Relating the Early Evolution of Microstructure with the Electrochemical Response and Mechanical Performance of a Cu-Rich and Cu-Lean 7xxx Aluminum Alloy

被引:65
作者
Gupta, R. K. [1 ,2 ]
Deschamps, A. [3 ]
Cavanaugh, M. K. [1 ]
Lynch, S. P. [2 ,4 ]
Birbilisa, N. [1 ,2 ]
机构
[1] Monash Univ, Dept Mat Engn, Clayton, Vic 3168, Australia
[2] Monash Univ, ARC Ctr Excellence Design Light Met, Clayton, Vic, Australia
[3] INPGrenoble CNRS UJF, SIMAP, St Martin Dheres, France
[4] Def Sci & Technol Org, Melbourne, Vic, Australia
基金
欧洲研究理事会; 澳大利亚研究理事会;
关键词
AL-ZN-MG; ANGLE X-RAY; STRESS-CORROSION CRACKING; PITTING CORROSION; DYNAMIC PRECIPITATION; INTERMETALLIC PHASES; STOCHASTIC-MODELS; STAINLESS-STEELS; VOLUME FRACTION; GRAIN-BOUNDARY;
D O I
10.1149/2.062211jes
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
In this work AA7150 and AA7079 were studied as examples of 7xxx aluminum alloys with a high and low Cu content. The alloys were carefully examined to determine the evolution (incl. density and size) of precipitates during heat-treatment using small angle X-ray scattering (SAXS). Such characterization made it possible to relate the evolution of microstructure to specific properties such as electrochemical response (including metastable pitting analysis), hardness and crack growth rate (from SCC testing). The results revealed several important findings, indicating that there is a critical precipitate size above which a transition in electrochemical response occurs; in addition it is seen that Cu has an important role in both metastable pitting and crack propagation. The corrosion initiation and propagation phases are distinct in their mechanisms, and this is a function of the nature and state of the precipitates. Increased aging times increased the metastable pitting rate and SCC velocity in the Cu-lean alloy, whereas increased aging times decreased the metastable pitting rate the Cu-rich alloy. A correlation between metastable pitting rate and stable pitting is also presented. (C) 2012 The Electrochemical Society. [DOI: 10.1149/2.062211jes] All rights reserved.
引用
收藏
页码:C492 / C502
页数:11
相关论文
共 55 条
[1]   Effect of thermo-mechanical processing on filiform corrosion of aluminium alloy AA3005 [J].
Afseth, A ;
Nordlien, JH ;
Scamans, GM ;
Nisancioglu, K .
CORROSION SCIENCE, 2002, 44 (11) :2491-2506
[2]  
[Anonymous], G16800 ASTM, P685
[3]   Investigation and discussion of characteristics for intermetallic phases common to aluminum alloys as a function of solution pH [J].
Birbilis, N. ;
Buchheit, R. G. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2008, 155 (03) :C117-C126
[4]   Nano-scale dissolution phenomena in Al-Cu-Mg alloys [J].
Birbilis, N. ;
Cavanaugh, M. K. ;
Kovarik, L. ;
Buchheit, R. G. .
ELECTROCHEMISTRY COMMUNICATIONS, 2008, 10 (01) :32-37
[5]   Electrochemical characteristics of intermetallic phases in aluminum alloys - An experimental survey and discussion [J].
Birbilis, N ;
Buchheit, RG .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (04) :B140-B151
[6]  
Birbilis N, 2011, WOODHEAD PUBL MATER, P574
[7]   SURFACE-ROUGHNESS AND THE METASTABLE PITTING OF STAINLESS-STEEL IN CHLORIDE SOLUTIONS [J].
BURSTEIN, GT ;
PISTORIUS, PC .
CORROSION, 1995, 51 (05) :380-385
[8]   Modeling pit initiation rate as a function of environment for Aluminum alloy 7075-T651 [J].
Cavanaugh, M. K. ;
Birbilis, N. ;
Buchheit, R. G. .
ELECTROCHIMICA ACTA, 2012, 59 :336-345
[9]  
Cavanaugh M.K., 2009, THESIS OHIO STATE U
[10]   Precipitate characterisation in metallic systems by small-angle X-ray or neutron scattering [J].
De Geuser, Frederic ;
Deschamps, Alexis .
COMPTES RENDUS PHYSIQUE, 2012, 13 (03) :246-256