Aging behavior and delamination in cold drawn and post-deformation annealed hyper-eutectoid steel wires

被引:33
作者
Joung, S. W. [1 ]
Kang, U. G. [1 ]
Hong, S. P. [2 ]
Kim, Y. W. [2 ]
Nam, W. J. [1 ]
机构
[1] Kookmin Univ, Sch Adv Mat Engn, Seoul 136702, South Korea
[2] Seoul Natl Univ, Dept Mat Sci & Engn, Seoul 151742, South Korea
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2013年 / 586卷
基金
新加坡国家研究基金会;
关键词
Annealing; Aging; Pearlite; Cementite; Delamination; PEARLITIC STEELS; CEMENTITE DECOMPOSITION; ATOM-PROBE; MICROSTRUCTURE; TEMPERATURE; DISSOLUTION; MECHANISMS; EVOLUTION;
D O I
10.1016/j.msea.2013.07.095
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of drawing strains and post-deformation annealing conditions on the aging behavior and the occurrence of delamination in cold drawn hyper-eutectoid steel wires were studied. At low annealing temperatures the increased tensile strength for a short annealing time would be attributed to age hardening, which came from the decomposition of the unstable cementite in deformed pearlite. The decrease of tensile strength at the high annealing temperature was due to age softening, which would be attributed to the decreased carbon content in lamellar ferrite through the spheroidization or the re-precipitation of cementite, and recovery or recrystallization of ferrite. The extent for the occurrence of delamination during annealing expanded to the high temperature region with the increased amount of deformation in steel wires. At high annealing temperatures, the decreased carbon content dissolved in lamellar ferrite due to age softening would result in the decrease of tensile strength and suppress the occurrence of delamination. The total magnitude of carbon content dissolved in lamellar ferrite either by the partial dissolution of lamellar cementite during wire drawing or by the partial decomposition of lamellar cementite during post-deformation annealing would control the occurrence of delamination in cold drawn steel wires. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:171 / 177
页数:7
相关论文
共 24 条
[1]   Direct evidence of cementite dissolution in drawn pearlitic steels observed by tomographic atom probe [J].
Danoix, F ;
Julien, D ;
Sauvage, X ;
Copreaux, J .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 250 (01) :8-13
[2]   Revealing microstructural and mechanical characteristics of cold-drawn pearlitic steel wires undergoing simulated galvanization treatment [J].
Fang, Feng ;
Hu, Xian-jun ;
Chen, Shao-hui ;
Xie, Zong-han ;
Jiang, Jian-qing .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 547 :51-54
[3]   Measurement of dynamic strain aging in pearlitic steels by tensile test [J].
Gonzalez, BM ;
Marchi, LA ;
da Fonseca, EJ ;
Modenesi, PJ ;
Buono, VTL .
ISIJ INTERNATIONAL, 2003, 43 (03) :428-432
[4]  
GRIDNEV VN, 1982, PHYS MET+, V4, P531
[5]   Atom probe and transmission electron microscopy investigations of heavily drawn pearlitic steel wire [J].
Hong, MH ;
Hono, K ;
Reynolds, WT ;
Tarui, T .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (03) :717-727
[6]   Cementite decomposition in heavily drawn pearlite steel wire [J].
Hono, K ;
Ohnuma, M ;
Murayama, M ;
Nishida, S ;
Yoshie, A ;
Takahashi, T .
SCRIPTA MATERIALIA, 2001, 44 (06) :977-983
[7]  
HOSFORD WF, 1964, T METALL SOC AIME, V230, P12
[8]  
Kanetsuki Y., 1981, P 6 INT C TEXT MAT I, P1127
[9]   Cementite dissolution in heavily cold drawn pearlitic steel wires [J].
Languillaume, J ;
Kapelski, G ;
Baudelet, B .
ACTA MATERIALIA, 1997, 45 (03) :1201-1212
[10]   Effects of post-deformation annealing conditions on the behavior of lamellar cementite and the occurrence of delamination in cold drawn steel wires [J].
Lee, J. W. ;
Lee, J. C. ;
Lee, Y. S. ;
Park, K. T. ;
Nam, W. J. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (12-13) :5300-5304