Structural and magnetic properties of Fe-Cr-Al alloys with DO3-type structure

被引:20
|
作者
Satula, D
Dobrzynski, L
Waliszewski, J
Szymanski, K
Recko, K
Malinowski, A
Bruckel, T
Scharpf, O
Blinowski, K
机构
[1] DESY,HASYLAB,D-2000 HAMBURG 52,GERMANY
[2] INST MAX VON LAUE PAUL LANGEVIN,F-38042 GRENOBLE,FRANCE
[3] INST ATOM ENERGY,PL-15400 OTWOCK,POLAND
关键词
Fe-Cr-Al alloys; crystal structure; magnetic moment;
D O I
10.1016/S0304-8853(96)00758-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
X-ray, neutron, magnetization and Mossbauer studies in the temperature range 10-300 K are reported for Fe3-xCrxAl system with x < 0.6. The experiments indicate that a single phase having the DO3-type structure is maintained in the range of Cr concentration studied. It was found that Cr atoms occupy preferentially B-sites and the lattice constant decreases with increasing concentration of chromium. The magnetic moment of chromium is small and diminishes the value of neighbouring iron atoms by about 0.1 mu(B) per Cr atom. The magnetic moments of iron at (A, C) and B sites were estimated to be 1.54 (22), 2.58 (22), 1.51 (27) and 2.32 (14) mu(B), for T = 10 and 300 K, respectively. The magnetic moment of iron decreases by 0.37(10) and 0.26(6)mu(B) at 10 K and T = 300 K, respectively, if one aluminium atom is found as a nearest neighbour of iron.
引用
收藏
页码:240 / 252
页数:13
相关论文
共 50 条
  • [41] Magnetic circular dichroism at transition metal L2,3 edges in DO3-type (Fe1-xMnx)3Al alloys
    Soda, K
    Yoshimoto, O
    Nozaki, H
    Takeuchi, T
    Mizutani, U
    Kato, H
    Kato, M
    Nishino, Y
    Imada, S
    Suga, S
    Matsushita, T
    Saitoh, Y
    JOURNAL OF SYNCHROTRON RADIATION, 2001, 8 (02) : 455 - 456
  • [42] High-temperature sulphidation behaviour of Fe-Cr-Al and Fe-Cr-Al-Y alloys
    Pillis, MF
    Ramanathan, LV
    CORROSION PREVENTION & CONTROL, 2003, 50 (04): : 167 - +
  • [43] Interdiffusion in Low-Al Fe-Cr-Al Alloys at 1000 °C
    Yoneda, Suzue
    Hayashi, Shigenari
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2023, 54 (12): : 4931 - 4939
  • [44] THE INFLUENCE OF SULFUR ON ADHERENCE OF AL2O3 GROWN ON FE-CR-AL ALLOYS
    SIGLER, DR
    OXIDATION OF METALS, 1988, 29 (1-2): : 23 - 43
  • [45] The Structural, Electronic, and Magnetic Properties of Binary Heusler Alloys ZCl3 (Z = Li, Na, K, Rb) with DO3-Type Structure from First Principle Calculations
    Jun-Tao Song
    Xiu-Mei Wei
    Jian-Min Zhang
    Journal of Superconductivity and Novel Magnetism, 2019, 32 : 3217 - 3226
  • [46] The Morphology of Thermally Grown α-Al2O3 Scales on Fe-Cr-Al Alloys
    Vladimir K. Tolpygo
    Oxidation of Metals, 1999, 51 : 449 - 477
  • [47] The morphology of thermally grown α-Al2O3 scales on Fe-Cr-Al alloys
    Tolpygo, VK
    OXIDATION OF METALS, 1999, 51 (5-6): : 449 - 477
  • [48] Criteria for the formation of protective Al2O3 scales on Fe-Al and Fe-Cr-Al alloys
    Zhang, ZG
    Gesmundo, F
    Hou, PY
    Niu, Y
    CORROSION SCIENCE, 2006, 48 (03) : 741 - 765
  • [49] RESISTANCE OF ALLOYS OF THE FE-CR-AL SYSTEM IN A NONISOTHERMAL SODIUM FLOW
    KURAPOV, YA
    SHESTAKOVA, EY
    KRAEV, ND
    ZHURAVLEVA, TS
    GONCHARENKO, AB
    PROTECTION OF METALS, 1991, 27 (05): : 632 - 635
  • [50] Comments on "Growth rates of alumina scales on Fe-Cr-Al alloys"
    Pieraggi, B
    OXIDATION OF METALS, 2005, 64 (5-6): : 397 - 403