Effect of different disinfectant methods on the initial microtensile bond strength of a self-etch adhesive to dentin

被引:23
|
作者
Dalkilic, Evrim Eliguzeloglu [1 ]
Arisu, Hacer Deniz [2 ]
Kivanc, Bagdagul Helvacioglu [3 ]
Uctasli, Mine Betul [2 ]
Omurlu, Huma [2 ]
机构
[1] Yuzuncu Yil Univ, Dept Restorat Dent, Fac Dent, TR-65080 Van, Turkey
[2] Gazi Univ, Dept Restorat Dent, Fac Dent, TR-06500 Ankara, Turkey
[3] Gazi Univ, Dept Endodont, Fac Dent, TR-06500 Ankara, Turkey
关键词
Ozone; Nd:YAG laser; Microtensile; Bond strength; Chlorhexidine; NDYAG LASER IRRADIATION; CARIOUS DENTIN; YAG LASER; IN-VITRO; OZONE; ENAMEL; CARIES; RESTORATIONS; SYSTEMS; CHLORHEXIDINE;
D O I
10.1007/s10103-011-0987-x
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The aim of this in vitro study was to evaluate the effect of different disinfection methods on the initial microtensile bond strength of a two-step, self-etch adhesive to dentin. Twenty mandibular molars were sectioned parallel to the occlusal plane to expose the mid-coronal dentin. All of the teeth were divided into four groups (n = 5 per group): (1) in group OZ, the dentin surfaces were exposed to ozone gas from the Ozonytron X delivery system (OzonyTron X-Bioozonix, Munich, Germany), (2) in group ND, the dentin surfaces were irradiated with an Nd:YAG laser (Pulsmaster 600 IQ, American Dental Technologies, U.S.), (3) in group CHX, the dentin surfaces were treated with a 2% chlorhexidine solution, and (4) in the control group, no treatment was applied. In all of the groups, the teeth were restored with Clearfil SE Bond (Kuraray, Tokyo, Japan) and Clearfil Majesty Posterior (Kuraray, Tokyo, Japan), according to the manufacturer's instructions. The teeth were sectioned perpendicular to the bonded surface (surface area of approximately 1 mm(2)). Thus, six to seven specimens were obtained from each tooth, and a total of 34 specimens were analyzed in each group. The specimens were attached to the microtensile test machine (Micro Tensile Tester, T-61010 K, Bisco, U.S.). The data was analyzed using the one-way analysis of variance (ANOVA) and Tukey test (p < 0.05). Fracture modes of each specimen were determined using a stereomicroscope (SZ-PT Olympus, Tokyo, Japan) and a scanning electron microscope (SEM). The lowest bond strength occurred in the OZ group. Significant differences were determined only between group OZ and the other groups (group ND, group CHX, and control group) (p < 0.05). In conclusion, although ozone decreased the microtensile bond strength of the self-etch adhesive system to dentin, the Nd:YAG laser and 2% chlorhexidine did not change the microtensile bond strength so in context of the present study it would appear that the Nd:YAG laser and 2% chlorhexidine may be used as pre-restorative sterilization procedures on the dentin prior to the application of a two-step, self-etch adhesive.
引用
收藏
页码:819 / 825
页数:7
相关论文
共 50 条
  • [41] The effect of warm air-blowing on the microtensile bond strength of one-step self-etch adhesives to root canal dentin
    Taguchi, Keita
    Hosaka, Keiichi
    Ikeda, Masaomi
    Kishikawa, Ryuzo
    Foxton, Richard
    Nakajima, Masatoshi
    Tagami, Junji
    JOURNAL OF PROSTHODONTIC RESEARCH, 2018, 62 (03) : 330 - 336
  • [42] Bond strength of composite to dentin: effect of acid etching and laser irradiation through an uncured self-etch adhesive system
    Castro, F. L. A.
    Carvalho, J. G.
    Andrade, M. F.
    Saad, J. R. C.
    Hebling, J.
    Lizarelli, R. F. Z.
    LASER PHYSICS, 2014, 24 (08)
  • [43] Influence of pulpotomy medicaments on the ultrastructure and shear bond strength of a self-etch adhesive to primary tooth dentin
    Shalan, Hanaa
    Awad, Salwa
    El-Fallal, Abeer Abd-El Sallam
    QUINTESSENCE INTERNATIONAL, 2012, 43 (06): : 517 - 523
  • [44] THE EFFECT OF DENTIN PRETREATMENT ON THE MICROTENSILE BOND STRENGTH OF SELF-ADHESIVE RESIN CEMENTS
    Pavan, Sabrina
    dos Santos, Paulo H.
    Berger, Sandrine
    Bedran-Russo, Ana Karina B.
    JOURNAL OF PROSTHETIC DENTISTRY, 2010, 104 (04): : 258 - 264
  • [45] Effect of Galardin and its Solvents on the Microtensile Bond Strength of Different Adhesive Systems to Dentin
    Chaharom, Mohammad Esmaeel Ebrahimi
    Bahari, Mahmoud
    Rahbar, Mahdi
    Golbaz, Sepideh
    PESQUISA BRASILEIRA EM ODONTOPEDIATRIA E CLINICA INTEGRADA, 2019, 19 (01):
  • [46] Effect of Exclusive Primer and Adhesive on Microtensile Bond Strength of Self-Adhesive Resin Cement to Dentin
    Kim, Bit-Na
    Son, Sung-Ae
    Park, Jeong-Kil
    MATERIALS, 2020, 13 (10)
  • [47] Enzymatic degradation of adhesive-dentin interfaces produced by mild self-etch adhesives
    De Munck, Jan
    Mine, Atsushi
    Van den Steen, Philippe E.
    Van Landuyt, Kirsten L.
    Poitevin, Andre
    Opdenakker, Ghislain
    Van Meerbeek, Bart
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2010, 118 (05) : 494 - 501
  • [48] Impact of Preceded Tumor Therapeutic Irradiation on the Microtensile Bond Strength of Universal Adhesives Applied in Self-Etch Mode to Human Dentin In Vitro
    Broscheit, Sina
    Vordermark, Dirk
    Gerlach, Reinhard
    Gernhardt, Christian Ralf
    APPLIED SCIENCES-BASEL, 2023, 13 (13):
  • [49] Influence of different Er,Cr:YSGG laser parameters on long-term dentin bond strength of self-etch adhesive
    Yildirim, Tahsin
    Ayar, Muhammet Kerim
    Yesilyurt, Cemal
    LASERS IN MEDICAL SCIENCE, 2015, 30 (09) : 2363 - 2368
  • [50] Modified Microtensile Bond Strength of Glass Ionomer to Composite Resin Using Universal Adhesive in Self-etch and Total-etch Modes
    Kermanshah, Hamid
    Omrani, Ladan R.
    Hemati, Omid
    Pedram, Prham
    Ahmadi, Elham
    OPEN DENTISTRY JOURNAL, 2020, 14 : 390 - 395