Effect of different disinfectant methods on the initial microtensile bond strength of a self-etch adhesive to dentin

被引:23
|
作者
Dalkilic, Evrim Eliguzeloglu [1 ]
Arisu, Hacer Deniz [2 ]
Kivanc, Bagdagul Helvacioglu [3 ]
Uctasli, Mine Betul [2 ]
Omurlu, Huma [2 ]
机构
[1] Yuzuncu Yil Univ, Dept Restorat Dent, Fac Dent, TR-65080 Van, Turkey
[2] Gazi Univ, Dept Restorat Dent, Fac Dent, TR-06500 Ankara, Turkey
[3] Gazi Univ, Dept Endodont, Fac Dent, TR-06500 Ankara, Turkey
关键词
Ozone; Nd:YAG laser; Microtensile; Bond strength; Chlorhexidine; NDYAG LASER IRRADIATION; CARIOUS DENTIN; YAG LASER; IN-VITRO; OZONE; ENAMEL; CARIES; RESTORATIONS; SYSTEMS; CHLORHEXIDINE;
D O I
10.1007/s10103-011-0987-x
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The aim of this in vitro study was to evaluate the effect of different disinfection methods on the initial microtensile bond strength of a two-step, self-etch adhesive to dentin. Twenty mandibular molars were sectioned parallel to the occlusal plane to expose the mid-coronal dentin. All of the teeth were divided into four groups (n = 5 per group): (1) in group OZ, the dentin surfaces were exposed to ozone gas from the Ozonytron X delivery system (OzonyTron X-Bioozonix, Munich, Germany), (2) in group ND, the dentin surfaces were irradiated with an Nd:YAG laser (Pulsmaster 600 IQ, American Dental Technologies, U.S.), (3) in group CHX, the dentin surfaces were treated with a 2% chlorhexidine solution, and (4) in the control group, no treatment was applied. In all of the groups, the teeth were restored with Clearfil SE Bond (Kuraray, Tokyo, Japan) and Clearfil Majesty Posterior (Kuraray, Tokyo, Japan), according to the manufacturer's instructions. The teeth were sectioned perpendicular to the bonded surface (surface area of approximately 1 mm(2)). Thus, six to seven specimens were obtained from each tooth, and a total of 34 specimens were analyzed in each group. The specimens were attached to the microtensile test machine (Micro Tensile Tester, T-61010 K, Bisco, U.S.). The data was analyzed using the one-way analysis of variance (ANOVA) and Tukey test (p < 0.05). Fracture modes of each specimen were determined using a stereomicroscope (SZ-PT Olympus, Tokyo, Japan) and a scanning electron microscope (SEM). The lowest bond strength occurred in the OZ group. Significant differences were determined only between group OZ and the other groups (group ND, group CHX, and control group) (p < 0.05). In conclusion, although ozone decreased the microtensile bond strength of the self-etch adhesive system to dentin, the Nd:YAG laser and 2% chlorhexidine did not change the microtensile bond strength so in context of the present study it would appear that the Nd:YAG laser and 2% chlorhexidine may be used as pre-restorative sterilization procedures on the dentin prior to the application of a two-step, self-etch adhesive.
引用
收藏
页码:819 / 825
页数:7
相关论文
共 50 条
  • [31] One-year evaluation of microtensile bond strength of universal adhesives in Self-etch or Etch and Rinse modes to dentin groups at different caries-affected degree
    Tuncer, Nurgul Cetin
    Barutcugil, Cagatay
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2025, 138
  • [32] Dentin-smear remains at self-etch adhesive interface
    Mine, Atsushi
    De Munck, Jan
    Cardoso, Marcio Vivan
    Van Landuyt, Kirsten L.
    Poitevin, Andre
    Van Ende, Annelies
    Matsumoto, Mariko
    Yoshida, Yasuhiro
    Kuboki, Talmo
    Yatani, Hirofumi
    Van Meerbeek, Bart
    DENTAL MATERIALS, 2014, 30 (10) : 1147 - 1153
  • [33] Effect of sonic application mode on the resin-dentin bond strength and nanoleakage of simplified self-etch adhesive
    Mena-Serrano, Alexandra
    Garcia, Eugenio Jose
    Loguercio, Alessandro Dourado
    Reis, Alessandra
    CLINICAL ORAL INVESTIGATIONS, 2014, 18 (03) : 729 - 736
  • [34] Effects of Desensitizers, Temporary Cements, and Dentin Cleaning Methods on the Bond Strength of Self-Etch/Adhesive Resin Cements to Dentin: An In Vitro Study
    Ugur, Mehmet
    Kavut, Idris
    Kulunk, Safak
    Akdeniz, Mehmet Serif
    Tanrikut, Ozgur Ozan
    JOURNAL OF ADVANCED ORAL RESEARCH, 2022, 13 (01) : 97 - 104
  • [35] The effect of dentin desensitizers, and Nd:YAG laser pre-treatment on microtensile bond strength of self-adhesive resin cement to dentin
    Acar, Ozlem
    Tuncer, Duygu
    Yuzugullu, Bulem
    Celik, Cigdem
    JOURNAL OF ADVANCED PROSTHODONTICS, 2014, 6 (02): : 88 - 95
  • [36] Effect of acid etching on dentin bond strength of ultra-mild self-etch adhesives
    Elkaffas, Ali A.
    Hamama, Hamdi H.
    Mahmoud, Salah H.
    Fawzy, Amr S.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2020, 99
  • [37] Influence of dentin biomodification with epigallocatechin-3-gallate on the bond strength of self-etch adhesive: Twelve-month results
    Neri, Jiovanne R.
    Yamauti, Monica
    da Silveira, Felipe D.
    Mendonca, Juliano S.
    de Carvalho, Ricardo M.
    Santiago, Sergio L.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2016, 71 : 81 - 86
  • [38] Effect of Configuration Factor on Shear Bond Strengths of Self-etch Adhesive Systems to Ground Enamel and Dentin
    Mcleod, M. E.
    Price, R. B. T.
    Felix, C. M.
    OPERATIVE DENTISTRY, 2010, 35 (01) : 84 - 93
  • [39] Effect of Alternative Self-Etch Applications on Dentin Bond Strength of "No Wait Concept" Universal Adhesives
    Serin-Kalay, Tugba
    Zaim, Beyza
    ODOVTOS INTERNATIONAL JOURNAL OF DENTAL SCIENCES, 2022, 24 (01) : 58 - 66
  • [40] The Effect of Endodontic Irrigants on the Microtensile Bond Strength of Different Dentin Adhesives
    Dikmen, B.
    Tarim, B.
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2018, 21 (03) : 280 - 286