摘要
The present study examines the potential of Zn-Al based alloys for replacing Pb-containing solders used in the die-attaching process. Four alloys (Zn-6wt.%Al, Zn-6wt.%Al-1wt.%Ga, Zn-3wt.%Al-3wt.%Mg, and Zn-4wt.%Al-3wt.%Ga-3wt.%Mg) were cast and characterized in terms of microstructure and mechanical behavior. Based on the criteria of thermodynamics (phase diagram extrapolations) and mechanical behavior (flow curves), it was possible to select the Zn-Al-Ga alloy as best meeting the requirements concerning melting range necessary for die attach and mechanical properties. A wire with 0.76-mm thickness was produced successfully by extrusion. However, the alloy, in the form of wires, is subject to substantial embrittlement after extruding to a degree that further handling becomes impossible. The reason for the embrittlement was investigated using x-ray techniques (x-ray diffraction and x-ray photo spectroscopy (XPS)) and transmission electron microscopy. The temperature dependence of the Ga solubility in the hexagonal close-packed (hcp) Zn-rich phase in combination with the affinity of Ga to the surface of the Al-rich and Zn-rich phases is held responsible for the embrittlement. A remedy for the embrittlement could be a reduction of the solubility at high temperatures in the Zn-rich phase. This will be attempted by adding small fractions of further alloying elements in future work.
引用
收藏
页码:278 / 285
页数:8
相关论文
共 27 条
  • [21] The effects of lanthanum on microstructure and electrochemical properties of Al-Zn-In based sacrificial anode alloys
    Ma, Jingling
    Wen, Jiuba
    CORROSION SCIENCE, 2009, 51 (09) : 2115 - 2119
  • [22] Microstructure Characterization and Creep Behavior of Pb-Free Sn-Rich Solder Alloys: Part I. Microstructure Characterization of Bulk Solder and Solder/Copper Joints
    R.S. Sidhu
    N. Chawla
    Metallurgical and Materials Transactions A, 2008, 39 : 340 - 348
  • [23] Current status of Pb-free PSCs and infer the highest achievable PCE via numerical modeling, and optimization of novel structure FAMASnGeI3 based PSCs
    Hamzah, Hairul Mardiah
    Miah, Md Helal
    Hossen, Md Jakir
    Soin, Norhayati Binti
    Abdul Wahab, Yasmin
    Khandaker, Mayeen Uddin
    Aminul Islam, Mohammad
    MATERIALS RESEARCH EXPRESS, 2024, 11 (06)
  • [24] Assessment of hydrogen embrittlement via image-based techniques in Al-Zn-Mg-Cu aluminum alloys
    Su, Hang
    Toda, Hiroyuki
    Shimizu, Kazuyuki
    Uesugi, Kentaro
    Takeuchi, Akihisa
    Watanabe, Yoshio
    ACTA MATERIALIA, 2019, 176 : 96 - 108
  • [25] Optimization and detail analysis of novel structure Pb-free CsGeI3-based all-inorganic perovskite solar cells by SCAPS-1D
    Miah, Md. Helal
    Rahman, Md. Bulu
    Khatun, Fatema
    Khandaker, Mayeen Uddin
    Hatta, Sharifah Fatmadiana Wan Muhammad
    Soin, Norhayati Binti
    Islam, Mohammad Aminul
    OPTIK, 2023, 281
  • [26] Influence of minor Zn additions on grain boundary anelasticity, grain boundary sliding, and superplasticity of Al-Mg-based alloys
    V. Mikhaylovskaya, Anastasia
    Yakovtseva, Olga A.
    Mochugovskiy, Andrey G.
    Cifre, Joan
    Golovin, Igor S.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 926
  • [27] Effect of Zn Addition on the Microstructural Heterogeneity and Mechanical Properties of Vacuum-Assisted High-Pressure Die Casting Al-Si-Mg-Cu alloys
    Jiang, Yuanhang
    Zheng, Huiting
    Liu, Fei
    Zhao, Haidong
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (09)