共 21 条
Effects of sealing on corrosion behaviour of plasma-sprayed Cr2O3-8TiO2 coating
被引:26
作者:
Zhang, Jingjing
[1
]
Wang, Zehua
[1
]
Lin, Pinghua
[2
]
机构:
[1] Hohai Univ, Coll Mech & Mat, Nanjing 210098, Jiangsu, Peoples R China
[2] Huazhong Univ Sci & Technol, Wuhan 430078, Peoples R China
基金:
中国国家自然科学基金;
关键词:
Coating;
Plasma-sprayed;
Sealing;
Corrosion;
THERMAL BARRIER COATINGS;
CERAMIC COATINGS;
ALUMINA COATINGS;
WEAR-RESISTANCE;
OXIDE COATINGS;
ENVIRONMENTS;
D O I:
10.1179/1743294413Y.0000000161
中图分类号:
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
Plasma-sprayed Cr2O3-8 wt-% TiO2 coatings were deposited on mild steel and sealed by epoxy resin and silicone resin in different processes. The microstructure and corrosion resistance of all coatings were investigated. The results showed that silicone resin sealant can seal the coating well and 91% of interconnected porosity was blocked. The sealant can penetrate into the coating by more than 280 mu m. The coating sealed with silicone resin in vacuum conditions had the highest corrosion potential E-corr (-375 mV) and lowest corrosion current density i(corr) (17 mA m(-2)) in electrochemical tests. Correspondingly, the unsealed coating had the lowest E-corr and highest i(corr). The corrosion resistance of the coatings was in the following order: coating sealed with silicone resin in vacuum>coating sealed with silicone resin in air. coating sealed with epoxy resin in vacuum>coating sealed with epoxy resin in air. unsealed coating.