The role of arsine in the deactivation of methanol synthesis catalysts

被引:25
作者
Quinn, R [1 ]
Mebrahtu, T [1 ]
Dahl, TA [1 ]
Lucrezi, FA [1 ]
Toseland, BA [1 ]
机构
[1] Air Prod & Chem Inc, Adsorpt Technol Ctr, Allentown, PA 18195 USA
关键词
deactivation; Cu/ZnO catalysts; methanol synthesis; arsine; arsenic; X-ray absorption spectroscopy;
D O I
10.1016/j.apcata.2003.12.034
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The liquid phase methanol (LPMEOH((TM))) process is successfully producing methanol from coal-derived synthesis gas on an industrial scale. This process uses a standard copper, zinc oxide, and alumina catalyst suspended in an inert mineral oil in a slurry bubble column reactor. An arsenic-containing species, most reasonably arsine, was found in the feed to the LPMEOH((TM)) commercial demonstration facility located at Eastman Chemical Company's chemicals-from-coal complex in Kingsport, TN. Laboratory testing showed that arsine is, in fact, a powerful methanol synthesis catalyst poison. At levels as low as 150 ppbv, arsine results in a rapid deactivation of the catalyst. Removal of arsine results in a deactivation rate consistent with a clean synthesis gas feeds that is, arsine poisoning stops when it is removed from the feed. We infer that arsine reacts irreversibly with the catalyst under the methanol synthesis conditions. X-ray absorption spectroscopy (XAS) of arsenic-containing used catalyst indicated the presence of zero-valent arsenic in an intermetallic surface phase that is structurally related to Domeykite (Cu(3)As). Experimental evidence, thermodynamics, and literature relating to other metal-arsine chemistry were consistent with dissociative adsorption of arsine on the copper surface to form gaseous H(2) and Cu(3)As. To deal with arsine poisoning, we have developed adsorption technology that can remove arsine to levels low enough that catalyst performance is unaffected. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:103 / 109
页数:7
相关论文
共 19 条
[11]   Arsenic poisoning of nickel catalysts for the adsorption of ethene [J].
Ng, CF ;
Ye, H ;
She, L ;
Chen, H ;
Lai, SY .
APPLIED CATALYSIS A-GENERAL, 1998, 171 (02) :293-299
[12]   ARSINE POISONING OF NICKEL SILICA CATALYSTS - HYDROGEN CHEMISORPTION STUDY BY MAGNETIC METHOD [J].
NG, CF ;
CHANG, YJ .
APPLIED CATALYSIS, 1991, 70 (02) :213-224
[13]   POISONING OF NICKEL-CATALYSTS BY ARSENIC [J].
NIELSEN, B ;
VILLADSEN, J .
APPLIED CATALYSIS, 1984, 11 (01) :123-138
[14]  
*OUT RES, THERM CALC PERF US H
[15]  
Peng XD, 1997, STUD SURF SCI CATAL, V111, P175
[16]   DEACTIVATION OF METHANOL SYNTHESIS CATALYSTS [J].
ROBERTS, GW ;
BROWN, DM ;
HSIUNG, TH ;
LEWNARD, JJ .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1993, 32 (08) :1610-1621
[17]   Surface organometallic chemistry on metals applied to the environment:: Hydrogenolysis of AsPh3 with nickel supported on alumina [J].
Ryndin, YA ;
Candy, JP ;
Didillon, B ;
Savary, L ;
Basset, JM .
JOURNAL OF CATALYSIS, 2001, 198 (01) :103-108
[18]   ADSORPTION AND INCORPORATION ON COPPER [J].
SALEH, JM .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS I, 1972, 68 (08) :1520-&
[19]  
SUBRAMANIAN PR, 1994, PHASE DIAGRAM BINARY