摘要
The forming properties of aluminium alloys are comparatively low, and consequently the forming processes turn out to be difficult. To reduce these problems, a process that optimizes the drawability of aluminium alloys was developed. By a laser-induced pre-treatment, the material properties are locally changed so that influencing of the material flow is possible. For hardenable aluminium alloys the laser-induced heat treatment results in a dissolution of the precipitations, i.e. a conversion from the stable naturally aged T4 to the unstable solution heat treated W-condition of the material. This leads to a reduction of the local flow stress. Using this softening of the material in the outer zone of deep drawing blanks, an increase of the limiting drawing ratio from 2.1 to 2.6 is possible for the alloy AA 6181 A. One interesting feature of this method is that after 1000 h at room temperature, the microstructural changes are recovered. For use in automotive lightweight constructions, this means weight optimized car body panels that can be produced in fewer process steps. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:127 / 132
页数:6
相关论文
共 50 条
[21]   Characteristic of weld line movements for the deep drawing with drawbeads of tailor-welded blanks [J].
Heo, YM ;
Choi, YH ;
Kim, HY ;
Seo, DY .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 111 (1-3) :164-169
[22]   Effects of weld line in deep drawing of tailor welded blanks of high strength steels [J].
Mennecart, Thomas ;
Guner, Alper ;
Ben Khalifa, Nooman ;
Tekkaya, A. Erman .
MATERIAL FORMING ESAFORM 2014, 2014, 611-612 :955-962
[23]   Limiting drawing ratio and deep drawing behavior of dual phase steel tailor welded blanks: FE simulation and experimental validation [J].
Bandyopadhyay, K. ;
Panda, S. K. ;
Saha, P. ;
Padrnanabham, G. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 217 :48-64
[24]   Evaluation of drawing force by a new dimensionless method in deep drawing process [J].
Hajiahmadi, Saeed ;
Elyasi, Majid ;
Shakeri, Mohsen .
PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2020, 234 (13) :1604-1614
[25]   Influence of anisotropy parameter on deep drawing of tailor welded blanks of low-carbon steels [J].
Vasudevan, Vysakh ;
Bandyopadhyay, Kaushik ;
Panda, Sushanta K. .
PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART B-JOURNAL OF ENGINEERING MANUFACTURE, 2014, 228 (09) :1162-1171
[26]   Reduction of Wrinkling Defect in Deep Drawing Process [J].
Kumaravel, D. ;
Venkatesh, K. .
ADVANCES IN MANUFACTURING PROCESSES, ICEMMM 2018, 2019, :133-139
[27]   Factors affecting the deep drawing process - A review [J].
Tiwari, Pushkar R. ;
Rathore, Akshay ;
Bodkhe, Mohan G. .
MATERIALS TODAY-PROCEEDINGS, 2022, 56 :2902-2908
[28]   A novel approach to the conventional deep drawing process [J].
Kabakci, Mehmet Okan ;
Karaagac, Ibrahim ;
Demirel, Mehmet Yasin .
PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART E-JOURNAL OF PROCESS MECHANICAL ENGINEERING, 2023, 237 (02) :280-289
[29]   An application of ultrasonic vibration to the deep drawing process [J].
Jimma, T ;
Kasuga, Y ;
Iwaki, N ;
Miyazawa, O ;
Mori, E ;
Ito, K ;
Hatano, H .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1998, 80-1 :406-412
[30]   Sensor integration for process control in deep drawing [J].
Jung, Robert Oliver ;
Seper, Christoph ;
Juricek, Christian ;
Bleicher, Friedrich .
MATERIAL FORMING, ESAFORM 2024, 2024, 41 :1399-1407