Effects of Sintering Holding Time on the Structural, Electrical and Magnetic Properties of Zn0.95Ni0.05O

被引:0
|
作者
Ginting, M. [1 ]
Aryanto, D. [1 ]
Kurniawan, C. [1 ]
Sari, A. Y. [1 ]
Subhan, A. [1 ]
Sudiro, T. [1 ]
Sebayang, P. [1 ]
Tarigan, E. R. [2 ]
Nasruddin, M. N. [2 ]
Sebayang, K. [2 ]
机构
[1] Indonesian Inst Sci, Res Ctr Phys, Tangerang Selatan 15314, Banten, Indonesia
[2] Univ Sumatera Utara, Postgrad Program, Medan 20155, Indonesia
关键词
Sintering; holding time; Zn0.95Ni0.05O; structure; electrical and magnetic property; DIELECTRIC-PROPERTIES; ZNO;
D O I
10.1088/1757-899X/202/1/012033
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Zn0.95Ni0.05O has been synthesized by mixing 5% mol of NiO into ZnO using solid state reaction and high-speed shaker mill method. The samples were sintered at 900 degrees C with holding time for 2, 4 and 8 hours. Crystal structure, electrical and magnetic properties of Zn0.95Ni0.05O were characterized by using XRD, I-V, C-V and VSM. XRD results showed that variation of holding time does not change the structure of ZnO and no other secondary phase observed. The value of lattice parameters (a and c) tends to decrease proportionally to the holding time. The Intensity value changes and the peak shifted to a higher 2 theta angle due to holding time variation. In general, the conductance of Zn0.95Ni0.05O decreases and the magnetic properties decrease also as the holding time is increased.