Formation of cationic silicon clusters in a remote silane plasma and their contribution to hydrogenated amorphous silicon film growth

被引:73
作者
Kessels, WMM [1 ]
Leewis, CM [1 ]
van de Sanden, MCM [1 ]
Schram, DC [1 ]
机构
[1] Eindhoven Univ Technol, Dept Appl Phys, NL-5600 MB Eindhoven, Netherlands
关键词
D O I
10.1063/1.371324
中图分类号
O59 [应用物理学];
学科分类号
摘要
The formation of cationic silicon clusters SinHm+ by means of ion-molecule reactions in a remote Ar-H-2-SiH4 plasma is studied by a combination of ion mass spectrometry and Langmuir probe measurements. The plasma, used for high growth rate deposition of hydrogenated amorphous silicon (a-Si:H), is based on SiH4 dissociation in a downstream region by a thermal plasma source created Ar-H-2 plasma. The electron temperature, ion fluence, and most abundant ion emanating from this plasma source are studied as a function of H-2 admixture in the source. The electron temperature obtained is in the range of 0.1-0.3 eV and is too low for electron induced ionization. The formation of silicon containing ions is therefore determined by charge transfer reactions between ions emanating from the plasma source and SiH4. While the ion fluence from the source decreases by about a factor of 40 when a considerable flow of H-2 is admixed in the source, the flux of cationic silicon clusters towards the substrate depends only slightly on this H-2 flow. This implies a strong dissociative recombination of silicon containing ions with electrons in the downstream region for low H-2 flows and it causes the distribution of the cationic silicon clusters with respect to the silicon atoms present in the clusters to be rather independent of H-2 admixture. The average cluster size increases, however, strongly with the SiH4 flow for constant plasma source properties. Moreover, it leads to a decrease of the ion beam radius and due to this, to an increase of the ion flux towards the substrate, which is positioned in the center of the beam. Assuming unity sticking probability the contribution of the cationic clusters to the total growth flux of the material is about 6% for the condition in which solar grade a-Si:H is deposited. Although the energy flux towards the film by ion bombardment is limited due to the low electron temperature, the clusters have a very compact structure and very low hydrogen content and can consequently have a considerable impact on film quality. The latter is discussed as well as possible implications for other (remote) SiH4 plasmas. (C) 1999 American Institute of Physics. [S0021-8979(99)00319-9].
引用
收藏
页码:4029 / 4039
页数:11
相关论文
共 50 条
  • [1] FILM FORMATION MECHANISMS IN THE PLASMA DEPOSITION OF HYDROGENATED AMORPHOUS-SILICON
    TSAI, CC
    KNIGHTS, JC
    CHANG, G
    WACKER, B
    JOURNAL OF APPLIED PHYSICS, 1986, 59 (08) : 2998 - 3001
  • [2] Surface reaction probability during fast deposition of hydrogenated amorphous silicon with a remote silane plasma
    Kessels, WMM
    van de Sanden, MCM
    Severens, RJ
    Schram, DC
    JOURNAL OF APPLIED PHYSICS, 2000, 87 (07) : 3313 - 3320
  • [4] Effect of film thickness on hydrogenated amorphous silicon grown with hydrogen diluted silane
    Danesh, P
    Pantchev, B
    Grambole, D
    Schmidt, B
    APPLIED PHYSICS LETTERS, 2002, 80 (14) : 2463 - 2465
  • [5] THE PRESENCE OF SILANE GAS IN PLASMA-DEPOSITED HYDROGENATED AMORPHOUS-SILICON
    BEKKAY, T
    IZQUIERDO, R
    STDENIS, M
    SACHER, E
    YELON, A
    SURFACE SCIENCE, 1989, 222 (2-3) : L831 - L836
  • [6] Silicon nitride film growth by remote plasma CVD using Tris(dimethylamino)silane
    Aoki, T
    Ogishima, T
    Wróbel, AM
    Nakanishi, Y
    Hatanaka, Y
    VACUUM, 1998, 51 (04) : 747 - 750
  • [7] Lower-temperature growth of hydrogenated amorphous silicon films from inductively coupled silane plasma
    Nagoya Univ, Nagoya, Japan
    Jpn J Appl Phys Part 2 Letter, 8 A (L1009-L1011):
  • [8] Lower-temperature growth of hydrogenated amorphous silicon films from inductively coupled silane plasma
    Goto, M
    Toyoda, H
    Kitagawa, M
    Hirao, T
    Sugai, H
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1996, 35 (8A): : L1009 - L1011
  • [9] Improvement of hydrogenated amorphous silicon properties with increasing contribution of SiH3 to film growth
    Kessels, WMM
    Boogaarts, MGH
    Hoefnagels, JPM
    Schram, DC
    van de Sanden, MCM
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 2001, 19 (03): : 1027 - 1029
  • [10] Hydrogenated amorphous silicon thin film transistor fabricated on plasma treated silicon nitride
    Lim, Byung Cheon
    Choi, Young Jin
    Choi, Jong Hyun
    Jang, Jin
    2000, IEEE, Piscataway, NJ, United States (47)