Influence of heat treatment on microstructure and sliding wear resistance of high chromium cast iron electroslag hardfacing layer

被引:19
作者
Wang, Hao [1 ]
Yu, Shengfu [1 ]
机构
[1] Huazhong Univ Sci & Technol, State Key Lab Mat Proc & Die & Mould Technol, Wuhan 430074, Peoples R China
关键词
Electroslag hardfacing; High chromium cast iron hardfacing layer; Heat treatment temperature; Microstructure; Sliding wear resistance; WHITE-IRON; SECONDARY-CARBIDES; PRECIPITATION; BEHAVIOR; STEEL; TRANSFORMATION; M23C6;
D O I
10.1016/j.surfcoat.2017.04.013
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, hypoeutectic high chromium cast iron (HCCI) is deposited on low alloy steel by using electroslag welding. The yielded mixture is furthered introspected by exposing it to range of temperatures (i.e. 440 degrees C, 480 degrees C, 520 degrees C, 560 degrees C, 600 degrees C). The respective microstructures are studied after the heat treatment, subsequently. Additionally, microstructures are also examined in terms of their hardness and wear resistance. The results demonstrate that hardness, wear resistance and coefficient of friction (COF) are correlated and these attributes reaches to their maximum value when the mixture is found to be composed of secondary carbides and martensite. It is evaluated that, when the HCCI hardfacing layer is post weld heat treated (PWHT) at 520 degrees C then the secondary carbides (M23C6) and martensite quantities are quantified as maximum and by comparing it with HCCI hardfacing layer, hardness, COF and wear resistance are found to be increased by 11.88%,25% and 30%, respectively. Wear resistance is also found to be at the maximum value at PWHT 520 degrees C holding crack at maximum depth of 2 pm. These findings reveal that HCCI hardfacing layer with PWHT temperature 520 degrees C can achieve the best outcome. (C) 2017 Published by Elsevier B.V.
引用
收藏
页码:182 / 190
页数:9
相关论文
共 50 条
  • [41] Influence of Niobium Content on the Mechanical Properties and Abrasion Wear Resistance of Heat-Treated High-Chromium Cast Iron
    Ibrahim, Mervat Mohamed
    El-Hadad, Shimaa
    Mourad, Mohamed
    INTERNATIONAL JOURNAL OF METALCASTING, 2021, 15 (02) : 500 - 509
  • [42] A Study on Influence of Aging Treatment on Sliding Wear Resistance of a Nickel Based Hardfacing Alloy
    Kesavan, D.
    Kamaraj, M.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2011, 64 (4-5) : 453 - 460
  • [43] A Study on Influence of Aging Treatment on Sliding Wear Resistance of a Nickel Based Hardfacing Alloy
    D. Kesavan
    M. Kamaraj
    Transactions of the Indian Institute of Metals, 2011, 64 : 453 - 460
  • [44] Microstructure and Corrosive Wear Property of Super High Chromium Cast Iron (SHCCI)
    Xu, Liujie
    Wei, Shizhong
    Li, Jiwen
    Zhang, Guoshang
    Ma, Xiangdong
    MACHINERY, MATERIALS SCIENCE AND ENGINEERING APPLICATIONS, PTS 1 AND 2, 2011, 228-229 : 905 - +
  • [45] Effect of Heat Treatment on Structure and Wear Resistance of High Chromium Cast Steel Containing Boron
    Qi-hong CEN
    Hai-bin ZHANG
    Han-guang FU
    JournalofIronandSteelResearch(International), 2014, 21 (05) : 532 - 538
  • [46] Effect of Heat Treatment on Structure and Wear Resistance of High Chromium Cast Steel Containing Boron
    Cen, Qi-hong
    Zhang, Hai-bin
    Fu, Han-guang
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2014, 21 (05) : 532 - 538
  • [47] Optimizing heat treatment and wear resistance of high chromium cast irons using computational thermodynamics
    Albertin, E.
    Beneduce, F.
    Matsumoto, M.
    Teixeira, I.
    WEAR, 2011, 271 (9-10) : 1813 - 1818
  • [48] Influence of Shot Peening Treatment in Erosion Wear Behavior of High Chromium White Cast Iron
    Gonzalez, Juan
    Borja Peral, Luis
    Zafra, Alfredo
    Fernandez-Pariente, Ines
    METALS, 2019, 9 (09)
  • [49] Influence of Ti and REE on Primary Crystallization and Wear Resistance of Chromium Cast Iron
    Dojka, Malwina
    Dojka, Rafal
    Stawarz, Marcin
    Studnicki, Andrzej
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (07) : 4002 - 4011
  • [50] Effect of surface Cr/C infiltration on microstructure, mechanical properties and wear resistance of high chromium cast iron
    Chen, Peng
    Wu, Zhao-yang
    Yi, Yan-liang
    Huang, Jian-bin
    Shang, Tao
    Li, Wei
    CHINA FOUNDRY, 2022, 19 (03) : 218 - 224