Measurement of debonding in cracked nanocomposite films by ultrasonic force microscopy

被引:33
作者
McGuigan, AP
Huey, BD
Briggs, GAD
Kolosov, OV
Tsukahara, Y
Yanaka, M
机构
[1] Univ Oxford, Dept Mat, Oxford OX1 3PH, England
[2] Toppan Printing Co Ltd, Toppan Res Inst, Sugito, Saitama 3458508, Japan
关键词
D O I
10.1063/1.1450058
中图分类号
O59 [应用物理学];
学科分类号
摘要
This letter reports the application of ultrasonic force microscopy (UFM) to investigate subsurface fracture mechanisms during tensile loading of nanocomposite films consisting of a brittle glass on a ductile polyethylene terephthalate (PET) substrate. Such materials are used in packaging applications where a gas barrier is required to maintain the product quality. Cracking or debonding of the surface glass layer results in destruction of the gas barrier properties of the film. Accurate evaluation of the continuity or discontinuity at the crack edge within the layered material is crucial for the correct characterization of both adhesive failure and crack propagation. Here simultaneous atomic force microscopy and UFM images are compared for a range of tensile strains to identify debonded regions of the glass film from the PET. Debonding occurred for strains greater than 6%. In some films, this debonding increased with applied strain. (C) 2002 American Institute of Physics.
引用
收藏
页码:1180 / 1182
页数:3
相关论文
共 13 条
[1]   ATOMIC-FORCE MICROSCOPY AND PERMEABILITY STUDY OF STRETCHING-INDUCED GAS BARRIER LOSS OF ALOX LAYERS [J].
BARKER, CP ;
KOCHEM, KH ;
REVELL, KM ;
KELLY, RSA ;
BADYAL, JPS .
THIN SOLID FILMS, 1995, 259 (01) :46-52
[2]  
DEGRVSE R, 1997, 11 INT C VAC WEB COA, P16
[3]   Mapping surface elastic properties of stiff and compliant materials on the nanoscale using ultrasonic force microscopy [J].
Dinelli, F ;
Castell, MR ;
Ritchie, DA ;
Mason, NJ ;
Briggs, GAD ;
Kolosov, OV .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 2000, 80 (10) :2299-2323
[4]   Imaging the elastic nanostructure of Ge islands by ultrasonic force microscopy [J].
Kolosov, OV ;
Castell, MR ;
Marsh, CD ;
Briggs, GAD ;
Kamins, TI ;
Williams, RS .
PHYSICAL REVIEW LETTERS, 1998, 81 (05) :1046-1049
[5]   Thermodynamic and micromechanical approaches to the adhesion between polyethylene terephthalate and silicon oxide [J].
Leterrier, Y ;
Sutter, P ;
Månson, JAE .
JOURNAL OF ADHESION, 1999, 69 (1-2) :13-30
[6]  
LETERRIER Y, 1999, P DURACOSYS 99 BRUSS, P11
[7]  
MCGUIGAN AP, UNPUB THIN SOLID FIL
[8]  
Poulingue M., 1998, P SOC PHOTO-OPT INS, V3578, P370
[9]  
SAKAMAKI C, 1982, P 6 INT C VAC WEB CO, P85
[10]   Cracking and loss of adhesion of Si3N4 and SiO2:P films deposited on Al substrates [J].
Scafidi, P ;
Ignat, M .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1998, 12 (11) :1219-1242