The Effect of Welding Current and Electrode Force on the Heat Input, Weld Diameter, and Physical and Mechanical Properties of SS316L/Ti6Al4V Dissimilar Resistance Spot Welding with Aluminum Interlayer

被引:7
|
作者
Taufiqurrahman, Iqbal [1 ]
Ahmad, Azlan [1 ]
Mustapha, Mazli [1 ]
Lenggo Ginta, Turnad [2 ]
Ady Farizan Haryoko, Luthfi [1 ]
Ahmed Shozib, Imtiaz [1 ]
机构
[1] Univ Teknol PETRONAS, Dept Mech Engn, Seri Iskandar 32610, Perak Darul Rid, Malaysia
[2] PT Orca Ind Akad, Jakarta 12950, Indonesia
关键词
resistance spot welding; stainless steel 316L; Ti6Al4V alloy; mechanical properties; aluminum interlayer; welding current; heat input; STAINLESS-STEEL; 316L; PROCESS PARAMETERS; TITANIUM-ALLOY; JOINT; MICROSTRUCTURE; STRENGTH; LASER;
D O I
10.3390/ma14051129
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Welding parameters obviously determine the joint quality during the resistance spot welding process. This study aimed to investigate the effect of welding current and electrode force on the heat input and the physical and mechanical properties of a SS316L and Ti6Al4V joint with an aluminum interlayer. The weld current values used in this study were 11, 12, and 13 kA, while the electrode force values were 3, 4, and 5 kN. Welding time and holding time remained constant at 30 cycles. The study revealed that, as the welding current and electrode force increased, the generated heat input increased significantly. The highest tensile-shear load was recorded at 8.71 kN using 11 kA of weld current and 3 kN of electrode force. The physical properties examined the formation of a brittle fracture and several weld defects on the high current welded joint. The increase in weld current also increased the weld diameter. The microstructure analysis revealed no phase transformation on the SS316L interface; instead, the significant grain growth occurred. The phase transformation has occurred on the Ti6Al4V interface. The intermetallic compound layer was also investigated in detail using the EDX (Energy Dispersive X-Ray) and XRD (X-Ray Diffraction) analyses. It was also found that both stainless steel and titanium alloy have their own fusion zone, which is indicated by the highest microhardness value.
引用
收藏
页码:1 / 20
页数:20
相关论文
共 45 条
  • [31] Dissimilar friction stir welding of Ti-6Al-4V alloy and aluminum alloy employing a modified butt joint configuration: Influences of process variables on the weld interfaces and tensile properties
    Li, Bo
    Zhang, Zhenhua
    Shen, Yifu
    Hu, Weiye
    Luo, Lei
    MATERIALS & DESIGN, 2014, 53 : 838 - 848
  • [32] Interfacial layer regulation and its effect on mechanical properties of Ti6Al4V titanium alloy and T2 copper dissimilar joints by cold metal transfer welding
    Huang, Libing
    Dong, Honggang
    Ma, Yueting
    Li, Peng
    Wang, Jiawei
    Yang, Jiang
    Wu, Baosheng
    JOURNAL OF MANUFACTURING PROCESSES, 2022, 75 : 1100 - 1110
  • [33] Analysis of mechanical properties and optimization of laser beam welding parameters on dissimilar metal titanium (Ti6Al4V) and aluminium (A6061) by factorial and ANOVA techniques
    Chandran, Sudhin
    Rajesh, R.
    Anand, M. Dev
    MATERIALS TODAY-PROCEEDINGS, 2021, 42 : 508 - 514
  • [34] The experimental study of CFRP interlayer of dissimilar joint AA7075-T651/Ti-6Al-4V alloys by friction stir spot welding on mechanical and microstructural properties
    Nasir, Tauqir
    Kalaf, Omer
    Asmael, Mohammed
    Zeeshan, Qasim
    Safaei, Babak
    Hussain, Ghulam
    Motallebzadeh, Amir
    NANOTECHNOLOGY REVIEWS, 2021, 10 (01) : 401 - 413
  • [35] The effect of vacuum brazing time on the microstructure and mechanical properties of Ti-6Al-4 V to 316 L dissimilar joint using BNi-2 filler metal
    Foumani, Milad
    Naffakh-Moosavy, Homam
    JOURNAL OF ADVANCED JOINING PROCESSES, 2024, 9
  • [36] CHARACTERIZING THE EFFECT OF POST WELD HEAT TREATMENT ON THE MECHANICAL PROPERTIES OF LASER BEAM WELDED ADDITIVE MANUFACTURED TI6AL4V
    Akinlabi, Esther T.
    Omoniyi, Peter
    Jen, Tien-Chien
    Mahamood, Rasheedat M.
    Mwema, Frederick
    Akinlabi, Stephen A.
    Abima, Cynthia S.
    PROCEEDINGS OF ASME 2023 INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION, IMECE2023, VOL 4, 2023,
  • [37] Effect of sheet thickness on the fusion zone temperature distribution, melt pool dimensions, mechanical properties, and microstructure in laser welding of Ti6Al4V alloy
    Khdair, Adnan I.
    Hader, Montasir
    Abushgair, Khaleel
    Khrais, Samir
    JOURNAL OF LASER APPLICATIONS, 2021, 33 (03)
  • [38] Analysis of the Microstructure and Mechanical Performance of Resistance Spot-Welding of Ti6Al4V to DP600 Steel Using Copper/Gold Cold-Sprayed Interlayers
    Szwajka, Krzysztof
    Zielinska-Szwajka, Joanna
    Szewczyk, Marek
    Mezher, Marwan T.
    Trzepiecinski, Tomasz
    MATERIALS, 2024, 17 (13)
  • [39] Effect of heat treatments on mechanical properties and wear resistance of laser-powder bed-fused Ti6Al4V alloy
    Wang, Sen
    Wang, Linzhi
    Li, Jing
    Li, Ting
    Qiu, Yingkun
    Yang, Runqi
    MODERN PHYSICS LETTERS B, 2024, 38 (26):
  • [40] Influence of Heat Input on Welding Processes, Weld Formation, Microstructure, and Mechanical Properties of Double-Sided Laser Beam Welded Ti-6Al-4V Alloy T-Joints
    Ma Xuyi
    Duan Aiqin
    Lu Wei
    Wang Xuedong
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (07) : 2300 - 2307