Composition and structure of an 18-year-old 5M KOH-activated ground granulated blast-furnace slag paste

被引:56
作者
Richardson, I. G. [1 ]
Li, S. [1 ,2 ]
机构
[1] Univ Leeds, Sch Civil Engn, Leeds LS2 9JT, W Yorkshire, England
[2] Haerbin Inst Technol, Sch Civil Engn, Haerbin 150000, Heilongjiang, Peoples R China
关键词
Slag; NMR; TEM; Microstructure; Alkali activation; C-S-H; ORDINARY PORTLAND-CEMENT; NMR; ALUMINUM; MICROSTRUCTURE; MICROANALYSIS; HYDRATION; AL-27;
D O I
10.1016/j.conbuildmat.2018.02.034
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The main hydration products were C-A-S-H(I), present in both inner (Ip) and outer product (Op), and a Mg-Al layered double hydroxide (LDH), present only in the Ip. The composition of C-A-S-H(I) was the same in Op and Ip. Reduced scatter in the data with age suggests a tendency towards compositional homogeneity. The mean length of the aluminosilicate anions in the C-A-S-H(I) increased with age. The layer spacings of the C-A-S-H(I) and Mg-Al LDH had not changed significantly with age. The Mg/Al ratio of the LDH was about 2.6 and had not changed between 1 and 18 years. (C) 2018 Elsevier Ltd. All rights reserved.
引用
收藏
页码:404 / 411
页数:8
相关论文
共 36 条
[1]   Incorporation of aluminum in the calcium silicate hydrate (C-S-H) of hydrated Portland cements:: A high-field 27Al and 29Si MAS NMR Investigation [J].
Andersen, MD ;
Jakobsen, HJ ;
Skibsted, J .
INORGANIC CHEMISTRY, 2003, 42 (07) :2280-2287
[2]  
[Anonymous], 2010, NDARWMD033
[3]  
ATKINS M, 1992, Waste Management, V12, P105, DOI 10.1016/0956-053X(92)90044-J
[4]   Characterization by multinuclear high-resolution NMR of hydration products in activated blast-furnace slag pastes [J].
Bonk, F ;
Schneider, J ;
Cincotto, MA ;
Panepucci, H .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (10) :1712-1719
[5]   Sodium silicate-based, alkali-activated slag mortars Part I. Strength, hydration and microstructure [J].
Brough, AR ;
Atkinson, A .
CEMENT AND CONCRETE RESEARCH, 2002, 32 (06) :865-879
[6]   Aluminium-27 solid state NMR spectroscopic studies of chloride binding in Portland cement and blends [J].
Chudek, JA ;
Hunter, G ;
Jones, MR ;
Scrimgeour, SN ;
Hewlett, PC ;
Kudryavtsev, AB .
JOURNAL OF MATERIALS SCIENCE, 2000, 35 (17) :4275-4288
[7]  
Department of Energy and Climate Change, 2014, IMPL GEOGL DISP FRAM
[8]  
Drits V.A., 2001, Layered double hydroxide, P41
[9]  
Engelhardt G., 1987, HIGH RESOLUTION SOLI
[10]   Long-term behaviour of cement pastes used for nuclear waste disposal: Review of physico-chemical mechanisms of water degradation [J].
Faucon, P ;
Adenot, F ;
Jacquinot, JF ;
Petit, JC ;
Cabrillac, R ;
Jorda, M .
CEMENT AND CONCRETE RESEARCH, 1998, 28 (06) :847-857