Microstructural evolution and shear strength of brazing C103 and Ti-6Al-4V using Ti-20Cu-20Ni-20Zr (wt.%) filler metal

被引:31
作者
Hong, IT [1 ]
Koo, CH [1 ]
机构
[1] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei 106, Taiwan
关键词
Ti-6Al-4V; C103; brazing; filler metal; microstructure; intermetallic alloys and compounds;
D O I
10.1016/j.ijrmhm.2005.05.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructural evolution and shear strength of the brazed C103 and Ti-6Al-4V joint using the Ti-20Cu-20Ni-20Zr (wt.%) filler metal were studied. The shear strength of the joint brazed at 950 degrees C increases with the brazing time. However, the shear strength of the joint brazed at 1000 degrees C decreases with the increasing brazing time, because of the formation of coarse acicular Widmanstatten structure in the joint interface during brazing. In the brazed joint, the width of eutectoid and Widmanstatten regions increase with the increasing brazing time. On the contrary, the thickness of central brazed layer reduces with the increasing brazing time. Additionally, it was found that to obtain a high joint strength of approximately 300 MPa, both the central brazed layer and the coarse Widmanstatten structure should be avoided forming in the brazed joint. (C) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:247 / 252
页数:6
相关论文
共 50 条
[31]   Effects of Fabrication Parameters on Interface of Zirconia and Ti-6Al-4V Joints Using Zr55Cu30Al10Ni5 Amorphous Filler [J].
Liu, Yuhua ;
Hu, Jiandong ;
Shen, Ping ;
Guo, Zuoxing ;
Liu, Huijie .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (09) :2602-2609
[32]   Microstructure evolution and joining strength of diamond brazed on Ti-6Al-4V substrates using Ti-free eutectic Ag-Cu filler alloy [J].
Liao, Xinjiang ;
Liu, Zhuo ;
Liu, Ruixiang ;
Mu, Dekui .
DIAMOND AND RELATED MATERIALS, 2022, 127
[33]   Vacuum brazing of SiO2 glass ceramic and Ti-6Al-4V alloy using AgCuTi filler foil [J].
Liu, H. B. ;
Zhang, L. X. ;
Wu, L. Z. ;
Liu, D. ;
Feng, J. C. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 498 (1-2) :321-326
[34]   The bonding of nickel foam to Ti-6Al-4V using Ti-Cu-Ni braze alloy [J].
Jarvis, T. ;
Voice, W. ;
Goodall, R. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (06) :2592-2601
[35]   Cu + TiB2 composite filler for brazing Al2O3 and Ti-6Al-4V alloy [J].
Yang, Minxuan ;
Lin, Tiesong ;
He, Peng .
JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 512 (01) :282-289
[36]   Brazing of C/C composite and Ti-6Al-4V with graphene strengthened AgCuTi filler: Effects of graphene on wettability, microstructure and mechanical properties [J].
Liu, Duo ;
Song, Yanyu ;
Zhou, Yinghao ;
Song, Xiaoguo ;
Fu, Wei ;
Feng, Jicai .
CHINESE JOURNAL OF AERONAUTICS, 2018, 31 (07) :1602-1608
[37]   Brazing of C/C composite and Ti-6Al-4V with graphene strengthened AgCuTi filler:Effects of graphene on wettability,microstructure and mechanical properties [J].
Duo LIU ;
Yanyu SONG ;
Yinghao ZHOU ;
Xiaoguo SONG ;
Wei FU ;
Jicai FENG .
Chinese Journal of Aeronautics, 2018, 31 (07) :1602-1608
[38]   Microstructure evolution and brazing mechanism of Ti5Si3/Ti3Al composite and Ni-based superalloy joints using Ti-Zr-Cu-Ni filler alloy [J].
Zhang, Tongtong ;
Yang, Xuesong ;
Miao, Kesong ;
Li, Danyang ;
Chen, Shuai ;
Cui, Xiping ;
Huang, Meng ;
Fan, Guohua ;
Geng, Lin .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 713 :28-34
[39]   Microstructure and shear strength of ZrB2-SiC/Ti-6Al-4V joint by TiCuZrNi with Cu foam [J].
Wang, Gang ;
Wang, Zhentao ;
Wang, Wei ;
He, Rujie ;
Gui, Kaixuan ;
Tan, Caiwang ;
Cao, Wei .
CERAMICS INTERNATIONAL, 2019, 45 (08) :10223-10229
[40]   Self-Powered Fast Brazing of Ti-6Al-4V Using Ni/Al Reactive Multilayer Films [J].
Bridges, Denzel ;
Rouleau, Christopher ;
Gosser, Zachary ;
Smith, Cary ;
Zhang, Zhili ;
Hong, Kunlun ;
Cheng, Jinquan ;
Bar-Cohen, Yoseph ;
Hu, Anming .
APPLIED SCIENCES-BASEL, 2018, 8 (06)