Influences of multiple firings and aging on surface roughness, strength and hardness of veneering ceramics for zirconia frameworks

被引:17
作者
Tang, Xuehua [1 ,2 ]
Luo, Huinan [3 ]
Bai, Yang [4 ]
Tang, Hui [5 ]
Nakamura, Takashi [2 ]
Yatani, Hirofumi [2 ]
机构
[1] Nanjing Med Univ, Affiliated Hosp 1, Dept Stomatol, Nanjing 210029, Jiangsu, Peoples R China
[2] Osaka Univ, Grad Sch Dent, Dept Fixed Prosthodont, Suita, Osaka 5650871, Japan
[3] Nanjing Univ, Sch Med, Jinling Hosp, Dept Stomatol, Nanjing 210002, Jiangsu, Peoples R China
[4] Nanjing Univ, Sch Med, Inst & Hosp Stomatol, Dept Oral Med, Nanjing 210008, Jiangsu, Peoples R China
[5] Nanjing Med Univ, Inst Stomatol, Nanjing 210029, Jiangsu, Peoples R China
关键词
Veneering ceramics; Multiple firings; Accelerated aging; Surface roughness; Flexural strength; Vickers hardness; CHEMICAL DURABILITY; CE-TZP/AL2O3; NANOCOMPOSITE; CRYSTALLIZATION BEHAVIOR; MECHANICAL-PROPERTIES; STABILIZED ZIRCONIA; FRACTURE-TOUGHNESS; DENTAL CERAMICS; GLASS-CERAMICS; MARGINAL FIT; DEGRADATION;
D O I
10.1016/j.jdent.2015.06.006
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To evaluate the effects of multiple firings and aging on surface roughness, strength, and hardness of veneering ceramics for zirconia frameworks. Methods: Five different veneering ceramics for zirconia frameworks were used: Vintage ZR (ZR), Cerabien ZR (CZR), VitaVM9 (VM9), Cercon ceram KISS (KISS), and IPS e.max ceram (e.max). Specimens were fired 2 or 10 times in order to accelerate aging. Surface roughness was evaluated using laser profilometry. Flexural strength and Vickers hardness were also measured. Surface topography was observed using scanning electron microscopy. Results: After accelerated aging, the surface roughness of all specimens fired 10 times was significantly lower than that of the same specimens fired 2 times (P = 0.000). Except for VM9, the flexural strength of all specimens fired 10 times was greater than that of the same specimens fired 2 times, and the differences were significant for ZR and CZR (P < 0.01). The flexural strength of VM9 fired 10 times was significantly lower than that of VM9 fired 2 times (P = 0.034). The Vickers hardness of ZR and VM9 fired 10 times was significantly higher than that of the same specimens fired 2 times (P < 0.05), but that of KISS fired 10 times was significantly lower than that of KISS fired 2 times (P = 0.000). Conclusions: Multiple firings had a positive effect on the surface roughness of all aged veneering ceramics used for zirconia restorations and on the strength and hardness of many aged veneering ceramics used for zirconia restorations. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1148 / 1153
页数:6
相关论文
共 52 条
  • [1] Morphology and bacterial colonisation of tooth/ceramic restoration interface after different cement excess removal techniques
    Anami, Lilian Costa
    Pereira, Cristiane Aparecida
    Guerra, Elen
    de Assuncao e Souza, Rodrigo Othavio
    Cardoso Jorge, Antonio Olavo
    Bottino, Marco Antonio
    [J]. JOURNAL OF DENTISTRY, 2012, 40 (09) : 742 - 749
  • [2] [Anonymous], 2008, 13356 INT STAND ORG
  • [3] Biaxial Flexure Strength and Low Temperature Degradation of Ce-TZP/Al2O3 Nanocomposite and Y-TZP as Dental Restoratives
    Ban, Seiji
    Sato, Hideo
    Suehiro, Yasuhiko
    Nakanishi, Hideo
    Nawa, Masahiro
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2008, 87B (02) : 492 - 498
  • [4] Structure, chemical durability and crystallization behavior of incinerator-based glassy systems
    Barbieri, L.
    Karamanov, A.
    Corradi, A.
    Lancellotti, I.
    Pelino, M.
    Rincon, J. Ma.
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 2008, 354 (2-9) : 521 - 528
  • [5] Fracture toughness, strength and slow crack growth in a ceria stabilized zirconia-alumina nanocomposite for medical applications
    Benzaid, Rajaa
    Chevalier, Jerome
    Saddaoui, Malika
    Fantozzi, Gilbert
    Nawa, Masahiro
    Diaz, Luis Antonio
    Torrecillas, Ramon
    [J]. BIOMATERIALS, 2008, 29 (27) : 3636 - 3641
  • [6] Marginal and internal fit of curved anterior CAD/CAM-milled zirconia fixed dental prostheses: An in-vitro study
    Buechi, Dominik L.
    Ebler, Sabine
    Haemmerle, Christoph H. F.
    Sailer, Irena
    [J]. QUINTESSENCE INTERNATIONAL, 2014, 45 (10): : 837 - 846
  • [7] MOLECULAR MECHANISMS FOR CORROSION OF SILICA AND SILICATE-GLASSES
    BUNKER, BC
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 1994, 179 : 300 - 308
  • [8] Effect of ion exchange on hardness and fracture toughness of dental porcelains
    Cesar, Paulo Francisco
    Gonzaga, Carla Castiglia
    Miranda, Walter Gomes, Jr.
    Yoshimura, Humberto Naoyuki
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2007, 83B (02) : 538 - 545
  • [9] The influence of process parameters and heat treatment on the properties of cold sprayed silver coatings
    Chavan, Naveen Manhar
    Ramakrishna, M.
    Phani, P. Sudharshan
    Rao, D. Srinivasa
    Sundararajan, G.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2011, 205 (20) : 4798 - 4807
  • [10] The influence of surface roughness on porcelain strength
    de Jager, N
    Feilzer, AJ
    Davidson, CL
    [J]. DENTAL MATERIALS, 2000, 16 (06) : 381 - 388