Corrosion Behaviour of 316L Stainless Steel in Hot Dilute Sulphuric Acid Solution with Sulphate and NaCl

被引:9
作者
Zhang, Jian [1 ]
Ju, Pengfei [2 ]
Wang, Chaoli [1 ]
Dun, Yuchao [1 ]
Zhao, Xuhui [1 ]
Zuo, Yu [1 ]
Tang, Yuming [1 ]
机构
[1] Beijing Univ Chem Technol, Key Lab Electrochem Proc & Technol Mat, Beijing 100029, Peoples R China
[2] Shanghai Aerosp Equipment Manufacture Co Ltd, Shanghai 200245, Peoples R China
基金
中国国家自然科学基金;
关键词
316L SS; hot dilute sulphuric acid; corrosion; sodium chloride; sodium sulphate; corrosion products; PITTING CORROSION; SINGLE PIT; CHLORIDE; TEMPERATURE; INITIATION; GROWTH; IONS; DISSOLUTION; CHROMIUM; AISI-304;
D O I
10.1134/S207020511901026X
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The corrosion behaviour of 316L stainless steel (316L SS) in 10% H2SO4 solution (94 degrees C) with various concentrations of NaCl (0-0.085 mol/L) was studied by immersion corrosion test and polarization methods, combined with SEM/EDS, XPS and XRD tests. The influence of NaCl on the corrosion of 316L SS was investigated. The results showed that at lower NaCl contents (0-0.0085 mol/L), the steel presented a general corrosion characteristic with a higher corrosion speed and the corrosion rate increased with the NaCl content. At higher NaCl contents (0.017 mol/L), the corrosion rate decreased remarkably due to the protective corrosion products precipitation which contained metallic sulphates and NaHSO4. However, the higher concentration of chloride ions caused micron pitting-like local dissolution on the surface. The addition of Na2SO4 effectively inhibited general corrosion of the steel because of a dense and continuous products layer enriched with more NaHSO4 and metallic sulphates formed.
引用
收藏
页码:148 / 156
页数:9
相关论文
共 34 条
[1]   A general model for the repassivation potential as a function of multiple aqueous solution species [J].
Anderko, A ;
Sridhar, N ;
Dunn, DS .
CORROSION SCIENCE, 2004, 46 (07) :1583-1612
[2]   Initiation and growth of a single pit on 316L stainless steel: Influence of SO42- and ClO4- anions [J].
Aouina, N. ;
Balbaud-Celerier, F. ;
Huet, F. ;
Joiret, S. ;
Perrot, H. ;
Rouillard, F. ;
Vivier, V. .
ELECTROCHIMICA ACTA, 2013, 104 :274-281
[3]   Single pit initiation on 316L austenitic stainless steel using scanning electrochemical microscopy [J].
Aouina, N. ;
Balbaud-Celerier, F. ;
Huet, F. ;
Joiret, S. ;
Perrot, H. ;
Rouillard, F. ;
Vivier, V. .
ELECTROCHIMICA ACTA, 2011, 56 (24) :8589-8596
[4]   Dependence of critical pitting temperature on the concentration of sulphate ion in chloride-containing solutions [J].
Deng, Bo ;
Jiang, Yiming ;
Liao, Jiaxing ;
Hao, Yunwei ;
Zhong, Cheng ;
Li, Jin .
APPLIED SURFACE SCIENCE, 2007, 253 (18) :7369-7375
[5]   Pit growth studies in stainless steel foils. II. Effect of temperature, chloride concentration and sulphate addition [J].
Ernst, P ;
Newman, RC .
CORROSION SCIENCE, 2002, 44 (05) :943-954
[6]   In situ local dissolution of duplex stainless steels in 1 M H2SO4+1 M NaCl by electrochemical scanning tunneling microscopy [J].
Femenia, M ;
Pan, J ;
Leygraf, C .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2002, 149 (06) :B187-B197
[7]   Effect of low-temperature plasma nitriding on corrosion of 304L stainless steel in sulfate and chloride solutions [J].
Flis, J ;
Kuczynska, M .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2004, 151 (11) :B573-B580
[8]   The effect of trace boron on corrosion resistance of the casted 0.04C-16Cr ferritic stainless steels in H2SO4 medium [J].
Guo, Tieming ;
Zhang, Dingcang ;
Han, Changsong ;
Hui, Zhi ;
Zhao, Liming .
NEW MATERIALS AND PROCESSES, PTS 1-3, 2012, 476-478 :263-268
[9]  
Hajjaji S.E., 1996, CORROSION, V52, P865, DOI [10.5006/1.3292079, DOI 10.5006/1.3292079]
[10]  
Hashiro H., 1990, CORROS SCI, V31, P485, DOI [10.1016/0010-938X(90)90150-4, DOI 10.1016/0010-938X(90)90150-4]