Alloy Design of 5%Mn-Cr-C System Austenitic Steel

被引:0
|
作者
Tsukahara, Hirokazu [1 ]
Masumura, Takuro [1 ]
Tsuchiyama, Toshihiro [2 ,3 ]
Takaki, Setsuo [2 ,3 ]
Nakashima, Koichi [4 ]
Hase, Kazukuni [4 ]
Endo, Shigeru [4 ]
机构
[1] Kyushu Univ, Nishi Ku, Fukuoka 8190395, Japan
[2] Kyushu Univ, Grad Sch Engn, Dept Mat Sci & Engn, Fukuoka 812, Japan
[3] Kyushu Univ, Int Inst Carbon Neutral Energy Res WPI I2CNER, Fukuoka 812, Japan
[4] JFE Steel Corp, Steel Res Lab, Pittsburgh, PA USA
来源
TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN | 2013年 / 99卷 / 08期
关键词
austenitic steel; medium-manganese steel; stability of austenite; work hardening; deformation-induced martensite; deformation twin; stacking fault energy; TRANSFORMATION; DEFORMATION; DEPENDENCE; MECHANISM; MN;
D O I
10.2355/tetsutohagane.99.509
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The range of chemical composition for obtaining austenitic single structure was defined in medium-manganese carbon steels. Among the defined composition, Fe-5%Mn-4%Cr-(0.8 similar to 1.4)%C was selected as the optimum range of composition to form stable austenitic structure. The tensile property and deformation substructure were investigated in the austenitic steels with corresponding composition. As a result, the work hardening behavior of the steels was varied depending on the carbon content, which was closely related with the development of deformation microstructure. In the 0.8%C steel, deformation-induced martensitic transformation as well as deformation twinning caused large work hardening until fracture took place. With increasing carbon content, namely increasing SFE, the deformation mode tended to shift to dislocation slipping, resulting in the lower work hardening rate. This trend seems to be similar to conventional TWIP steel where the work hardening behavior is explained with SFE.
引用
收藏
页码:509 / 516
页数:8
相关论文
共 50 条
  • [21] Fatigue behaviors and damage mechanism of a Cr-Mn-N austenitic steel
    Lv, Z.
    Cai, P.
    Yu, T.
    Jin, Y.
    Zhang, H.
    Fu, W.
    Zhai, T.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 691 : 103 - 109
  • [22] INFLUENCE OF MOLYBDENUM ON PROPERTIES OF AUSTENITIC CR-MN-NI-AL STEEL
    KARTASHO.LI
    ZUDIN, IF
    BANNYKH, OA
    RUSSIAN METALLURGY-METALLY-USSR, 1971, (04): : 131 - &
  • [23] WELDED JOINT FAILURE OF AUSTENITIC CREEP RESISTING Cr-Mn STEEL
    Bernasovsky, P.
    Orszaghova, J.
    WELDING IN THE WORLD, 2009, 53 (7-8) : 20 - 23
  • [24] Flow stress and microstructural evolution during hot working of alloy 22Cr-13Ni-5Mn-0.3N austenitic stainless steel
    Mataya, MC
    Perkins, CA
    Thompson, SW
    Matlock, DK
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (05): : 1251 - 1266
  • [25] TEMPERING PROCESSES STUDIES IN AUSTENITIC CR-MN-C STEELS
    NEMIROVSKIY, YR
    NEMIROVSKIY, MR
    KIBALNIK, VD
    MIKHAYLOV, SV
    FIZIKA METALLOV I METALLOVEDENIE, 1989, 68 (03): : 531 - 539
  • [26] Corrosion resistance of oxidation-induced Mn depletion layer on austenitic Fe24Mn4Al5Cr alloy
    Zhu, Xuemei
    Zhang, Zhenwei
    Wang, Xinjian
    Zhang, Yansheng
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2015, 44 (12): : 3197 - 3201
  • [27] STUDY ON A CRYOGENIC AND NON-MAGNETIC AUSTENITIC STEEL, 30Mn23Al4Cr5.
    Zhang Yansheng
    Jinshu Xuebao/Acta Metallurgica Sinica, 1983, 19 (04):
  • [28] THE INFLUENCE OF NON-METALLIC INCLUSION ON THE FRACTURE BEHAVIORS OF 25MN-5CR-LNI AUSTENITIC STEEL
    MAEKAWA, I
    TANABE, Y
    LEE, JH
    NISHIDA, S
    ENGINEERING FRACTURE MECHANICS, 1987, 28 (5-6) : 577 - 587
  • [29] Phonon dispersion and elastic constants in Fe-Cr-Mn-Ni austenitic steel
    Danilkin, SA
    Fuess, H
    Wieder, T
    Hoser, A
    JOURNAL OF MATERIALS SCIENCE, 2001, 36 (04) : 811 - 814
  • [30] HIGH-TEMPERATURE OXIDATION OF A COMMERCIAL CR-MN AUSTENITIC STEEL IN AIR
    GESMUNDO, F
    DEASMUNDIS, C
    BATTILANA, G
    RUEDL, E
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1987, 38 (07): : 367 - 375