The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs

被引:36
|
作者
Venturini, Andressa B. [1 ]
Prochnow, Catina [1 ]
Pereira, Gabriel K. R. [1 ,2 ]
Werner, Arie [3 ,4 ]
Kleverlaan, Cornelis J. [3 ,4 ]
Valandro, Luiz Felipe [1 ]
机构
[1] Univ Fed Santa Maria, Fac Odontol, Santa Maria, RS, Brazil
[2] IMED, Merid Fac, Sch Dent, Passo Fundo, RS, Brazil
[3] Univ Amsterdam, Acad Ctr Dent Amsterdam ACTA, Dept Dent Mat Sci, Amsterdam, Netherlands
[4] Vrije Univ, Amsterdam, Netherlands
关键词
Acid etching; Glass ceramics; Fatigue; Surface treatment; Mechanical cycling; BOND STRENGTH; RESIN; SURFACE; IMPACT; GLASS; PERFORMANCE;
D O I
10.1016/j.dental.2018.01.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. This study investigated the influence of hydrofluoric acid (HF) etching at different concentrations on the fatigue failure load of adhesively cemented feldspathic ceramic discs (Vita Mark II). Besides, their effect on the micromorphology of ceramic surface was investigated. Methods. Eighty ceramic discs (phi = 10 mm; thickness = 1.5 mm) were cemented to epoxy supporting discs (phi = 10 mm; thickness = 2.0 mm) using different surface conditioning methods (n = 20): nonetched control (CTRL), or etched for 60 s with different HF concentrations: 1% (HF1), 5% (HF5), or 10% (HF10). All the ceramic discs received a silane application (Monobond Plus). The epoxy discs were etched with 10% HF for 60 s and received a primer coating (Multilink Primer A + B). Adhesively cementation was performed (Multilink Automix), and the assemblies (ceramic discs/epoxy discs) were subjected to cyclic loads in water by a staircase approach (500,000 cycles; 20 Hz; initial load = 290 N; step size = 30 N). Fatigue failure load data were analyzed using 1-way ANOVA and post-hoc Tukey's tests (alpha =.05). Results. Mean failure load of the HF5 group (255.0 +/- 23.0 N) was significantly lower; HF1 group (301.7 +/- 71.0 N) presented intermediate values, and the highest values were achieved in CTRL (351.7 +/- 13.4 N) and HF10 (341.7 +/- 20.6 N) groups. All the failures were radial cracks starting from the bonding surface. (C) 2018 The Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:667 / 675
页数:9
相关论文
共 50 条
  • [21] The effect of hydrofluoric acid surface treatment and bond strength of a zirconia veneering ceramic
    Chaiyabutr, Yada
    McGowan, Steve
    Phillips, Keith M.
    Kois, John C.
    Giordano, Russell A.
    JOURNAL OF PROSTHETIC DENTISTRY, 2008, 100 (03): : 194 - 202
  • [22] Effect of hydrofluoric acid chemical corrosion on the grinding of silicon nitride ceramic ball
    Ge, Ziqiang
    Li, Songhua
    Wu, Yuhou
    Sha, Yong
    Sun, Jian
    Tian, Junxing
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2022, 23 (05): : 685 - 693
  • [23] Load Ratio Effect on the Fatigue Behaviour of Adhesively Bonded Joints: An Enhanced Damage Model
    Katnam, K. B.
    Crocombe, A. D.
    Khoramishad, H.
    Ashcroft, I. A.
    JOURNAL OF ADHESION, 2010, 86 (03): : 257 - 272
  • [24] Effect of occlusal anatomy of CAD/CAM feldspathic posterior crowns in the stress concentration and fracture load
    Souto Borges, Alexandre Luiz
    Mendes Tribst, Joao Paulo
    de Lima, Aline Lins
    de Oliveira Dal Piva, Amanda Maria
    Ozcan, Mutlu
    CLINICAL AND EXPERIMENTAL DENTAL RESEARCH, 2021, 7 (06): : 1190 - 1196
  • [25] Fatigue Failure Load of Resin-bonded Simplified Lithium Disilicate Glass-Ceramic Restorations: Effect of Ceramic Conditioning Methods
    Mendes Tribst, Joao Paulo
    Monteiro, Jaiane Bandoli
    Venturini, Andressa Borin
    Rocha Pereira, Gabriel Kalil
    Bottino, Marco Antonio
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    JOURNAL OF ADHESIVE DENTISTRY, 2019, 21 (04): : 373 - 381
  • [26] THE EFFECT OF A FATIGUE FAILURE ON THE WELLHEAD ULTIMATE LOAD CAPACITY
    Reinas, Lorents
    Saether, Morten
    Aadnoy, Bernt Sigve
    PROCEEDINGS OF THE ASME 31ST INTERNATIONAL CONFERENCE ON OCEAN, OFFSHORE AND ARTIC ENGINEERING, VOL 1, 2012, : 307 - 314
  • [27] Effect of hydrofluoric acid (HF) concentration to pores size diameter of silicon membrane
    Norhafizah, Burham
    Hamzah, Azrul Azlan
    Majlis, Burhanuddin Yeop
    BIO-MEDICAL MATERIALS AND ENGINEERING, 2014, 24 (06) : 2203 - 2209
  • [28] The effect of hydrofluoric acid and resin cement formulation on the bond strength to lithium disilicate ceramic
    Sundfeld, Daniel
    Muniz Palialol, Alan Rodrigo
    Fugolin, Ana Paula Piovesan
    Bovi Ambrosano, Glaucia Maria
    Correr-Sobrinho, Lourenco
    Marcondes Martins, Luis Roberto
    Pfeifer, Carmem Silvia
    BRAZILIAN ORAL RESEARCH, 2018, 32
  • [29] The effect of different cooling rates and coping thicknesses on the failure load of zirconia-ceramic crowns after fatigue loading
    Tang, Yu Lung
    Kim, Jee-Hwan
    Shim, June-Sung
    Kim, Sunjai
    JOURNAL OF ADVANCED PROSTHODONTICS, 2017, 9 (03): : 152 - 158
  • [30] Load-bearing capacity under fatigue and survival rates of adhesively cemented yttrium-stabilized zirconia polycrystal monolithic simplified restorations
    Zucuni, Camila Pauleski
    Venturini, Andressa Borin
    Prochnow, Catina
    Rocha Pereira, Gabriel Kalil
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2019, 90 : 673 - 680