The friction and wear of electroless Ni-P matrix with PTFE and/or SiC particles composite

被引:113
|
作者
Wu, YT [1 ]
Liu, HZ [1 ]
Shen, B [1 ]
Liu, L [1 ]
Hu, WB [1 ]
机构
[1] Shanghai Jiao Tong Univ, State Key Lab Met Matrix Composites, Shanghai 200030, Peoples R China
关键词
electroless nickel plating; SiC particles; PTFE particles; friction and wear;
D O I
10.1016/j.triboint.2005.04.032
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this paper, the friction behaviour and wear mechanism of electroless Ni-P matrix with PTFE and/or SiC particles composite coating are investigated by virtue of ring-on-disk wear machine at a high load of 150 N. The worn surface, wear debris and the composition changes after wear were characterized using scanning electron microscopy (SEM) and energy-dispersive analysis of X-ray (EDAX). By comparison with Ni-P and Ni-P-SiC coatings, the results indicated that the combination of a PTFE-rich mechanical mixed layer (PRMML) formed on the worn surface and hard SiC were responsible for the good tribological properties of the hybrid Ni-P-PTFE-SiC composites at high load. After heat treatment at 400 degrees C for 1h, the wear rate of Ni-P matrix composites decreased with corresponding increase in microhardness. During sliding, an obvious decrease in the temperature rise with PTFE addition was attributed to the good anti-friction of PTFE. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:553 / 559
页数:7
相关论文
共 50 条
  • [31] Evaluation of Wear Properties for Ni-P Electroless Coatings
    Hadipour, A.
    Bahrololoom, M. E.
    Monirvaghefi, S. M.
    Bahramkia, A. R.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (09) : 1733 - 1743
  • [32] Wear performance and mechanism of electroless Ni-P coating
    Staia, MH
    Castillo, EJ
    Puchi, ES
    Lewis, B
    Hintermann, HE
    SURFACE & COATINGS TECHNOLOGY, 1996, 86-7 (1-3): : 598 - 602
  • [33] The effect of heat treatment on the microstructure of electroless Ni-P coatings containing SiC particles
    Chen, CK
    Feng, HM
    Lin, HC
    Hon, MH
    THIN SOLID FILMS, 2002, 416 (1-2) : 31 - 37
  • [34] Electroless plating Ni-P matrix composite coating reinforced by carbon nanotubes
    邓福铭
    陈小华
    陈卫祥
    李文铸
    TransactionsofNonferrousMetalsSocietyofChina, 2004, (04) : 681 - 685
  • [35] Electroless plating Ni-P matrix composite coating reinforced by carbon nanotubes
    Deng, FM
    Chen, XH
    Chen, WX
    Li, WZ
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2004, 14 (04) : 681 - 685
  • [36] Wear resistance of electroless Ni-P-nano SiC composite coating
    Nongye Gongcheng Xuebao, 2007, 12 (105-108):
  • [37] Novel approaches on the study of wear performance of electroless Ni-P/diamond composite deposites
    Jappes, J. T. Winowlin
    Ramamoorthy, B.
    Nair, P. Kesavan
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2009, 209 (02) : 1004 - 1010
  • [38] Simultaneous friction and wear reduction of Ni-P/PTFE composites under dry sliding condition
    Li, Fei
    Yang, Yulin
    Song, Laizhou
    Liang, Lifen
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2021, 73 (04) : 581 - 587
  • [39] Micro-scale wear characteristics of electroless Ni-P/SiC composite coating under two different sliding conditions
    Franco, M.
    Sha, W.
    Malinov, S.
    Liu, H.
    WEAR, 2014, 317 (1-2) : 254 - 264
  • [40] The study of electroless Ni-P and Ni-P-PTFE coating on steel tire mold
    Guo, Jian-zhang
    Xu, Bin
    PROGRESS IN POLYMER PROCESSING, 2012, 501 : 316 - 320