Synergistic strengthening behavior and microstructural optimization of hybrid reinforced titanium matrix composites during thermomechanical processing

被引:17
作者
Li, Shaopeng [1 ]
Han, Yuanfei [1 ,2 ]
Shi, Zhusheng [3 ]
Huang, Guangfa [1 ]
Zong, Nan [1 ]
Le, Jianwen [1 ]
Qiu, Peikun [1 ]
Lu, Weijie [1 ,2 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, State Key Lab Met Matrix Composites, Shanghai 200240, Peoples R China
[2] Shanghai Key Lab Adv High Temp Mat & Precis Formi, Shanghai 200240, Peoples R China
[3] Imperial Coll London, Dept Mech Engn, London SW7 2AZ, England
基金
中国国家自然科学基金;
关键词
Titanium matrix composites; Thermomechanical processing; IMI834; Microstructure; Strengthening; TENSILE PROPERTIES; MECHANICAL-PROPERTIES; TIBW/TI6AL4V COMPOSITE; FRACTURE-TOUGHNESS; TIB WHISKERS; SITU; TEMPERATURE; EXTRUSION; DEFORMATION; FABRICATION;
D O I
10.1016/j.matchar.2020.110527
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, titanium matrix composites (TMCs) reinforced with hybrid TiB, TiC and RexOy (rare earth oxides) were successfully fabricated by vacuum arc melting technique. Subsequently thermomechanical processing was carried out to optimize the microstructure and investigate the synergistic strengthening behavior. It is found that the optimized microstructure mainly contained two typical regions: Region 1, reinforcement-lean region with coarse lamellar grains. Region 2, reinforcement-rich region containing fine equiaxed alpha grains comparing with reinforcement-lean region, all hybrid reinforcements distributed homogeneously at their grain boundaries and TiB fibers are perpendicular to the forging direction. It is shown that the reinforcement can stimulate the dynamic/static recrystallization during the thermomechanical processing. The tensile strength was significantly enhanced by the ternary reinforcements and the thermomechanical processing. A well-matched relationship between microstructure and mechanical properties is obtained. When the reinforcement content is 2.5 vol%, the tensile strength at room temperature and high temperature (700 degrees C) increased to 1214 MPa and 552 MPa, while the TMCs maintained a good elongation of 5.1% and 58% respectively. The strengthening mechanism could be attributed to the refinement of the matrix grain, the solid solution strengthening of C element and the load-bearing capability of TiB and ternary oxide clusters.
引用
收藏
页数:12
相关论文
共 45 条
  • [31] Effect of solid-solution strengthening on fracture toughness in extruded Mg-Zn alloys
    Somekawa, Hidetoshi
    Osawa, Yoshiaki
    Mukai, Toshiji
    [J]. SCRIPTA MATERIALIA, 2006, 55 (07) : 593 - 596
  • [32] Mechanical alloying and milling
    Suryanarayana, C
    [J]. PROGRESS IN MATERIALS SCIENCE, 2001, 46 (1-2) : 1 - 184
  • [33] Influence of spark plasma sintering and subsequent hot rolling on microstructure and flexural behavior of in-situ TiB and TiC reinforced Ti6Al4V composite
    Tabrizi, Saeid Ghesmati
    Sajjadi, Seyed Abdolkarim
    Babakhani, Abolfazl
    Lu, Weijie
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 624 : 271 - 278
  • [34] Processing-structure-property aspects of particulate- and whisker-reinforced titanium matrix composites
    Tjong, S. C.
    Mai, Yiu-Wing
    [J]. COMPOSITES SCIENCE AND TECHNOLOGY, 2008, 68 (3-4) : 583 - 601
  • [35] Wear and friction properties of experimental Ti-Si-Zr alloys for biomedical applications
    Tkachenko, Serhii
    Datskevich, Oleg
    Kulak, Leonid
    Jacobson, Staffan
    Engqvist, Hakan
    Persson, Cecilia
    [J]. JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2014, 39 : 61 - 72
  • [36] Effects of heat treatments on microstructure and tensile properties of as-extruded TiBw/near-α Ti composites
    Wang, B.
    Huang, L. J.
    Geng, L.
    Rong, X. D.
    Liu, B. X.
    [J]. MATERIALS & DESIGN, 2015, 85 : 679 - 686
  • [37] Effect of temperature on microstructure and mechanical properties of ECAPed (TiB + La2O3)/Ti-6Al-4V composites
    Xiang, Juan
    Han, Yuanfei
    Le, Jianwen
    Huang, Guangfa
    Xiao, Lv
    Liu, Jiayu
    Lu, Weijie
    [J]. MATERIALS CHARACTERIZATION, 2018, 146 : 149 - 158
  • [38] Ferroelectric polarization and fatigue characterization in bismuth-based Aurivillius thin films at lower voltage
    Yang, J.
    Song, D. P.
    Yin, Y.
    Chen, L. Z.
    Chen, L-Y.
    Wang, Y.
    Wang, J. Y.
    [J]. MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2019, 248
  • [39] Effect of reinforcements on β→α transformation and tensile properties of a near α titanium matrix composite
    Yang, Jianhui
    Chen Yuyong
    Xiao, Shulong
    Xu, Lijuan
    Wang, Xiaopeng
    Zhang, Dongdong
    Li, Mingao
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 766
  • [40] The tensile and fracture toughness properties of a (TiBw + TiCp)/Ti-3.5Al-5Mo-6V-3Cr-2Sn-0.5Fe composites after heat treatment
    Yang Jianhui
    Xiao Shulong
    Chen, Yuyong
    Xu Lijuan
    Wang Xiaopeng
    Zhang Dongdong
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 729 : 21 - 28