Densification of Sm0.2Ce0.8O1.9 with the addition of lithium oxide as sintering aid

被引:50
|
作者
Le, Shiru [1 ,2 ]
Zhu, Shengcai [3 ]
Zhu, Xiaodong [1 ,2 ]
Sun, Kening [1 ,2 ]
机构
[1] Harbin Inst Technol, Nat Sci Res Ctr, Acad Fundamental & Interdisciplinary Sci, Harbin 150001, Heilongjiang, Peoples R China
[2] Harbin Inst Technol, State Key Lab Urban Water Resource & Environm, Harbin 150090, Peoples R China
[3] Harbin Inst Technol, Dept Appl Chem, Harbin 150001, Heilongjiang, Peoples R China
基金
高等学校博士学科点专项科研基金;
关键词
Solid oxide fuel cells; Samarium doped cerium oxide; Sintering aid; Mechanism; Sintering parameters; IONIC-CONDUCTIVITY; BEHAVIOR; POWDERS;
D O I
10.1016/j.jpowsour.2012.08.020
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
20 mol% samarium doped cerium oxide (Sm0.2Ce0.8O1.9, SDC) has one of the highest ionic conductivities as electrolyte for solid oxide fuel cell in intermediate temperature, but is restricted to commercial application for its poor densification behavior. The addition of 2 mol% Li2O in the Sm0.2Ce0.8O1.9 (SDC2) improves its maximum shrinkage rate from 4.6 x 10(-3) min(-1)-1.1 min(-1) at a heating rate of 10 degrees C min(-1). The relative density of SDC2 achieves 99.5% at 898 degrees C and 3 degrees C.min(-1), while it is only 82% for SDC at 1250 degrees C and 3 degrees C min(-1). The grain boundary diffusion is the densification mechanism, and the mobility of grain boundary increases from 9.8 x 10(-19)m(3) N-1 s(-1) of SDC to 4.2 x 10(-17) m(3) N-1 s(-1) of SDC2 at 900 degrees C. The activation energy for densification as high as 5.5 +/- 0.5 eV for SDC2 contributes to the formation of liquid phase in the grain boundary. The open circuit voltage of the cell using SDC2 as electrolyte as high as 0.78 V at 600 degrees Cunder solid oxide fuel cell (SOFC) working conditions demonstrates its promising for SOFC electrolyte. (c) 2012 Elsevier B.V All rights reserved.
引用
收藏
页码:367 / 372
页数:6
相关论文
共 50 条
  • [31] Methane-fueled IT-SOFCs with facile in situ inorganic templating synthesized mesoporous Sm0.2Ce0.8O1.9 as catalytic layer
    Wang, Kang
    Ran, Ran
    Shao, Zongping
    JOURNAL OF POWER SOURCES, 2007, 170 (02) : 251 - 258
  • [32] Characterization of nanosized Ce0.8Sm0.2O1.9-infiltrated Sm0.5Sr0.5Co0.8Cu0.2O3-δ cathodes for solid oxide fuel cells
    Fu, Yen-Pei
    Ouyang, Jie
    Li, Chien-Hung
    Hu, Shao-Hua
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2012, 37 (24) : 19027 - 19035
  • [33] La0.6Ca0.4Fe0.8Ni0.2O3-δ - Sm0.2Ce0.8O1.9 composites as symmetrical bi-electrodes for solid oxide fuel cells through infiltration and in-situ exsolution
    Ding, Xifeng
    Liu, Hao
    Gao, Zhipeng
    Hua, Guixiang
    Wang, Lixi
    Ding, Liming
    Yuan, Guoliang
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (39) : 24968 - 24977
  • [34] Influence of Lithium on the Sintering Behavior and Electrical Properties of Ce0.8Gd0.2O1.9 for Intermediate-Temperature Solid Oxide Fuel Cells
    Accardo, Grazia
    Ferone, Claudio
    Cioffi, Raffaele
    ENERGY TECHNOLOGY, 2016, 4 (03) : 409 - 416
  • [35] Preparation and Electrochemical Properties of La1.0Sr1.0FeO4+δ-Sm0.2Ce0.8O1.9 Composite Cathode for Intermediate Temperature Solid Oxide Fuel Cells
    Xie Yan
    Wang Yarong
    Jin Chao
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 : 536 - 540
  • [36] Characteristics of Li2CO3 as sintering aid for Ce0.8Sm0.2O2-δ electrolyte in solid oxide fuel cells
    Park, Gwang Seon
    Mo, Su In
    Kim, Jun Ho
    Yun, Jeong Woo
    KOREAN JOURNAL OF CHEMICAL ENGINEERING, 2022, 39 (07) : 1796 - 1804
  • [37] Characteristics of Li2CO3 as sintering aid for Ce0.8Sm0.2O2−δ electrolyte in solid oxide fuel cells
    Gwang Seon Park
    Su In Mo
    Jun Ho Kim
    Jeong Woo Yun
    Korean Journal of Chemical Engineering, 2022, 39 : 1796 - 1804
  • [38] In-Situ Synthesis of Sm0.5Sr0.5Co0.5O3-δ@Sm0.2Ce0.8O1.9 Composite Oxygen Electrode for Electrolyte-Supported Reversible Solid Oxide Cells (RSOC)
    Yang, Xiaoxing
    Miao, He
    Pan, Baowei
    Chen, Ming
    Yuan, Jinliang
    ENERGIES, 2022, 15 (06)
  • [39] Synthesis and characterization of Ce0.8Sm0.2O1.9 nanopowders using an acrylamide polymerization process
    Zheng Yingping
    Wang Shaorong
    Wang Zhenrong
    Wu Liwei
    Sun Yueming
    JOURNAL OF RARE EARTHS, 2010, 28 (01) : 92 - 95
  • [40] Enhanced ionic conductivity of Ce0.8Sm0.2O2-δ by Sr addition
    Gao, Zhan
    Liu, Xingmin
    Bergman, Bill
    Zhao, Zhe
    JOURNAL OF POWER SOURCES, 2012, 208 : 225 - 231