Laser cladding of Inconel 718 powder on a non-weldable substrate: Clad bead geometry-solidification cracking relationship

被引:54
作者
Alizadeh-Sh, M. [1 ]
Marashi, S. P. H. [1 ]
Ranjbarnodeh, E. [1 ]
Shoja-Razavi, R. [2 ]
机构
[1] Amirkabir Univ Technol, Dept Mat & Met Engn, Tehran, Iran
[2] Malek Ashtar Univ Technol, Fac Mat & Mfg Engn, Tehran, Iran
关键词
Laser cladding; Solidification cracking; A-286; alloy; Inconel; 718; Linear regression analysis; Processing map; Dilution ratio; EMPIRICAL-STATISTICAL MODEL; STAINLESS-STEEL; MICROSTRUCTURAL EVOLUTION; HEAT-TREATMENT; DEPOSITION; OPTIMIZATION; PRECIPITATION; PREDICTION; CORROSION; DILUTION;
D O I
10.1016/j.jmapro.2020.04.045
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present paper addresses the solidification cracking during laser cladding of Inconel 718 powder on A-286 iron based superalloy which is known as hot crack susceptible alloy. Linear regression analysis was performed to propose empirical-statistical correlations between the key processing parameters and the geometrical attributes of single laser clad tracks. These correlations were used in the development of a processing map to study the effects of geometrical characteristics on the solidification cracking and the required conditions to obtain crack-free clads. The solidification cracking of the single clad tracks was inspected by macrostructural examinations using scanning electron microscopy in backscattered electron mode. The processing map revealed that the dilution ratio is the governing macrostructural attribute to avoid solidification cracking. The role of this macrostructural feature in reducing the susceptibility of fusion zone to solidification cracking is discussed.
引用
收藏
页码:54 / 62
页数:9
相关论文
共 51 条
[1]   A 3D dynamic numerical approach for temperature and thermal stress distributions in multilayer laser solid freeform fabrication process [J].
Alimardani, Masoud ;
Toyserkani, Ehsan ;
Huissoon, Jan P. .
OPTICS AND LASERS IN ENGINEERING, 2007, 45 (12) :1115-1130
[2]   Development of highly hard and corrosion resistant A286 stainless steel through plasma nitrocarburizing process [J].
Alphonsa, J. ;
Raja, V. S. ;
Mukherjee, S. .
SURFACE & COATINGS TECHNOLOGY, 2015, 280 :268-276
[3]  
[Anonymous], 2004, ASM HDB, V6
[4]   An empirical-statistical model for coaxial laser cladding of NiCrAlY powder on Inconel 738 superalloy [J].
Ansari, M. ;
Razavi, R. Shoja ;
Barekat, M. .
OPTICS AND LASER TECHNOLOGY, 2016, 86 :136-144
[5]   A Three-Stage Mechanistic Model for Solidification Cracking During Welding of Steel [J].
Aucott, L. ;
Huang, D. ;
Dong, H. B. ;
Wen, S. W. ;
Marsden, J. ;
Rack, A. ;
Cocks, A. C. F. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (05) :1674-1682
[6]   Dilution and microsegregation in dissimilar metal welds between super austenitic stainless steel and nickel base alloys [J].
Banovic, SW ;
DuPont, JN ;
Marder, AR .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2002, 7 (06) :374-383
[7]   Nd:YAG laser cladding of Co-Cr-Mo alloy on γ-TiAl substrate [J].
Barekat, Masoud ;
Razavi, Reza Shoja ;
Ghasemi, Ali .
OPTICS AND LASER TECHNOLOGY, 2016, 80 :145-152
[8]   Thermal effect on clad dimension for laser deposited Inconel 718 [J].
Bennett, Jennifer L. ;
Wolff, Sarah J. ;
Hyatt, Gregory ;
Ehmann, Kornel ;
Cao, Jian .
JOURNAL OF MANUFACTURING PROCESSES, 2017, 28 :550-557
[9]   Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting [J].
Chauvet, Edouard ;
Kontis, Paraskevas ;
Jaegle, Eric A. ;
Gault, Baptiste ;
Raabe, Dierk ;
Tassin, Catherine ;
Blandin, Jean-Jacques ;
Dendievel, Remy ;
Vayre, Benjamin ;
Abed, Stephane ;
Martin, Guilhem .
ACTA MATERIALIA, 2018, 142 :82-94
[10]   Predicting the geometric form of clad in laser cladding by powder using multiple regression analysis (MRA) [J].
Davim, J. Paulo ;
Oliveira, Carlos ;
Cardoso, A. .
MATERIALS & DESIGN, 2008, 29 (02) :554-557