-BODY ABRASIVE WEAR AND DESIGN OF A NEW TESTER [J].
MISRA, A ;
FINNIE, I .
WEAR, 1980, 60 (01) :111-121
[4]  
Rabinowicz E., 1995, FRICTION WEAR MAT, P315
[5]   Exploring total media wear [J].
Radziszewski, P .
MINERALS ENGINEERING, 2002, 15 (12) :1073-1087
[6]   Environmental rheology for waste minimisation in the minerals industry [J].
Sofrá, F ;
Boger, DV .
CHEMICAL ENGINEERING JOURNAL, 2002, 86 (03) :319-330
[7]   DETERMINATION OF BASIC FACTORS AFFECTING THE ABRASIVE WEAR OF PIPES [J].
SOLOVEV, YG ;
YUSHKEVICH, PM ;
BONDAR, NP ;
KRAVCHENKO, NV .
METAL SCIENCE AND HEAT TREATMENT, 1986, 28 (3-4) :214-216