Microporosity formation in partially melted zone during welding of high nitrogen austenitic stainless steels

被引:32
作者
Kamiya, O [1 ]
Chen, ZW
Kikuchi, Y
机构
[1] Akita Univ, Fac Engn & Resources Sci, Akita 010, Japan
[2] Auckland Univ Technol, Fac Sci & Engn, Auckland, New Zealand
[3] Osaka Univ, Joining & Welding Res Inst, Suita, Osaka 565, Japan
关键词
Austenite - Electric arc welding - Energy dispersive spectroscopy - Hardness - Melting - Microporosity - Microstructure - Nitrogen - Particles (particulate matter) - Pore size - Scanning electron microscopy - Solubility;
D O I
10.1023/A:1015427204629
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Gas tungsten arc welding experiments were conducted using austenitic stainless steel containing 0.51%N and 0.78%N. Microstructure observation and hardness measurement were made to study the loss of nitrogen. It was found that welding resulted in a considerable loss of hardness in the weld metal for the case of 0.78%N steel, but not for 0.51%N steel. We explain this in terms of a higher nitrogen content enabling a significantly smaller critical pore size and hence N-2 porosity formation to be energetically more favourable. The major finding was that, for the case of 0.78%N steel, a band of microporosity was observed along and near the complete fusion boundary of the weld. It was identified that these micropores were present in the parent metal, not in the weld metal. Partial melting in the zone next to the complete fusion boundary resulted in a nitrogen content significantly higher than the solubility of nitrogen in the liquid channels or pockets. Nitrogen gas pores then formed and became trapped in that zone. Supporting this forming mechanism of microporosity band was the fact that hardness decreased in that zone due to the loss of nitrogen in gamma phase matrix for solute strengthening and that nitride particles disappeared after welding. (C) 2002 Kluwer Academic Publishers.
引用
收藏
页码:2475 / 2481
页数:7
相关论文
共 16 条
  • [1] Gavriljuk V.G., 1999, High Nitrogen Steels
  • [2] GROB V, 1999, MATER SCI FORUM, V318, P597
  • [3] Recent developments on the weldability of a new high nitrogen stainless steel
    Harzenmoser, M
    Rennhard, C
    Hereth, M
    Diener, M
    [J]. HIGH NITROGEN STEELS '98, 1999, 318-3 : 591 - 596
  • [4] Influence of shielding gas composition and welding parameters on the N-content and corrosion properties of welds in N-alloyed stainless steel grades
    Hertzman, S
    Pettersson, RJ
    Blom, R
    Kivineva, E
    Eriksson, J
    [J]. ISIJ INTERNATIONAL, 1996, 36 (07) : 968 - 976
  • [5] An experimental and theoretical study of nitrogen flux in stainless steel TIG welds
    Hertzman, S
    Wessman, S
    [J]. HIGH NITROGEN STEELS '98, 1999, 318-3 : 579 - 589
  • [6] INAGAKI M, 1985, STAINLESS STEEL HDB, P732
  • [7] Comparison of welding behavior of SUS316L steel by gas tungsten and gas metal arc processes in high pressure nitrogen atmosphere
    Kamiya, O
    Kikuchi, Y
    [J]. HIGH NITROGEN STEELS '98, 1999, 318-3 : 609 - 614
  • [8] KAMIYA O, 2001, P INT C PROC MAN ADV
  • [9] KIKUCHI M, 1989, P INT C HIGH NITR ST, P7
  • [10] Nitrogen content of 316L weld metal and its fine particle by means of high-pressure MIG arc welding
    Kikuchi, Y
    Matsuda, F
    Okabe, T
    Ohta, M
    [J]. ISIJ INTERNATIONAL, 1996, 36 (07) : 977 - 982