The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs

被引:36
|
作者
Venturini, Andressa B. [1 ]
Prochnow, Catina [1 ]
Pereira, Gabriel K. R. [1 ,2 ]
Werner, Arie [3 ,4 ]
Kleverlaan, Cornelis J. [3 ,4 ]
Valandro, Luiz Felipe [1 ]
机构
[1] Univ Fed Santa Maria, Fac Odontol, Santa Maria, RS, Brazil
[2] IMED, Merid Fac, Sch Dent, Passo Fundo, RS, Brazil
[3] Univ Amsterdam, Acad Ctr Dent Amsterdam ACTA, Dept Dent Mat Sci, Amsterdam, Netherlands
[4] Vrije Univ, Amsterdam, Netherlands
关键词
Acid etching; Glass ceramics; Fatigue; Surface treatment; Mechanical cycling; BOND STRENGTH; RESIN; SURFACE; IMPACT; GLASS; PERFORMANCE;
D O I
10.1016/j.dental.2018.01.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. This study investigated the influence of hydrofluoric acid (HF) etching at different concentrations on the fatigue failure load of adhesively cemented feldspathic ceramic discs (Vita Mark II). Besides, their effect on the micromorphology of ceramic surface was investigated. Methods. Eighty ceramic discs (phi = 10 mm; thickness = 1.5 mm) were cemented to epoxy supporting discs (phi = 10 mm; thickness = 2.0 mm) using different surface conditioning methods (n = 20): nonetched control (CTRL), or etched for 60 s with different HF concentrations: 1% (HF1), 5% (HF5), or 10% (HF10). All the ceramic discs received a silane application (Monobond Plus). The epoxy discs were etched with 10% HF for 60 s and received a primer coating (Multilink Primer A + B). Adhesively cementation was performed (Multilink Automix), and the assemblies (ceramic discs/epoxy discs) were subjected to cyclic loads in water by a staircase approach (500,000 cycles; 20 Hz; initial load = 290 N; step size = 30 N). Fatigue failure load data were analyzed using 1-way ANOVA and post-hoc Tukey's tests (alpha =.05). Results. Mean failure load of the HF5 group (255.0 +/- 23.0 N) was significantly lower; HF1 group (301.7 +/- 71.0 N) presented intermediate values, and the highest values were achieved in CTRL (351.7 +/- 13.4 N) and HF10 (341.7 +/- 20.6 N) groups. All the failures were radial cracks starting from the bonding surface. (C) 2018 The Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:667 / 675
页数:9
相关论文
共 50 条
  • [1] Fatigue failure load of feldspathic ceramic crowns after hydrofluoric acid etching at different concentrations
    Venturini, Andressa B.
    Prochnow, Catina
    May, Liliana G.
    Kleverlaan, Cornelis J.
    Valandro, Luiz Felipe
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (02): : 278 - 285
  • [2] Effect of Hydrofluoric Acid Concentration on Resin Adhesion to a Feldspathic Ceramic
    Venturini, Andressa Borin
    Prochnow, Catina
    Rambo, Dagma
    Gundel, Andre
    Valandro, Luiz Felipe
    JOURNAL OF ADHESIVE DENTISTRY, 2015, 17 (04): : 313 - 320
  • [3] Fatigue Failure Load of a Bonded Simplified Monolithic Feldspathic Ceramic: Influence of Hydrofluoric Acid Etching and Thermocycling
    Guilardi, L. F.
    Pereira, G. K. R.
    Vallau, A. S.
    Silva, I. A.
    Giordani, J. C.
    Valandro, L. F.
    Rippe, M. P.
    OPERATIVE DENTISTRY, 2020, 45 (01) : E21 - E31
  • [4] Fatigue failure load of zirconia-reinforced lithium silicate glass ceramic cemented to a dentin analogue: Effect of etching time and hydrofluoric acid concentration
    Monteiro, Jaiane Bandoli
    Oliani, Marcelo Gallo
    Guilardi, Luis Felipe
    Prochnow, Catina
    Rocha Pereira, Gabriel Kalil
    Bottino, Marco Antonio
    de Melo, Renata Marques
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2018, 77 : 375 - 382
  • [5] Influence of hydrofluoric acid concentration on the flexural strength of a feldspathic ceramic
    Venturini, Andressa B.
    Prochnow, Catina
    May, Liliana G.
    Bottino, Marco C.
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2015, 48 : 241 - 248
  • [6] Fatigue Failure Load of Restored Premolars: Effect of Etching the Intaglio Surface of Ceramic Inlays With Hydrofluoric Acid at Different Concentrations
    Missau, T.
    Venturini, A. B.
    Pereira, G. K. R.
    Prochnow, C.
    Valandro, L. F.
    Rippe, M. P.
    OPERATIVE DENTISTRY, 2018, 43 (02) : E81 - E91
  • [7] Fatigue failure load of an adhesively-cemented lithium disilicate glass-ceramic: Conventional ceramic etching vs etch & prime one-step primer
    Scherer, Maite Munhoz
    Prochnow, Catina
    Venturini, Andressa Borin
    Rocha Pereira, Gabriel Kalil
    de Lima Burgo, Thiago Augusto
    Rippe, Marilia Pivetta
    Valandro, Luiz Felipe
    DENTAL MATERIALS, 2018, 34 (08) : 1134 - 1143
  • [8] Hydrofluoric acid concentration, time and use of phosphoric acid on the bond strength of feldspathic ceramics
    Duarte Moura, Dayanne Monielle
    Medeiros de Araujo, Arthur Magno
    de Souza, Karina Barbosa
    Verissimo, Aretha Heitor
    Mendes Tribst, Joao Paulo
    de Assuncao e Souza, Rodrigo Othavio
    BRAZILIAN ORAL RESEARCH, 2020, 34
  • [9] Resin microtensile bond strength to feldspathic ceramic:: Hydrofluoric acid etching vs tribochemical silica coating
    Pelogia, Fernanda
    Valandro, Luiz Felipe
    Brigagao, Vinicius
    Neisser, Maximiliano Piero
    Bottino, Marco A.
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2007, 20 (05) : 532 - 534
  • [10] Effect of Hydrofluoric Acid Concentration and Etching Time on Bond Strength to Lithium Disilicate Glass Ceramic
    Puppin-Rontani, J.
    Sundfeld, D.
    Costa, A. R.
    Correr, A. B.
    Puppin-Rontani, R. M.
    Borges, G. A.
    Sinhoreti, M. A. C.
    Correr-Sobrinho, L.
    OPERATIVE DENTISTRY, 2017, 42 (06) : 606 - 615