Fatigue strength for pipes with allowable flaws and design fatigue curve

被引:39
作者
Hasegawa, K [1 ]
Sakata, K [1 ]
Miyazaki, K [1 ]
Kanno, S [1 ]
机构
[1] Hitachi Ltd, Hitachi Engn & Prod Div, Hitachi Works, Hitachi, Ibaraki 3178511, Japan
关键词
fatigue strength; allowable flaw; carbon steel pipe; design fatigue curve; seismic event;
D O I
10.1016/S0308-0161(01)00129-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To evaluate the structural integrity for nuclear power piping systems, low cycle fatigue tests were performed on 4 in. diameter carbon steel pipes with flaws. The flaws are local wall thinning, taking into account the minimum wall thickness required for design pressure and circumferentially part-through cracks based on the acceptance standards in the ASME Code Section XI. The applied load was four-point bending with or without an internal pressure under displacement-control led conditions at ambient temperature. The results show that the flaws above do not influence the integrity of the piping system and pipes do not break within the seismic regime of stress and cycles. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:37 / 44
页数:8
相关论文
共 6 条
[1]  
HEALD JD, 1974, J PRESS VESSEL T AUG
[2]  
KOBAYASHI H, 2000, ASME PVP, V407, P153
[3]  
MAYFIELD ME, 1979, ASME PRESS VESS PIP
[4]  
MIYAZAKI M, 1996, ASME PVP, V1, P241
[5]  
POOLE AB, 1993, ORNLNPR9264
[6]  
SCOTT PM, 1995, ASME PVP, V306, P129