Sagging resistance of warm formed aluminum brazing sheet

被引:15
作者
Benoit, M. J. [1 ]
Kaur, R. [1 ]
Wells, M. A. [1 ]
Jin, H. [2 ]
Amirkhiz, B. Shalchi [2 ]
Winkler, S. [3 ]
机构
[1] Univ Waterloo, Dept Mech & Mechatron Engn, 200 Univ Ave W, Waterloo, ON N2L 3G1, Canada
[2] CanmetMATERIALS, 183 Longwood Rd S, Hamilton, ON L8P 0A5, Canada
[3] Dana Canada Corp, 656 Kerr Sc, Oakville, ON L6K 3E4, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Warm forming; Brazing; Sagging distance; Liquid film migration (LFM); Recrystallization; Strain induced boundary migration (SIBM); LIQUID-FILM MIGRATION; ALLOYS; BRAZEABILITY;
D O I
10.1016/j.jmatprotec.2017.11.041
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Interrupted tensile tests, performed between room temperature (RT) and 250 degrees C, were used to simulate warm forming of an AA3003/AA4045 brazing sheet. Brazing performance was predicted from sagging distance measurements after a thermal cycle. The sagging distance as a function of strain for sheets strained at 150 degrees C was similar to that of RT strained samples, while the sagging distances were larger at all levels of applied strain for sheets strained at 200 degrees C and 250 degrees C. Large sagging distances were correlated with the occurrence of liquid film migration during simulated brazing and a recovered substructure in the core alloy, while small sagging distances were associated with a coarse, recrystallized core alloy. The poor brazing performance of sheets formed above 150 degrees C was attributed to a reduction in the stored strain energy during forming, resulting in recovery rather than recrystallization during brazing, leaving a microstructure which is susceptible to liquid film migration.
引用
收藏
页码:353 / 360
页数:8
相关论文
共 50 条
[31]   Chemical dissolution resistance of anodic oxide layers formed on aluminum [J].
Bensalah, W. ;
Feki, M. ;
Wery, M. ;
Ayedi, H. F. .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (07) :1673-1679
[32]   Corrosion resistance of tungsten carbide-based cermet coatings formed by sinter-brazing [J].
Joo, Hyung Goun ;
Zhang, Da Quan ;
Gao, Li Xin ;
Liu, Tao ;
Lee, Kang Yong .
INTERNATIONAL JOURNAL OF SURFACE SCIENCE AND ENGINEERING, 2014, 8 (04) :380-391
[33]   Effects of Annealing and Deformation on Sagging Resistance of a Hot-Rolled, Four-Layered Al Alloy Clad Sheet [J].
Kang, Minglong ;
Zhou, Li ;
Deng, Yunlai ;
Lei, Jinqin .
ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2021, 2021
[34]   Interfacial phenomena in brazing of a stainless steel face sheet to a honeycomb core [J].
Mehrizi, S. ;
Hadian, A. M. ;
Hadian, A. ;
Vosughi, A. .
ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, PTS 1 AND 2, 2010, 83-86 :1236-1242
[35]   A combined FEA and design of experiments approach for the design and analysis of warm forming of aluminum sheet alloys [J].
Kim, Hong Seok .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2010, 51 (1-4) :1-14
[36]   A combined FEA and design of experiments approach for the design and analysis of warm forming of aluminum sheet alloys [J].
Hong Seok Kim .
The International Journal of Advanced Manufacturing Technology, 2010, 51 :1-14
[37]   Friction characterization and application to warm forming of a high strength 7000-series aluminum sheet [J].
Noder, J. ;
George, R. ;
Butcher, C. ;
Worswick, M. J. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2021, 293
[38]   Laser brazing of steel - Aluminum assembly [J].
Rodriguez, L ;
Mathieu, A ;
Langlade, C ;
Vannes, A ;
Grevey, D ;
Mattei, S .
LASERS IN ENGINEERING, 2005, 15 (5-6) :413-425
[39]   Microstructure and properties of aluminum foam/aluminum sandwich prepared by brazing [J].
Zhang J. ;
Cheng H. ;
Huang X. ;
Sun D. .
Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (08) :144-149
[40]   Predicting Sheet Forming Limit of Aluminum Alloys for Cold and Warm Forming by Developing a Ductile Failure Criterion [J].
Sheng, Z. Q. ;
Mallick, P. K. .
JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2017, 139 (11)