Effect of the Basicity on the Crystallization Behavior of Titanium Bearing Blast Furnace Slag

被引:11
作者
Hu Meilong [1 ]
Wei Ruirui [1 ]
Gao Leizhang [1 ]
Liu Lu [1 ]
Bai Chenguang [1 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, 174 Shazheng St, Chongqing 400044, Peoples R China
基金
高等学校博士学科点专项科研基金; 中国国家自然科学基金;
关键词
basicity; cystallization behavior; titanium bearing slag; CLSM; VISCOUS BEHAVIOR; SILICATE MELTS; TIO2; SPECTROSCOPY; REDUCTION; VISCOSITY;
D O I
10.1515/htmp-2016-0058
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Basicity of titanium bearing blast furnace (BF) slag is critical for its crystallization behavior. Thermodynamics calculation indicates that rutile is the main phase after crystallization (or at room temperature). It precipitates during the cooling when the basicity of the slag is lower than 0.7. With increasing basicity, perovskite appears and becomes the main phase instead which contains titanium. Crystallization temperature of perovskite is higher than that of rutile and the other phases. Namely, perovskite crystallizes firstly from the molten slag during decreasing temperature. XRD analysis shows that CaTi21O38 is the main phase with a basicity of 0.6. CaMg0.39Al0.87Ti0.48Si1.26O6, CaTiSiO5 and CaMgSi2O6 are the main crystallization phases with a basicity of 0.8. The difference between experimental and thermodynamics calculation is due to the complicate crystallization behavior of the multiple slag under super cooling rate. When the slag basicity increases to 1.1, the main precipitatied phase is perovskite, which agrees well with theory calculation. In addition, the crystal structure of the synthesized titanium bearing slag is basically similar regardless of the basicity.
引用
收藏
页码:193 / 200
页数:8
相关论文
共 15 条
[11]   Influence of TiO2 on the Viscous Behavior of Calcium Silicate Melts Containing 17 mass% Al2O3 and 10 mass% MgO [J].
Sohn, Il ;
Wang, Wanlin ;
Matsuura, Hiroyuki ;
Tsukihashi, Fumitaka ;
Min, Dong Joon .
ISIJ INTERNATIONAL, 2012, 52 (01) :158-160
[12]   Co-modification and Crystalline-control of Ti-bearing Blast Furnace Slags [J].
Sun, Yongqi ;
Li, Zhongmin ;
Liu, Lili ;
Wang, Xidong ;
Zhang, Zuotai .
ISIJ INTERNATIONAL, 2015, 55 (01) :158-165
[13]   Effect of B2O3 on the Structure and Viscous Behavior of Ti-Bearing Blast Furnace Slags [J].
Sun, Yongqi ;
Liao, Junlin ;
Zheng, Kai ;
Wang, Xidong ;
Zhang, Zuotai .
JOM, 2014, 66 (10) :2168-2175
[14]   Crystallization Kinetics of CaO-SiO2(CaO/SiO2=1)-TiO2-10 mass%B2O3 Glassy Slag by Differential Thermal Analysis [J].
Wang, Zhen ;
Shu, Qifeng ;
Chou, Kuochih .
ISIJ INTERNATIONAL, 2015, 55 (04) :709-716
[15]  
Zhou B. Z. Z., 1999, IRON STEEL VAN TITAN, V20, P37