Micropillar compression deformation of single crystals of the intermetallic compound Γ-Fe4Zn9

被引:15
|
作者
Hashizume, Yukichika [1 ]
Inomoto, Masahiro [1 ]
Okamoto, Norihiko L. [1 ,2 ,4 ]
Takebayashi, Hiroshi [3 ]
Inui, Haruyuki [1 ,2 ]
机构
[1] Kyoto Univ, Dept Mat Sci & Engn, Kyoto 6068501, Japan
[2] Kyoto Univ, Ctr Elements Strategy Initiat Struct Mat ESISM, Kyoto 6068501, Japan
[3] Nippon Steel Corp Ltd, 20-1 Shintomi, Futtsu, Chiba 2938511, Japan
[4] Tohoku Univ, Inst Mat Res, Aoba Ku, Sendai, Miyagi 9808577, Japan
关键词
Intermetallic compounds; Plastic deformation; Micropillar compression; Dislocation structures; Focused ion beam (FIB); Transmission electron microscopy (TEM); FE-ZN SYSTEM; X-RAY; PLASTIC-DEFORMATION; MECHANICAL-PROPERTIES; STRUCTURE REFINEMENT; FRACTURE-TOUGHNESS; YIELD STRENGTH; COATING LAYER; PHASE; GAMMA;
D O I
10.1016/j.actamat.2020.08.062
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The plastic deformation behavior of single crystals of the Gamma (Fe4Zn9) phase compound in the Fe-Zn system, which has been believed to be the most detrimental phase causing brittle failure in the coating layer (such as powdering) on galvannealed (GA) steels, has been investigated by micropillar compression tests at room temperature as a function of crystal orientation and specimen size. All micropillar specimens exhibit rich deformability in compression. Two distinct slip systems, {(1) over bar 01}<111> and {(1) over bar 01}<010>, are observed to operate. The critical resolved shear stress (CRSS) values for {(1) over bar 01}<111> and {(1) over bar 01}<010> both obey an inverse power-law scaling against the micropillar size with an exponent of -0.245 and - 0.046, respectively. The bulk CRSS values for these two slip systems are estimated respectively to be 238 and 649 MPa by considering the specimen size effects of CRSS. The crystal orientation range for the operation of {(1) over bar 01}<010> slip is limited to the vicinity of < 111 > because of the considerable difference in the CRSS values for these two slip systems. Dislocations with b (Burgers vector) = (010) dissociate into two partial dislocations, while those with b = 1/2<111> do not show any dissociation, both of which are consistent with the result of theoretical calculation of the generalized stacking fault energy on the {(1) over bar 01} slip plane. Possible reasons for brittle failure related to the Gamma phase occurring in the coating layer on GA steels are discussed based on the results obtained. (C) 2020 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:514 / 522
页数:9
相关论文
共 50 条
  • [21] Fracture Toughness of Fe-Zn Intermetallic Compound Layer
    Inoue, Junya
    Miwa, Satoshi
    Koseki, Toshihiko
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2014, 100 (03): : 383 - 389
  • [22] Anomalous size-dependent strength in micropillar compression deformation of commercial-purity aluminum single-crystals
    Takata, Naoki
    Takeyasu, Soichiro
    Li, Hongmei
    Suzuki, Asuka
    Kobashi, Makoto
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 772
  • [23] Understanding size effects on the strength of single crystals through high-temperature micropillar compression
    Soler, Rafael
    Wheeler, Jeffrey M.
    Chang, Hyung-Jun
    Segurado, Javier
    Michler, Johann
    Llorca, Javier
    Molina-Aldareguia, Jon M.
    ACTA MATERIALIA, 2014, 81 : 50 - 57
  • [24] Room temperature deformation of single crystals of Ti5Si3 with the hexagonal D88 structure investigated by micropillar compression tests
    Kishida, Kyosuke
    Fukuyama, Takayoshi
    Maruyama, Takuto
    Inui, Haruyuki
    SCIENTIFIC REPORTS, 2020, 10 (01)
  • [25] Micropillar compression of single crystal tungsten carbide, Part 1: Temperature and orientation dependence of deformation behaviour
    Jones, Helen
    Tong, Vivian
    Ramachandramoorthy, Rajaprakash
    Mingard, Ken
    Michler, Johann
    Gee, Mark
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 102
  • [26] Deformation mechanisms of Mg-Ca-Zn alloys studied by means of micropillar compression tests
    Wang, Jingya
    Chen, Yiwen
    Chen, Zhe
    Llorca, Javier
    Zeng, Xiaoqin
    ACTA MATERIALIA, 2021, 217
  • [27] Plastic deformation of bulk and micropillar single crystals of Mo5Si 3 with the tetragonal D8m structure
    Kishida, Kyosuke
    Chen, Zhenghao
    Matsunoshita, Hirotaka
    Maruyama, Takuto
    Fukuyama, Takayoshi
    Sasai, Yuta
    Inui, Haruyuki
    Heilmaier, Martin
    INTERNATIONAL JOURNAL OF PLASTICITY, 2022, 155
  • [28] Room-temperature deformation of single crystals of transition-metal disilicides (TMSi2) with the C11b (TM = Mo) and C40 (TM = V, Cr, Nb and Ta) structures investigated by micropillar compression
    Kishida, Kyosuke
    Nakatsuka, Satoshi
    Nose, Hiroaki
    Inui, Haruyuki
    ACTA MATERIALIA, 2022, 223
  • [29] Micropillar compression of single crystal tungsten carbide, part 2: Lattice rotation axis to identify deformation slip mechanisms
    Tong, Vivian
    Jones, Helen
    Mingard, Ken
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 103
  • [30] Insight into the deformation behavior of niobium single crystals under uniaxial compression and tension at the nanoscale
    Kim, Ju-Young
    Jang, Dongchan
    Greer, Julia R.
    SCRIPTA MATERIALIA, 2009, 61 (03) : 300 - 303