Plasticity of Mg-Gd alloys between 4 K and 298 K

被引:37
作者
Kula, A. [1 ,2 ]
Noble, K. [1 ]
Mishra, R. K. [3 ]
Niewczas, M. [1 ]
机构
[1] McMaster Univ, Mat Sci & Engn, Hamilton, ON, Canada
[2] AGH Univ Sci & Technol, Fac Nonferrous Met, PL-30059 Krakow, Poland
[3] Gen Motors Global R&D Ctr, Warren, MI USA
基金
加拿大自然科学与工程研究理事会;
关键词
Mg-Gd alloys; mechanical properties; work hardening; strengthening mechanisms; twinning; ductility; fracture; MAGNESIUM SINGLE-CRYSTALS; WORK-HARDENING BEHAVIOR; RARE-EARTH; DEFORMATION-BEHAVIOR; GRAIN-SIZE; TEXTURE DEVELOPMENT; YIELD STRENGTH; NONBASAL SLIP; DEPENDENCE; SOLUTE;
D O I
10.1080/14786435.2015.1123820
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Mechanisms of strength and ductility in textured Mg-Gd binary alloys are investigated under conditions of uniaxial tension and compression at 4.2, 78 and 298 K. The alloys obey solution strengthening relationships between the critical stress sigma(ss) and the concentration of the solute c, which scales as sigma(ss) similar to c(n), with n assuming values 0.30-0.53 for tension and 0.73-0.87 for compression. The results suggest that Gd solute hardens the compressive yield modes more than the tensile yield modes, with basal slip and extension twinning being the principal yielding mechanisms in tension and compression. Temperature dependence of the yield stress and sss stress suggests contribution of non-basal slip systems to the yielding of alloys. Twinning accounts for more than 80% of sample strain in the first 7% of compression, resulting in characteristic S-shape flow curves with four hardening stages. The work hardening in Stage A is determined by the extension twins propagating throughout primary grains and interacting with grain boundaries. Slip-twin interactions control the work hardening rate during Stage B, whereas slip-slip interactions determine the work hardening in fully twinned materials during Stage C and D. Under tension twining is less active, the plastic flow is associated with Stage III of work hardening, determined predominantly by slip-slip interactions. Increasing Gd concentration in the alloys leads to the reduction of tension-compression asymmetry, in agreement with results in the literature. Addition of Gd influences the failure and promotes ductile, transgranular fracture mode in Mg-Gd alloys down to the low temperatures. It is argued that Gd improves the cohesion strength of grain boundaries, which suppresses intergranular failure and affects favourably ductility of Mg-Gd alloys.
引用
收藏
页码:134 / 165
页数:32
相关论文
共 81 条
[21]  
Bohlen J., 2005, 10 INT S PHYS MAT IS
[22]   On the influence of the grain size and solute content on the AE response of magnesium alloys tested in tension and compression [J].
Bohlen, Jan ;
Dobron, Patrik ;
Swiostek, Jacek ;
Letzig, Dietmar ;
Chmelik, Frantisek ;
Lukac, Pavel ;
Kainer, Karl Ulrich .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 462 (1-2) :302-306
[23]   Segregation and clustering of solutes at grain boundaries in Mg-rare earth solid solutions [J].
Bugnet, M. ;
Kula, A. ;
Niewczas, M. ;
Botton, G. A. .
ACTA MATERIALIA, 2014, 79 :66-73
[24]   SOLID-SOLUTION HARDENING [J].
BUTT, MZ ;
FELTHAM, P .
JOURNAL OF MATERIALS SCIENCE, 1993, 28 (10) :2557-2576
[25]   Strain hardening due to {10(1)over-bar2} twinning in pure magnesium [J].
Caceres, C. H. ;
Lukac, P. ;
Blake, A. .
PHILOSOPHICAL MAGAZINE, 2008, 88 (07) :991-1003
[26]   On the strain hardening behaviour of magnesium at room temperature [J].
Caceres, C. H. ;
Blake, A. H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 462 (1-2) :193-196
[27]   Grain Size Hardening in Mg and Mg-Zn Solid Solutions [J].
Caceres, C. H. ;
Mann, Gemma E. ;
Griffiths, J. R. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (07) :1950-1959
[28]  
Caceres C. H., 2005, INT S PHYS MAT ISPMA
[29]  
Cáceres CH, 2002, PHYS STATUS SOLIDI A, V194, P147, DOI 10.1002/1521-396X(200211)194:1<147::AID-PSSA147>3.0.CO
[30]  
2-L