Pyrolysis of wood-PVC mixtures. Formation of chloromethane from lignocellulosic materials in the presence of PVC

被引:47
作者
Czegeny, Zsuzsanna [1 ]
Jakab, Emma [1 ]
Bozi, Janos [1 ]
Blazso, Marianne [1 ]
机构
[1] Hungarian Acad Sci, Inst Mat & Environm Chem, Res Ctr Nat Sci, H-1117 Budapest, Hungary
关键词
Pyrolysis; PVC; Biomass; Chloromethane; THERMAL-DECOMPOSITION; CO-PYROLYSIS; POLY(VINYL CHLORIDE); CELLULOSE; PRODUCTS; DEGRADATION;
D O I
10.1016/j.jaap.2014.11.016
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
Thermal decomposition of polyvinylchloride (PVC)-wood and wood component mixtures were examined under slow and fast heating by pyrolysis-gas chromatography/mass spectrometry (Py-GC/MS) and thermogravimetry/mass spectrometry(TG/MS) techniques in order to clarify the chemical interaction of biomass materials and PVC during thermal decomposition. A hardwood and a softwood (beech and pine), their lignin and two types of cellulose (Avicel and Whatman) were chosen as natural polymer components. Comparing the gaseous and liquid pyrolysis products of pure samples to those of mixtures it was found that considerably lower amount of several reactive compounds have been produced when the biomass sample was mixed with PVC. On the other hand significant amount of chloromethane appeared in the pyrolysate of wood and lignin samples mixed with PVC under fast and slow pyrolysis conditions as well, but only in traces of chlorinated organic compounds were detected from cellulose mixtures. It was concluded that the methoxy groups at phenolic rings in lignin are the methyl source of chloromethane formation, and this reaction consumed most of the HCl evolved from PVC. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:123 / 132
页数:10
相关论文
共 23 条
[1]  
[Anonymous], DEGRADATION STABILIZ
[2]   Effect of metals, metal oxides, and carboxylates on the thermal decomposition processes of poly (vinyl chloride) [J].
Blazsó, M ;
Jakab, E .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 1999, 49 (1-2) :125-143
[3]   Thermal decomposition of polyamides in the presence of poly(vinyl chloride) [J].
Czégény, Z ;
Blazsó, M .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2001, 58 :95-104
[4]  
Czégény Z, 2002, MACROMOL MATER ENG, V287, P277, DOI 10.1002/1439-2054(20020401)287:4<277::AID-MAME277>3.0.CO
[5]  
2-#
[6]   Pyrolysis of wood, cellulose, lignin-brominated epoxy oligomer flame retardant mixtures [J].
Czegeny, Zsuzsanna ;
Jakab, Emma ;
Blazso, Marianne .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2013, 103 :52-59
[7]   Pyrolysis of mixed plastics used in the electronics industry [J].
Day, M ;
Cooney, JD ;
Touchette-Barrette, C ;
Sheehan, SE .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 1999, 52 (02) :199-224
[8]   Volatile products of catalytic flash pyrolysis of celluloses [J].
Dobele, G ;
Meier, D ;
Faix, O ;
Radtke, S ;
Rossinskaja, G ;
Telysheva, G .
JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2001, 58 (58-59) :453-463
[9]   THERMAL-DEGRADATION PRODUCTS OF WOOD - GAS-CHROMATOGRAPHIC SEPARATION AND MASS-SPECTROMETRIC CHARACTERIZATION OF POLYSACCHARIDE DERIVED PRODUCTS [J].
FAIX, O ;
FORTMANN, I ;
BREMER, J ;
MEIER, D .
HOLZ ALS ROH-UND WERKSTOFF, 1991, 49 (05) :213-219
[10]   Thermal and burning properties of wood flour-poly(vinyl chloride) composite [J].
Fang, Yiqun ;
Wang, Qingwen ;
Bai, Xiaoyan ;
Wang, Weihong ;
Cooper, Paul A. .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2012, 109 (03) :1577-1585