Wear of SiC-reinforced Al-matrix composites in the temperature range 20-200 degrees C

被引:90
作者
Martin, A
Martinez, MA
LLorca, J
机构
[1] Department of Materials Science, Polytechnic University of Madrid, E.T.S. de Ingenieros de Caminos
关键词
metal-matrix composites; aluminium alloys; high temperature;
D O I
10.1016/0043-1648(95)06704-3
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The influence of temperature on wear resistance was studied in a 2618 Al alloy reinforced with 1.5 vol% SiC particulates and the corresponding unreinforced alloy in the temperature range 20-200 degrees C. A transition from mild to severe wear (shown by an increase of two orders of magnitude in the wear rates) was observed in both materials beyond a critical temperature. The addition of the SiC particulates improved the wear resistance by a factor of two in the mild wear region, and the transition temperature, which was around 50 degrees C higher in the composite. This higher transition temperature was due to the retention of the mechanical properties in the composite at elevated temperature. Heat treatments (either natural or artificial aging) did not modify substantially the wear resistance of either the composite or the unreinforced alloy.
引用
收藏
页码:169 / 179
页数:11
相关论文
共 17 条
  • [1] METAL-MATRIX COMPOSITES IN THE AUTOMOTIVE INDUSTRY - OPPORTUNITIES AND CHALLENGES
    ALLISON, JE
    COLE, GS
    [J]. JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 1993, 45 (01): : 19 - 24
  • [2] SLIDING AND ABRASIVE WEAR BEHAVIOR OF AN ALUMINUM (2014)-SIC PARTICLE REINFORCED COMPOSITE
    ALPAS, AT
    EMBURY, JD
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (05): : 931 - 935
  • [3] EFFECT OF MICROSTRUCTURE (PARTICULATE SIZE AND VOLUME FRACTION) AND COUNTERFACE MATERIAL ON THE SLIDING WEAR-RESISTANCE OF PARTICULATE-REINFORCED ALUMINUM-MATRIX COMPOSITES
    ALPAS, AT
    ZHANG, J
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (05): : 969 - 983
  • [4] EFFECT OF SIC PARTICULATE REINFORCEMENT ON THE DRY SLIDING WEAR OF ALUMINUM SILICON ALLOYS (A356)
    ALPAS, AT
    ZHANG, J
    [J]. WEAR, 1992, 155 (01) : 83 - 104
  • [5] ON THE WEAR OF ALUMINUM CORUNDUM COMPOSITES
    ANAND, K
    KISHORE
    [J]. WEAR, 1983, 85 (02) : 163 - 169
  • [6] HATCH JE, 1993, ALUMINUM PROPERTIES, P367
  • [7] COMPOSITES OF ALUMINUM-ALLOYS - FABRICATION AND WEAR BEHAVIOR
    HOSKING, FM
    PORTILLO, FF
    WUNDERLIN, R
    MEHRABIAN, R
    [J]. JOURNAL OF MATERIALS SCIENCE, 1982, 17 (02) : 477 - 498
  • [8] FAILURE MICROMECHANISMS IN PARTICULATE-REINFORCED METAL-MATRIX COMPOSITES
    LLORCA, J
    [J]. JOURNAL DE PHYSIQUE IV, 1993, 3 (C7): : 1793 - 1798
  • [9] LLORCA J, 1992, SCR METALL T A, V24, P1575
  • [10] WEAR OF AL-SI ALLOYS AND AL-SI/SIC COMPOSITES AT AMBIENT AND ELEVATED-TEMPERATURES
    MARTINEZ, MA
    MARTIN, A
    LLORCA, J
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1993, 28 (02): : 207 - 212