The mechanical response and microstructural evolution of 2195 Al-Li alloy during hot tensile deformation

被引:24
|
作者
Li, Qun [1 ]
Ning, Jian [1 ]
Chen, Lei [2 ]
Hu, Jianliang [1 ]
Liu, Yuanxi [1 ]
机构
[1] Yanshan Univ, Key Lab Adv Forging & Stamping Technol & Sci, Minist Educ, Qinhuangdao 066004, Hebei, Peoples R China
[2] Yanshan Univ, Natl Engn Res Ctr Equipment & Technol Cold Strip, Qinhuangdao 066004, Hebei, Peoples R China
基金
中国国家自然科学基金;
关键词
2195 Al-Li alloy; Tensile deformation; Elongation; Fracture mode; Grain coarsening; FLOW BEHAVIOR; PRECIPITATION; ORIENTATION; AEROSPACE; TEXTURE; SHEET; MG; RECRYSTALLIZATION; TEMPERATURE;
D O I
10.1016/j.jallcom.2020.156515
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Hot tensile deformation behavior of 2195 Al-Li alloy was investigated at the temperature of 420-520 degrees C and the strain rates of 0.01-1 s(-1). The mechanical characteristics and microstructural mechanism were discussed. Overall, the tensile strength increased with decreasing temperature and increasing strain rate, and the total elongation was more sensitive to temperature than to strain rate. At each strain rate, the elongation firstly increased and then decreased with the rise of temperature and it showed the maximum at 440 degrees C. Particularly, the fracture mode gradually changed from ductile fracture with dimples to brittle fracture with cleavage steps when the temperature exceeded 440 degrees C at each strain rate. This was attributed to the larger proportion of coarsening grains with a diameter exceeding 15 mu m. The total elongation (E) showed a linear relationship with the proportion of coarsening grain (P). The larger the P was, the lower the E was. EBSD results showed that although the dynamic recrystallization (DRX) level, facilitating to improvement of ductility, increased with the rising of temperature, the recrystallized grains became larger at higher temperatures due to rapid growth rate, especially at lower strain rate, then a decline of the total elongation displayed. Moreover, a large number of fine precipitations of theta' and delta' phases distributed dispersedly in the matrix at the deformation temperature of 440 degrees C. However, the overall number of the precipitations decreased when the deformation temperature further increased. The theta' phase completely dissolved into the matrix, only a small amount of delta' phases could be observed at 480 degrees C and 500 degrees C, thus the pinning effects on the grain boundary migration were weakened, whereby the grain size displayed an additional increase. (C) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Evolution of grain structure in AA2195 Al-Li alloy plate during recrystallization
    杜予晅
    张新明
    叶凌英
    刘胜胆
    Transactions of Nonferrous Metals Society of China, 2006, (02) : 321 - 326
  • [32] Evolution of grain structure in AA2195 Al-Li alloy plate during recrystallization
    Du, YX
    Zhang, XM
    Ye, LY
    Liu, SD
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 (02) : 321 - 326
  • [33] Strength and structure variation of 2195 Al-Li alloy caused by different deformation processes of hot extrusion and cold-rolling
    Ma, Yun-long
    Li, Jin-feng
    Zhang, Run-zhe
    Tang, Jian-guo
    Huang, Cheng
    Li, Hong-ying
    Zheng, Zi-qiao
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2020, 30 (04) : 835 - 849
  • [34] Local microstructure evolution and mechanical performance of friction stir additive manufactured 2195 Al-Li alloy
    Shen, Z.
    Chen, S.
    Cui, L.
    Li, D.
    Liu, X.
    Hou, W.
    Chen, H.
    Sun, Z.
    Li, W. Y.
    MATERIALS CHARACTERIZATION, 2022, 186
  • [35] Effect of Aging Regime on Microstructure and Mechanical Properties of 2195 Al-Li Alloy
    Wang Yun
    Xu Yong
    Xia Liangliang
    Chen Shuaifeng
    Yin Kuo
    Men Xiangnan
    Deng Tao
    Shi-Hong Zhang
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (10) : 3884 - 3891
  • [36] Effect of the aging process and pre-deformation on the precipitated phase and mechanical properties of 2195 Al-Li alloy
    Xie, Bingxin
    Huang, Liang
    Xu, Jiahui
    Su, Hongliang
    Zhang, Huiping
    Xu, Yike
    Li, Jianjun
    Wang, Yu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 832
  • [37] Hot deformation behavior and microstructure characteristic of 2055 Al-Li alloy during uniaxial compression
    Jiang, Dongmei
    Yuan, Changqing
    Li, Xiang
    Yu, Hui
    MATERIALS RESEARCH EXPRESS, 2020, 7 (07)
  • [38] Dynamic microstructural evolution of Al-Cu-Li alloys during hot deformation
    Tang, Ya
    Xiao, Daihong
    Huang, Lanping
    You, Renxuan
    Zhao, Xinyue
    Lin, Nan
    Ma, Yunzhu
    Liu, Wensheng
    MATERIALS CHARACTERIZATION, 2022, 191
  • [39] Processing and performance of electromagnetic deformation combined with heat treatment of 2195 Al-Li alloy
    Xu, J. H.
    Huang, L.
    Xie, B. X.
    Li, J. J.
    19TH INTERNATIONAL CONFERENCE ON METAL FORMING, MF 2022, 2022, 1270
  • [40] Effects of pre-rolling on mechanical properties and fatigue crack growth rate of 2195 Al-Li alloy
    Chen Meng-xi
    Li Yi-bo
    Xia Lin-yan
    Huang Ming-hui
    Wu Zhen-yu
    Yang Yi
    Qu Zi-jing
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2022, 29 (03) : 836 - 847