SON68 nuclear glass dissolution kinetics: Current state of knowledge and basis of the new GRAAL model

被引:290
作者
Frugier, P. [1 ]
Gin, S. [1 ]
Minet, Y. [1 ]
Chave, T. [1 ]
Bonin, B. [2 ]
Godon, N. [1 ]
Lartigue, J. -E. [1 ]
Jollivet, P. [1 ]
Ayral, A. [3 ]
De Windt, L. [4 ]
Santarini, G. [5 ]
机构
[1] CEA Marcoule, DTCD, SECM, LCLT, F-30207 Bagnols Sur Ceze, France
[2] CEA Saclay, DEN, DIR, DS, F-91191 Gif Sur Yvette, France
[3] Univ Montpellier 2, CNRS, IEM, ENSCM, F-34095 Montpellier 5, France
[4] ENSMP, F-77305 Fontainebleau, France
[5] CEA Saclay, HC, CAB, F-91191 Gif Sur Yvette, France
关键词
D O I
10.1016/j.jnucmat.2008.06.044
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This article summarizes the present state of knowledge concerning aqueous alteration of R7T7-type nuclear containment glasses, represented mainly by the inactive reference glass designated SON68. Based on this review, we propose to describe the glass alteration kinetics up to and including the final residual rate regime by means of a new mechanistic model known as GRAAL (glass reactivity with allowance for the alteration layer). Phenomenological analysis findings are reviewed for the various glass alteration regimes: interdiffusion, initial rate, rate drop, residual rate and, under very particular circumstances, resumption of alteration. These alteration regimes are associated with predominant mechanisms. Published work interpreting and modeling these mechanisms was examined in detail. There is a broad consensus on the general mechanisms of the initial rate and even the interdiffusion regime, whereas the mechanisms controlling the rate drop remain a subject of dispute not only with regard to nuclear glasses but also for the dissolution of silicate minerals. The reaction affinity responsible for the rate drop is expressed differently by different authors and depending on the underlying theories. The disagreement concerns the nature of the phase (glass or gel) or the activated complex controlling the rate drop, which in turn determines the elements that must be taken into account in the overall affinity term. Progress in recent years, especially in identifying the mechanisms responsible for the residual rate, has shed new light on these issues, allowing us to propose new theoretical foundations for modeling the different kinetic regimes of SON68 nuclear glass dissolution. The GRAAL model considers that water diffusion in the passivating reaction zone (the gel formed under saturation conditions) is a rate-limiting step in the overall glass dissolution kinetics. Moreover, this passivation zone is a soluble phase whose stability is directly dependent on the nature of the secondary phases likely to precipitate and on the solution renewal conditions. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:8 / 21
页数:14
相关论文
共 69 条
[1]   THERMODYNAMIC AND KINETIC CONSTRAINTS ON REACTION-RATES AMONG MINERALS AND AQUEOUS-SOLUTIONS .1. THEORETICAL CONSIDERATIONS [J].
AAGAARD, P ;
HELGESON, HC .
AMERICAN JOURNAL OF SCIENCE, 1982, 282 (03) :237-285
[2]  
ADVOCAT T, 1991, MATER RES SOC SYMP P, V212, P57, DOI 10.1557/PROC-212-57
[3]  
Advocat T., 1995, Scientific Basis for Nuclear Waste Management XVII. Symposium, P31
[4]   Influence of glass composition and alteration solution on leached silicate glass structure: A solid-state NMR investigation [J].
Angeli, Frederic ;
Gaillard, Marina ;
Jollivet, Patrick ;
Charpentier, Thibault .
GEOCHIMICA ET COSMOCHIMICA ACTA, 2006, 70 (10) :2577-2590
[5]  
Arab M, 2007, MATER RES SOC SYMP P, V985, P193
[6]  
BOKSAY Z, 1968, PHYS CHEM GLASSES, V9, P69
[7]  
Bourcier W., 1992, WAT INT VOLS 1 2, P81
[8]  
BOURCIER WL, 1990, SCI BASIS NUCL WASTE, V176, P209
[9]   MOLECULAR MECHANISMS FOR CORROSION OF SILICA AND SILICATE-GLASSES [J].
BUNKER, BC .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1994, 179 :300-308
[10]  
CAILLETEAU C, 2007, 21 INT C GLASS ICG20