Twinning and dynamic precipitation upon hot compression of a Mg-Gd-Y-Nd-Zr alloy

被引:38
作者
Hou, Xiuli [1 ,2 ]
Cao, Zhanyi [2 ]
Sun, Xu [2 ]
Wang, Lidong [1 ,2 ]
Wang, Limin [1 ]
机构
[1] CAS, State Key Lab Rare Earth Resource Utilizat, Changchun Inst Appl Chem, Changchun 130022, Peoples R China
[2] Jilin Univ, Key Lab Automobile Mat, Minist Educ, Changchun 130025, Peoples R China
关键词
Mg-Gd-Y-Nd-Zr alloy; Hot compression; Deformation twinning; Dynamic precipitation; DEFORMATION MECHANISMS; RECRYSTALLIZATION; 250-DEGREES-C;
D O I
10.1016/j.jallcom.2012.02.081
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The microstructure evolution in Mg-8Gd-2Y-1Nd-0.3Zn-0.6Zr alloy subjected to hot compression at 350 degrees C and the strain rate of 0.5 s(-1) was systematically investigated. Twinning and dynamic precipitation are two characteristic processes during compressive deformation. Crystallographic analysis indicates that the majority of deformation twins are of the {1 0 (1) over bar 1}-{1 0 (1) over bar 2} type, possessing the misorientation of 37.5 degrees from parent grain about the c-axis. With strain accumulation, the twin-twin intersections lead to grain fragmentation of the original grains. Extensive dynamic precipitation is observed in the alloy. The beta precipitates with irregular shapes are observed to form firstly on twin boundaries. Then the formation of rectangular beta' precipitates proceeds in the Mg matrix. The morphology of the beta' precipitates differs from that of the same phase obtained by solution and ageing treatment (i.e. T6 heat treatment), but their orientation relationships with Mg matrix keep consistent. Crown Copyright (C) 2012 Published by Elsevier B. V. All rights reserved.
引用
收藏
页码:103 / 109
页数:7
相关论文
共 23 条
[1]   Relationship between deformation twinning and surface step formation in AZ31 magnesium alloys [J].
Ando, D. ;
Koike, J. ;
Sutou, Y. .
ACTA MATERIALIA, 2010, 58 (13) :4316-4324
[2]  
[Anonymous], 2003, Magnesium alloys containing rare earth metals: structure and properties
[3]   Influence of aging pre-treatment on the compressive deformation of WE54 alloy [J].
Beladi, H. ;
Barnett, M. R. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 452 (306-312) :306-312
[4]   Precipitation in a Mg-10Gd-3Y-0.4Zr (wt.%) alloy during isothermal ageing at 250°C [J].
He, S. M. ;
Zeng, X. Q. ;
Peng, L. M. ;
Gao, X. ;
Nie, J. F. ;
Ding, W. J. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2006, 421 (1-2) :309-313
[5]   Structure and mechanical properties of extruded Mg-Gd based alloy sheet [J].
Hou, Xiuli ;
Peng, Qiuming ;
Cao, Zhanyi ;
Xu, Shiwei ;
Kamado, Shigeharu ;
Wang, Lidong ;
Wu, Yaoming ;
Wang, Limin .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 520 (1-2) :162-167
[6]  
Humphreys F.J., 2005, RECRYSTALLIZATION RE
[7]   Interaction of recrystallization and precipitation:: The effect of Al3SC on the recrystallization behaviour of deformed aluminium [J].
Jones, MJ ;
Humphreys, FJ .
ACTA MATERIALIA, 2003, 51 (08) :2149-2159
[8]  
Kainer K.U., 2003, MAGNESIUM ALLOYS TEC
[9]   Elastic strain energies of sphere, plate and needle inclusions [J].
Kato, M ;
Fujii, T ;
Onaka, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 211 (1-2) :95-103
[10]   THEORETICAL-ANALYSIS OF STRAIN-INDUCED SHAPE CHANGES IN CUBIC PRECIPITATES DURING COARSENING [J].
KHACHATURYAN, AG ;
SEMENOVSKAYA, SV ;
MORRIS, JW .
ACTA METALLURGICA, 1988, 36 (06) :1563-1572