摘要
The surface cracks of 40Cr bars produced by Henan Jiyuan Iron & Steel (GROUP) CO., LTD are investigated by sampling, examining and analyzing, and the reason for surface cracking in the bar is also verified. The results indicate that the contents of silicate nonmetallic inclusion exceed the allowable levels. Combining with productive process, it can be concluded that the silicate nonmetallic inclusion, carbon segregation as well as high drawing speed at the process of continuous casting are the reason for the surface cracking of 40Cr bar. The emergence of surface cracks can be controlled effectively with series measures, such as improving the quality of molten steel smelting, strengthening the test of the top slag and reforming the corresponding equipments, and so on, then the percent defective of steel could be decreased from 0.68% to 0.35%.
引用
收藏
页码:16 / 19
页数:4
相关论文
共 50 条
  • [31] Low temperature superplasticity of 40Cr steel
    Xu, XJ
    Shi, LJ
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2004, 11 (04) : 56 - 58
  • [32] Research on the Forging Penetration Efficiency of 40Cr Axial Forging by the Simulation of Dynamic Recrystallization
    Tong, Ying
    FRONTIERS OF MANUFACTURING SCIENCE AND MEASURING TECHNOLOGY, PTS 1-3, 2011, 230-232 : 315 - 319
  • [33] 40Cr整体飞轮开裂原因分析
    杜昌忠
    王春奕
    王建元
    张全新
    物理测试, 2021, 39 (06) : 6 - 10
  • [34] 40Cr热处理工艺剖析
    战中学
    刘泽林
    刘国忠
    李海豹
    宋亚辉
    郑宏伟
    中国高新技术企业, 2014, (06) : 42 - 44
  • [35] 齿轮(40Cr)中频淬火工艺研究
    柴宾元
    水力采煤与管道运输, 2003, (02) : 35 - 36
  • [36] 40Cr钢主轴开裂原因分析
    闾宏
    贺凯林
    陈辉
    彭君建
    热处理, 2021, 36 (04) : 42 - 43+46
  • [37] 40Cr 压下螺杆破断分析
    黄福祥
    材料工程, 1997, (11) : 47 - 49
  • [38] 40Cr高强螺栓断裂原因分析
    牛禧
    张睿
    许先果
    热加工工艺, 2012, 41 (20) : 217 - 218+222
  • [39] Laser surface alloying of 40Cr steel with carbon
    Wei, Lun
    Chen, Qinghua
    Li, Junchang
    Long, Jinming
    Chen, Juncai
    Jiguang Jishu/Laser Technology, 2002, 26 (01):
  • [40] Analysis and modeling of flow stress of 40Cr steel
    Li, Xiong
    Zhang, Hong-Bing
    Ruan, Xue-Yu
    Luo, Zhong-Hua
    Zhang, Yan
    Cailiao Gongcheng/Journal of Materials Engineering, 2004, (11): : 41 - 44