Durability and mechanical characteristics of sustainable self-curing concrete utilizing crushed ceramic and brick wastes

被引:26
|
作者
Younis, M. O. [1 ,2 ]
Amin, Mohamed [2 ,3 ]
Tahwia, Ahmed M. [1 ]
机构
[1] Mansoura Univ, Struct Engn Dept, Fac Engn, Mansoura, Egypt
[2] Mansoura High Inst Engn & Technol, Civil Engn Dept, Mansoura, Egypt
[3] Suez Univ, Fac Technol & Educ, Civil Arch Construct Dept, Suez, Egypt
关键词
Sustainability; Polyethylene glycol; Ceramic; Brick; Self-curing concrete; Durability; PERFORMANCE; SHRINKAGE; STRENGTH; FIBER; ASH;
D O I
10.1016/j.cscm.2022.e01251
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Saving natural resources and utilizing building wastes (crushed bricks (CB) and crushed ceramic (CC)) are the major goals of this project. Polyethylene glycol 6000 (PEG6000) was employed as an internal chemical curing material, and CB and CC were used as coarse aggregate substitutes with 25 %, 50 %, and 75 % of dolomite as an internal physical curing agent. Mechanical properties tests compression, splitting tensile, flexural stresses, and modulus of elasticity have been carried out. Durability is inferred by investigating sorptivity, water absorption, drying shrinkage, and chloride penetration tests. Finally, Scanning Electron Microscope (SEM) and Energy Dispersive Spectroscopy (EDS) microstructure testing were performed that showed the bond and cohesion between different aggregates and mortar, and also showed mortar compounds. The ideal PEG 6000 dosage is 1.5 % of cement weight for self-curing concrete mechanical characteristics which resulted in an increment of compressive strength by 48.9 % after 28 days, at 2 % PEG for the greatest durability results the water absorption, sorptivity, and drying shrinkage decreased by 37.5 %, 27 %, and 44 % respectively, and 4 % PEG showed the best chloride penetrability defense and the penetration depth decreased by about 78.7 % all compared to the air cured (AC) mix. The optimum CC replacement percentage is 50 % with 1 % PEG for self-curing (SC) concrete mechanical characteristics which caused a rise in compressive, splitting tensile, flexural strengths, and modulus of elasticity by 55.6 %, 55.35 %, 54.47 %, and 28 % compared to the AC mix.
引用
收藏
页数:20
相关论文
共 50 条
  • [21] Fresh, Mechanical, and Durability Characteristics of Self-Consolidating Concrete Incorporating Recycled Asphalt Pavements
    Ibrahim, Ahmed
    Mahmoud, Enad
    Khodair, Yasser
    Patibandla, Varun Chowdary
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2014, 26 (04) : 668 - 675
  • [22] Effect of recycled concrete aggregates on the mechanical and durability properties of self-cured concrete for sustainable construction
    Dinesh, S. V.
    Mamatha, K. H.
    Susheel Kumar, G.
    INTERNATIONAL JOURNAL OF SYSTEM ASSURANCE ENGINEERING AND MANAGEMENT, 2023, 14 (03) : 865 - 877
  • [23] Effect of recycled concrete aggregates on the mechanical and durability properties of self-cured concrete for sustainable construction
    S. V. Dinesh
    K. H. Mamatha
    G. Susheel Kumar
    International Journal of System Assurance Engineering and Management, 2023, 14 : 865 - 877
  • [24] Mechanical and durability properties of sustainable self-compacting concrete with recycled concrete aggregate and fly ash, slag and silica fume
    Guo, Zhanggen
    Jiang, Tao
    Zhang, Jing
    Kong, Xiangkun
    Chen, Chen
    Lehman, Dawn E.
    CONSTRUCTION AND BUILDING MATERIALS, 2020, 231
  • [25] Mechanical and durability characteristics of sustainable concrete modified with partial substitution of waste foundry sand
    Ahmad, Jawad
    Aslam, Fahid
    Zaid, Osama
    Alyousef, Rayed
    Alabduljabbar, Hisham
    STRUCTURAL CONCRETE, 2021, 22 (05) : 2775 - 2790
  • [26] Mechanical and durability characteristics of sustainable coconut fibers reinforced concrete with incorporation of marble powder
    Ahmad, Jawad
    Zaid, Osama
    Siddique, Muhammad Shahid
    Aslam, Fahid
    Alabduljabbar, Hisham
    Khedher, Khaled Mohamed
    MATERIALS RESEARCH EXPRESS, 2021, 8 (07)
  • [27] Assessment of the mechanical and durability characteristics of bio-mineralized Bacillus subtilis self-healing concrete blended with hydrated lime and brick powder
    Abu Bakr, Mohd
    Singh, Birendra Kumar
    Deifalla, Ahmed Farouk
    Pandey, Shatrudhan
    Hussain, Ahmed
    Ragab, Adham E.
    Alvi, Sahir Sultan
    Hasnain, S. M. Mozammil
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2023, 19
  • [28] Sustainable self-compacting conventional concrete development with optimal content of ladle furnace slag concerning mechanical and durability characteristics
    Panda, Soumyaranjan
    Pradhan, Monalin
    Panigrahi, Saubhagya Kumar
    CONSTRUCTION AND BUILDING MATERIALS, 2025, 471
  • [29] Fresh, Mechanical, and Durability Characteristics of Self-Consolidating Concrete Incorporating Volcanic Ash
    Hossain, K. M. A.
    Lachemi, M.
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2010, 22 (07) : 651 - 657
  • [30] Predictive modeling of rheological, mechanical and durability characteristics of hybrid fiber-reinforced self-compacting concrete
    Agrawal, Achal
    Chandak, Narayan R.
    INNOVATIVE INFRASTRUCTURE SOLUTIONS, 2024, 9 (05)