Oxidation of Zr2[Al(Si)]4C5 and Zr3[Al(Si)]4C6 in air

被引:38
作者
He, L. F. [1 ,2 ]
Bao, Y. W. [1 ]
Li, M. S. [1 ]
Wang, J. Y. [1 ]
Zhou, Y. C. [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
[2] Chinese Acad Sci, Grad Sch, Beijing 100039, Peoples R China
关键词
D O I
10.1557/JMR.2008.0411
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The oxidation behavior of Zr-2[Al(Si)](4)C-5 and Zr-3[Al(Si)](4)C-6 in air has been investigated. The oxidation kinetics of bulk Zr-2[Al(Si)](4)C-5 and Zr-3[Al(Si)](4)C-6 at 900-1300 degrees C generally follow a parabolic law at a very short initial stage and then a linear law for a long period with the activation energy of 237.9 and 226.8 kJ/mol, respectively. The oxide scales have a duplex structure, consisting of mainly an outer porous layer of ZrO2, Al2O3, and aluminosilicate/mullite, and a thin inner compact layer of these oxides plus remaining carbon. The oxidation resistance of Zr-2[Al(Si)](4)C-5 and Zr-3[Al(Si)](4)C-6 has been improved compared with Zr2Al3C4, and is much better than Zr-3[Al(Si)](4)C-6 to larger fraction of protective oxidation products, Al2O3 and aluminosilicate/mullite.
引用
收藏
页码:3339 / 3346
页数:8
相关论文
共 29 条
[1]  
[Anonymous], REFRACTORY CARBIDES
[2]  
Bartsch M, 1999, J AM CERAM SOC, V82, P1388, DOI 10.1111/j.1151-2916.1999.tb01928.x
[3]  
Chiang Y.M., 1997, Physical ceramics - Principles for ceramic science and engineering MIT Series in Material Science and Engineering
[4]  
Fukuda K, 2007, J MATER RES, V22, P2888, DOI [10.1557/jmr.2007.0372, 10.1557/JMR.2007.0372]
[5]   Synthesis, crystal structure and thermoelectric properties of a new carbide Zr2[Al3.56Si0.44]C5 [J].
Fukuda, Koichiro ;
Hisamura, Miyuki ;
Iwata, Tomoyuki ;
Tera, Nobuyuki ;
Sato, Kimiyasu .
JOURNAL OF SOLID STATE CHEMISTRY, 2007, 180 (06) :1809-1815
[6]   Improving the high-temperature oxidation resistance of Zr2Al3C4 by silicon pack cementation [J].
He, L. F. ;
Bao, Y. W. ;
Li, M. S. ;
Wang, J. Y. ;
Zhou, Y. C. .
JOURNAL OF MATERIALS RESEARCH, 2008, 23 (08) :2275-2282
[7]   Elastic and thermal properties of Zr2Al3C4:: Experimental investigations and ab initio calculations [J].
He, L. F. ;
Wang, J. Y. ;
Bao, Y. W. ;
Zhou, Y. C. .
JOURNAL OF APPLIED PHYSICS, 2007, 102 (04)
[8]   Isothermal oxidation of bulk Zr2Al3C4 at 500 to 1000 °C in air [J].
He, L. F. ;
Lin, Z. J. ;
Bao, Y. W. ;
Li, M. S. ;
Wang, J. Y. ;
Zhou, Y. C. .
JOURNAL OF MATERIALS RESEARCH, 2008, 23 (02) :359-366
[9]   Synthesis and characterization of bulk Zr2Al3C4 ceramic [J].
He, Lingfeng ;
Lin, Zhijun ;
Wang, Jingyang ;
Bao, Yiwang ;
Li, Meishuan ;
Zhou, Yanchun .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (11) :3687-3689
[10]   Oxidation behavior of Al4SiC4 ceramic up to 1700°C [J].
Huang, X. X. ;
Wen, G. W. ;
Cheng, X. M. ;
Zhang, B. Y. .
CORROSION SCIENCE, 2007, 49 (05) :2059-2070