Influence of Cr on the oxidation of Fe3Al and Ni3Al at 500°C

被引:17
作者
Velon, A [1 ]
Yi, DQ [1 ]
机构
[1] Chalmers Univ Technol, Dept Engn Met, S-41296 Gothenburg, Sweden
来源
OXIDATION OF METALS | 2002年 / 57卷 / 1-2期
关键词
aluminides; Ni3Al; Fe3Al; dry air; Cr; high-temperature oxidation;
D O I
10.1023/A:1013386427567
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The influence of chromium on the mechanical properties of the aluminides Fe3Al and Ni3Al has been studied extensively. In order to evaluate the role of Cr during the early stages of oxidation, Fe3Al and Ni3Al containing 2 and 4 at.% Cr were oxidized in dry air at 500degreesC for 6, 50, and 100 hr. The oxide scale on Fe3Al consists of a layer of Fe2O3 mixed with FeAl2O4 on top of a continuous layer of (Al, Cr)(2)O-3. Ni3Al is covered with a mixed layer of (Al, Cr)(2)O-3 and NiO/NiAl2O4 underneath a layer of NiO/NiAl2O4. Moreover, Cr induces the nucleation and growth of Fe2O3 and NiO particles at the oxide surface of Fe3Al and Ni3Al, respectively. This is due to enhanced cationic diffusion through the Cr-modified oxides. As a conclusion, additions of Cr zip to 4 at.% are detrimental to the oxidation behavior of both aluminides at 500degreesC.
引用
收藏
页码:13 / 31
页数:19
相关论文
共 29 条
[1]   DUCTILIZATION OF L12 INTERMETALLIC COMPOUND NI3AL BY MICROALLOYING WITH BORON [J].
AOKI, K .
MATERIALS TRANSACTIONS JIM, 1990, 31 (06) :443-448
[2]   THE OXIDATION BEHAVIOR OF NIAL .1. PHASE-TRANSFORMATIONS IN THE ALUMINA SCALE DURING OXIDATION OF NIAL AND NIAL-CR ALLOYS [J].
BRUMM, MW ;
GRABKE, HJ .
CORROSION SCIENCE, 1992, 33 (11) :1677-&
[3]   THE OXIDATION SULFIDATION BEHAVIOR OF IRON-ALLOYS CONTAINING 16-40 AT-DEGREES ALUMINUM [J].
DEVAN, JH ;
TORTORELLI, PF .
CORROSION SCIENCE, 1993, 35 (5-8) :1065-1071
[4]  
DEVAN JH, 1990, P 1 INT C U CAMBR UK, P169
[5]   EFFECTS OF MOLYBDENUM, TITANIUM AND SILICON ADDITIONS ON THE DO3 REVERSIBLE B2 TRANSITION-TEMPERATURE FOR ALLOYS NEAR FE3AL [J].
FORTNUM, RT ;
MIKKOLA, DE .
MATERIALS SCIENCE AND ENGINEERING, 1987, 91 :223-231
[6]   EFFECTS OF CHROMIUM ON CRACK-GROWTH AND OXIDATION IN NICKEL ALUMINIDE [J].
HIPPSLEY, CA ;
STRANGWOOD, M ;
DEVAN, JH .
ACTA METALLURGICA ET MATERIALIA, 1990, 38 (12) :2393-2410
[7]  
HUANG SC, 1984, ACTA METALL, V32, P1073
[8]   High temperature corrosion behaviour of a new Ni-30Fe-10Al-Cr-alloy [J].
Klower, J ;
Sauthoff, G .
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1997, 48 (08) :489-498
[9]   MICROSTRUCTURE AND MECHANICAL-PROPERTIES OF FE3AL ALLOYS WITH CHROMIUM [J].
KNIBLOE, JR ;
WRIGHT, RN ;
TRYBUS, CL ;
SIKKA, VK .
JOURNAL OF MATERIALS SCIENCE, 1993, 28 (08) :2040-2048
[10]  
Kofstad P., 1988, HIGH TEMPERATURE COR, P389