Effect of double-step homogenization treatments on the microstructure and mechanical properties of Al-Cu-Li-Zr alloy

被引:46
|
作者
Deng, Yunlai [1 ,2 ,3 ]
Xu, Jinjun [1 ,2 ]
Chen, Jiqiang [4 ,5 ]
Guo, Xiaobin [3 ]
机构
[1] Cent South Univ, Light Alloy Res Inst, Changsha, Peoples R China
[2] Cent South Univ, State Key Lab High Performance & Complex Mfg, Changsha, Peoples R China
[3] Cent South Univ, Sch Mat Sci & Engn, Changsha, Peoples R China
[4] Jiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou, Peoples R China
[5] Dongguan Eontec Co Ltd, Dongguan 523662, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 795卷 / 795期
基金
美国国家科学基金会; 中国博士后科学基金;
关键词
Al-Cu-Li-Zr alloy; Homogenization; beta ' phase; Mechanical properties; Microstructures; RECRYSTALLIZATION BEHAVIOR; VOLUME FRACTION; T-1; PHASE; EVOLUTION; MG; PRECIPITATION; DEFORMATION; ADDITIONS; STRENGTH; AG;
D O I
10.1016/j.msea.2020.139975
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Al3Zr particles formed in the Al-Cu-Li-Zr alloy during single and double-step homogenization treatments contributed to various microstructures and mechanical properties during the subsequent thermomechanical treatment. Compared with the single-step homogenization treatment (ST), the double-step homogenization treatment (DT) generated higher density and more uniform distribution of beta' (Al3Zr) phases, which makes the alloy retain more substructures and improve the initial strength of solid solution. During the ageing process, Al3Zr particles induced the T-1 precipitation in grain interior and the width of PFZ get narrowed. Therefore, the strength and toughness of the DT sample improved in peak aged state compared with that of the ST sample. The peak hardness value of DT sample is 167.8 HV, which is higher than that of ST sample with 153.1 HV. Furthermore, the tensile strength and elongation of the DT sample at peak aged state (521 MPa, 556 MPa and 8.8 %, respectively) are higher than those of the STA sample (492 MPa, 535 MPa and 6.7 %, respectively), and the impact toughness of the DTA sample (13.2 J cm(-2)) is also higher than those of STA sample (9.1 J cm(-2)). Strength model showed that more uniform distribution of Al3Zr phases and substructures improve the initial strength of solid solution state, which increased by 16 MPa in the DT sample compared with the ST sample. The promotion of T i precipitation inducing the strength increased by 18 MPa in the DT sample at the peak aged state compared with that of the ST sample. The increase of elongation and toughness contributed from the oriented grains with finer distribution and higher Schmid factor, less grain boundaries precipitates and narrower PFZ width.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Effects of enhanced solution treatment on microstructure and mechanical properties of Al-Cu-Li-Sc alloy
    Yang, Ruibin
    Zhi, Qian
    Wang, Feizhou
    Zhang, Yunjie
    Liu, Zhongxia
    Wang, Jiefang
    Tan, Xinrong
    Chen, Yadong
    Cao, Yanjie
    MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (10) : 1201 - 1211
  • [22] Effect of composition on microstructure and properties of as-cast 2196 Al-Cu-Li alloy
    Chen, Kaixuan
    Li, Zongxuan
    Cao, Yudong
    Wu, Xuehua
    Chen, Xiaohua
    Wang, Zidong
    Tian, Yuxing
    Pan, Shiwei
    MATERIALS SCIENCE AND TECHNOLOGY, 2022, 38 (15) : 1168 - 1184
  • [23] Effect of Rolling Reduction on Microstructures and Mechanical Properties of Sc-Containing Al-3.2Cu-1.5Li Alloy
    Wang, Jian
    Kan, Yun
    Xu, Wenting
    Lu, Yalin
    Zhou, Dongshuai
    Li, Shenao
    METALS, 2023, 13 (04)
  • [24] Effect of Trace Sc Addition on Microstructure and Mechanical Properties of Al-Zn-Mg-Cu-Zr Alloy
    Huang, Yuchen
    Xia, Linfei
    Yang, Huabing
    Wang, Chengguo
    Wu, Yuying
    Liu, Xiangfa
    MATERIALS, 2025, 18 (03)
  • [25] Effect of heat treatment on the microstructure and mechanical properties of cryogenic rolling 2195 Al-Cu-Li alloy
    He, Guoai
    Li, Kai
    Yang, Yong
    Liu, Yu
    Wu, Wenke
    Huang, Cheng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 822
  • [26] Regulating the microstructure and mechanical properties of Al-Cu-Li alloys via optimizing Cu/Li ratio and homogenization
    Liu, Fuyuan
    Wang, Chong
    Li, Guangshu
    Wang, Guantao
    Guo, Enyu
    Zhang, Zhirou
    Chen, Zongning
    Kang, Huijun
    Wang, Tongming
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1004
  • [27] Effect of isothermal multidirectional compression on microstructure and mechanical properties of Al-Zn-Mg-Cu-Zr alloy with minor Sc addition
    Sun, Qian
    Xu, Chao
    Yu, Sha
    Hu, Zhili
    MATERIALS CHEMISTRY AND PHYSICS, 2024, 313
  • [28] Effect of Sc and Zr on Microstructure and Mechanical Properties of As-Cast Al-Li-Cu Alloys
    Wang, Yang
    Li, Zheng
    Yu, Tianfu
    Medjahed, Aboubakr
    Wu, Ruizhi
    Hou, Legan
    Zhang, Jinghuai
    Li, Xinlin
    Zhang, Milin
    ADVANCED ENGINEERING MATERIALS, 2018, 20 (04)
  • [29] The effect of major constituents on microstructure and mechanical properties of cast Al-Li-Cu-Zr alloy
    Wu, Liang
    Li, Xianfeng
    Wang, Haowei
    MATERIALS CHARACTERIZATION, 2021, 171
  • [30] Microstructure evolution of the 1469 Al-Cu-Li-Sc alloy during homogenization
    Jia, Min
    Zheng, Ziqiao
    Gong, Zhu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 614 : 131 - 139