Physical properties of RF sputtered ITO thin films and annealing effect

被引:133
作者
Kerkache, L [1 ]
Layadi, A
Dogheche, E
Rémiens, D
机构
[1] Univ Ferhat Abbas, Fac Sci, Dept Phys, Setif 19000, Algeria
[2] Univ Valenciennes & Hainaut Cambresis, CNRS, UMR 8520, IEMN, F-59000 Lille, France
关键词
D O I
10.1088/0022-3727/39/1/027
中图分类号
O59 [应用物理学];
学科分类号
摘要
The structural, electrical and optical properties of RF sputtered In2O3 : Sn (ITO) thin films and the effect of post-deposition annealing have been studied. The thickness ranges from 225 to 862 nm. X-ray diffraction, scanning electron microscopy (SEM) and atomic force microscopy (AFM) experiments were performed to study the structure and the surface morphology of these samples. We found that thinner films have a < 100 > texture and as the film grows the preferred orientation changes from < 100 > to < 111 >. The lattice parameters are found to be larger than the bulk value, indicating that the samples are under a tensile stress. The grain size increases with increasing thickness. SEM images show a dense granular structure with grains having different shapes and sizes. From AFM images, the average surface roughness (rms) was estimated to be 3.89 nm. The energy gap was found to decrease from 3.65 to 3.50 eV as t increases from 225 to 866 nm. Annealing experiments were done, in the air, at temperature T in the 100-500 degrees C range. We found that the < 111 > texture becomes stronger after the annealing treatment. A large increase of the grain size with increasing T is observed. The lattice constant decreases with T to become closer to the bulk value, i.e. annealing seems to relieve the stress present in the as-deposited films; T = 400 degrees C seems to be the best temperature to obtain practically a stress free sample. We observe a large decrease in the electrical resistivity p after annealing. The lowest p value (16 x 10(-4) Omega cm) was noted in the 699 nm thick sample annealed at 500 degrees C. The decrease of p seems to be the consequence of a larger grain size and a stronger < 111 > texture.
引用
收藏
页码:184 / 189
页数:6
相关论文
共 22 条
  • [1] Fabrication of ITO thin films by filtered cathodic vacuum arc deposition
    Chen, BJ
    Sun, XW
    Tay, BK
    [J]. MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2004, 106 (03): : 300 - 304
  • [2] Properties of ITO films on glass fabricated by pulsed laser deposition
    Choi, JB
    Kim, JH
    Jeon, KA
    Lee, SY
    [J]. MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2003, 102 (1-3): : 376 - 379
  • [3] Cruz LR, 2004, MATER RES BULL, V39, P993, DOI [10.1016/j.mattersbull.2004.03.008, 10.1016/j.materresbull.2004.03.008]
  • [4] Microstructure study of indium tin oxide thin films by optical methods
    Cui, HN
    Teixeira, V
    Monteiro, A
    [J]. VACUUM, 2002, 67 (3-4) : 589 - 594
  • [5] Densification of In2O3:: Sn multilayered films elaborated by the dip-coating sol-gel route
    Daoudi, K
    Canut, B
    Blanchin, MG
    Sandu, CS
    Teodorescu, VS
    Roger, JA
    [J]. THIN SOLID FILMS, 2003, 445 (01) : 20 - 25
  • [6] PROPERTIES OF ELECTRON-BEAM-EVAPORATED TIN OXIDE-FILMS
    DAS, D
    BANERJEE, R
    [J]. THIN SOLID FILMS, 1987, 147 (03) : 321 - 331
  • [7] Effect of substrate temperature on electrical, structural, optical and cathodoluminescent properties of In2O3-Sn thin films prepared by spray pyrolysis
    El Hichou, A
    Kachouane, A
    Bubendorff, JL
    Addou, M
    Ebothe, J
    Troyon, M
    Bougrine, A
    [J]. THIN SOLID FILMS, 2004, 458 (1-2) : 263 - 268
  • [8] CHARACTERISTICS OF INDIUM TIN OXIDE-FILMS DEPOSITED BY RF MAGNETRON SPUTTERING
    JOSHI, RN
    SINGH, VP
    MCCLURE, JC
    [J]. THIN SOLID FILMS, 1995, 257 (01) : 32 - 35
  • [9] CHEMICAL VAPOR-DEPOSITION OF TRANSPARENT ELECTRICALLY CONDUCTING LAYERS OF INDIUM OXIDE DOPED WITH TIN
    KANE, J
    SCHWEIZER, HP
    KERN, W
    [J]. THIN SOLID FILMS, 1975, 29 (01) : 155 - 163
  • [10] Structural and electrical properties of as-deposited and annealed DC sputtered ITO thin films
    Kerkache, L
    Sadaoui, K
    Layadi, A
    [J]. EUROPEAN PHYSICAL JOURNAL-APPLIED PHYSICS, 1998, 1 (02) : 177 - 180